Simulation Analysis on the Effect of Cathode and Anode Center Distance on Electrothermal Field of 15 kA Rare Earth Electrolytic Cell AITranslate

School of Mechanical and Electrical Engineering,Jiangxi University of Science and Technology;School of Mechanical and Electrical Engineering,Jiangxi University of Science and Technology;School of Mechanical and Electrical Engineering,Jiangxi University of Science and Technology;School of Mechanical and Electrical Engineering,Jiangxi University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In order to solve the problem of ununiform thermal field distribution in rare earth electrolytic cell,a three-dimensional model of 15 kA rare earth electrolytic cell was established and the distance between anode and cathode of the model was adjusted. COMSOL software was used to simulate and analyze the electrothermal fibld in the electrolytic cell with different center distance between anode and cathode,to obtain the distribution of the three-dimensional electrothermal field in the electrolytic cell. The results show that with the increase of cathode and anode center distance, the high temperature isothermal surface in the electrolytic cell constantly shift towards the center of the cell, the highest isothermal surface of the right cathode gradually narrows to fall off the anode, and the highest isothermal surface near the left cathode constantly extends and shifts towards to the cell center. The maximum current density in the electrolytic cell has no obvious change regularity with the increase of cathode and anode center distance, reaching the maximum value at the center distance of d=33 mm and meanwhile obtaining the most uniform distribution of high temperature isothermal surface. The optimal distance between anode and cathode in the electrolytic cell is 33 mm.

KeyWords AITranslate

rare earth electrolytic cell cathode and anode center distance three-dimensional thermal field current density COMSOL software simulation analysis

1刘中兴,韩文帅,伍永福,胡永胜,鞠阳.60kA底部阴极稀土电解槽电场数值模拟[J].稀有金属与硬质合金,2015,43(1):26-28. 被引量:4

2王军,张作良,涂赣峰,吴文远.10kA底部阴极稀土熔盐电解槽电场的模拟[J].稀土,2010,31(4):36-39. 被引量:21

3王亮亮,颜波,刘木根.阳极结构调整对稀土电解槽的影响[J].中国稀土学报,2015,33(2):217-222. 被引量:10

4刘庆生,王建鲁,汤卫东.稀土铁合金电解槽电热场数值模拟[J].中国稀土学报,2016,34(4):444-452. 被引量:12

5王海辉,逄启寿,郜飘飘.稀土电解槽温度场的模拟分析与研究[J].稀有金属与硬质合金,2017,45(4):12-15. 被引量:10

6尹小东,刘中兴,曹运涛.稀土熔盐电解槽的热平衡计算[J].包头钢铁学院学报,2002,21(1):19-22. 被引量:16

7董云芳,刘中兴,伍永福,许立勇,何金辉.60kA底部阴极稀土电解槽极距的模拟优化[J].有色金属:冶炼部分,2013(10):32-35. 被引量:9

8王海辉,逄启寿,郜飘飘.大电流稀土电解槽三维电场的数值仿真[J].中国稀土学报,2017,35(4):514-519. 被引量:15

1廖春发,郭超,林觉远,蔡伯清,王旭.电流密度对稀土熔盐电解影响的研究进展[J].稀土,2021(1):122-128. 被引量:4

2逄启寿,张雨开,黄杰,张浩.稀土电解槽不同阴极结构的电解特性分析[J].稀土,2019,40(5):17-23. 被引量:4

3闫光礼,冯羽生,徐水太.镝铁阴极电蚀对稀土电解槽电解特性的影响[J].有色金属科学与工程,2019,10(6):92-96. 被引量:1

4叶楠,逄启寿,张浩,王海辉.大电流稀土电解槽阳极结构研究[J].中国稀土学报,2020,38(1):83-89. 被引量:5

5唐焱,刘金.稀土金属及合金12kA电解槽优化设计仿真研究[J].装备制造技术,2020(3):5-9. 被引量:2

6逄启寿,叶楠,张浩,周宏杰.6kA稀土电解槽电极位置对电场影响的模拟分析[J].机械设计与制造,2021(2):157-159. 被引量:1

7龚姚腾,林小程,逄启寿,叶楠.稀土电解槽阳极腐蚀消耗规律研究[J].中国稀土学报,2021,39(4):601-607.

1闫光礼,冯羽生,徐水太.镝铁阴极电蚀对稀土电解槽电解特性的影响[J].有色金属科学与工程,2019,10(6):92-96. 被引量:1

2刘庆生,程华金,谈成亮,邱建民,李华杰.非均一极距对稀土电解多相流影响的数值模拟及实验验证[J].有色金属科学与工程,2020,11(5):59-68.

3冯羽生,严少卿.管式稀土萃取槽中搅拌桨转速优选研究[J].现代矿业,2021,37(4):149-151. 被引量:1

4李忠岐,陈淑梅,洪侃,梁鑫,徐建兵,赖耀斌,陈东英,蔡伯清.LiF-CeF_(3)-CeO_(2)熔盐体系密度的影响因素研究[J].中国稀土学报,2021,39(2):282-286. 被引量:1

5龚姚腾,林小程,逄启寿,叶楠.稀土电解槽阳极腐蚀消耗规律研究[J].中国稀土学报,2021,39(4):601-607.

6冯硕,伍永福,刘中兴,周一凡,李赛楠.稀土熔盐电解过程阳极消耗形变对碳颗粒杂质运动规律影响[J].稀土,2021,42(6):31-41. 被引量:1

7冀燕子,肖发新,孙树臣,陈俊强,涂赣峰.大电流稀土熔盐电解槽槽型研究进展[J].中国稀土学报,2022,40(1):38-45.

8唐焱,梁冰,邵留宝.稀土熔融负压采集流体动力学仿真[J].冶金设备,2022(3):87-92.

9杨培宏,王新春,刘玉宝,张耀,张自雷,吕东澔.稀土熔盐电解智能控制系统研究与应用[J].稀土,2022,43(3):34-40. 被引量:2

10李科臻,王新春.稀土电解槽槽电阻数据的降噪与分析[J].新型工业化,2022,12(8):153-158. 被引量:1

1赵洪兴.基于铝电解槽电热场模拟分析的工艺参数再优化[J].轻金属,2017(10):29-31. 被引量:2

2董云芳,冯猛,刘中兴,伍永福,鞠阳,武殿斌.稀土电解槽电场对阳极气体气含率分布影响的数值模拟[J].稀有金属与硬质合金,2018,46(1):10-13. 被引量:3

3王亮,逄启寿.稀土电解槽三维电场和温度场的分析研究[J].中国有色冶金,2017,46(6):44-47. 被引量:7

4丁林,李明喜.激光熔覆Co基合金温度场的数值模拟[J].激光技术,2012,36(1):103-106. 被引量:3

5王兆丰,柯巍,马向攀.低温取芯过程热传递方式的数值模拟和实验研究[J].中国安全生产科学技术,2018,14(1):35-41. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]

Citation Information:

In order to solve the problem of ununiform thermal field distribution in rare earth electrolytic cell,a three-dimensional model of 15 kA rare earth electrolytic cell was established and the distance between anode and cathode of the model was adjusted. COMSOL software was used to simulate and analyze the electrothermal fibld in the electrolytic cell with different center distance between anode and cathode,to obtain the distribution of the three-dimensional electrothermal field in the electrolytic cell. The results show that with the increase of cathode and anode center distance, the high temperature isothermal surface in the electrolytic cell constantly shift towards the center of the cell, the highest isothermal surface of the right cathode gradually narrows to fall off the anode, and the highest isothermal surface near the left cathode constantly extends and shifts towards to the cell center. The maximum current density in the electrolytic cell has no obvious change regularity with the increase of cathode and anode center distance, reaching the maximum value at the center distance of d=33 mm and meanwhile obtaining the most uniform distribution of high temperature isothermal surface. The optimal distance between anode and cathode in the electrolytic cell is 33 mm.

quote

GB/T 7714-2015 [1] GONG Yao-teng, ZHOU Hong-jie, PANG Qi-shou, et al. Simulation Analysis on the Effect of Cathode and Anode Center Distance on Electrothermal Field of 15 kA Rare Earth Electrolytic Cell[J]. Rare Metals and Cemented Carbides, 2018(2): 1-5.
MLA [1] GONG Yao-teng, et al., "Simulation Analysis on the Effect of Cathode and Anode Center Distance on Electrothermal Field of 15 kA Rare Earth Electrolytic Cell." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 1-5.
APA [1] GONG Yao-teng, ZHOU Hong-jie, PANG Qi-shou, & WANG Hai-hui. (2018). Simulation Analysis on the Effect of Cathode and Anode Center Distance on Electrothermal Field of 15 kA Rare Earth Electrolytic Cell. Rare Metals and Cemented Carbides(2), 1-5.
IEEE [1] GONG Yao-teng, ZHOU Hong-jie, PANG Qi-shou, and WANG Hai-hui, "Simulation Analysis on the Effect of Cathode and Anode Center Distance on Electrothermal Field of 15 kA Rare Earth Electrolytic Cell," Rare Metals and Cemented Carbides, no. 2, pp. 1-5, 2018. keywords: {rare earth electrolytic cell;cathode and anode center distance;three-dimensional thermal field;current density;COMSOL software;simulation analysis}