Effect of Additives on the Micro Separation Mechanism of Low Grade Rare Earth-Niobium-Iron Crude Concentrate During Reduction Roasting AITranslate
Abstract AITranslate
The effects were studied of additives on the separation of iron, rare earth and niobium from low grade rare earth-niobium-iron crude concentrate during reduction roasting. The results show that when the crude concentrate with 31.9% TFe,3.16G REO and 2.91~//00 Nb205 is processed by direct reduction roast- ing,the iron grade of magnetic material is only 54. 45% ,and the recoveries of rare earth and niobium are 44.28% and 62.65% ,respectively. The reduction roasting effect is the best when 15% Na2SO4 and 5% activated carbon powder are added,the iron grade of magnetic material in the product is 89. 32% ,the iron recovery is 91.47%, REO and Nb20s contents of the non-magnetic materials are 5. 36% and 4. 62%, and their recoveries reach 96.09% and 95.83% ,respectively. The microstructure research results indicate that in the product from reduction roasting without additives, the iron granules are fine and have no clear boundary with other minerals, the aggregation degree of most rare earth and niobium granules are low, the grains are not well-knit, and the separation is not effective. In the product from reduction roasting added with Na2SO4 and activated carbon powder,iron,rare earth and niobium granules aggregate and grow up, and boundary between iron, rare earth, niobium and other minerals is clear, which is benefit for separation.
KeyWords AITranslate
1赵增祺.关于如何保护和利用好我国白云鄂博稀土矿资源的建议与思考[J].稀土信息,2011,17(5):5-7. 被引量:5
2杨武斌,罗勇,单强,牛贺才,于学元.内蒙古巴尔哲稀有稀土多金属矿床特征[J].矿物学报,2009,29(S1):266-266. 被引量:8
3特大型稀土稀有金属矿山在扎鲁特旗开工建设[J].稀土信息,2010,16(2):34-34. 被引量:5
4冯守忠.巴尔哲碱性花岗岩稀有稀土矿床地质特征及成因探讨[J].中国有色金属学报,1994,4(4):14-17. 被引量:4
5武建斌.山西省交口县赵家圪垛稀土 铌钽矿矿床特征[J].华北国土资源,2007(1):18-19. 被引量:7
6李英霞.从包钢强磁尾矿中回收稀土和铌的研究[J].广东有色金属学报,1999,9(2):101-105. 被引量:21
7叶志平,孙兴来,李英霞.强磁尾矿综合回收稀土、铌选矿工艺研究[J].有色金属:选矿部分,1996(6):1-4. 被引量:19
8白炜,刘志强,陈怀杰,梁振锋.某低品位复杂稀土精矿中提取稀土的研究[J].稀土,2009,30(6):67-70. 被引量:10
9刘牡丹,刘勇,刘珍珍.复杂稀有金属矿稀土回收新工艺[J].有色金属:冶炼部分,2012(1):32-34. 被引量:7
10刘牡丹,刘勇,刘珍珍.复杂稀有金属矿综合利用新工艺[J].有色金属:冶炼部分,2012(7):37-39. 被引量:6
1徐中华.人民陪审员制度改革中的参审职权研究[J].法制与经济,2018,27(3):27-28.
2彭莉娟.降低电池级碳酸锂产品中磁性物质含量的措施[J].江西化工,2018,34(1):29-32. 被引量:2
3胡友红,张毅,刘立德,谢祥,高长益,盛光敏.铌铁与铌氮的复合强化机理及对钢材强度的影响[J].冶金信息导刊,2017,54(4):21-27. 被引量:1
4Bromand Nourozi,Arash Boochani,Ahmad Abdolmaleki,Elmira Sartpi,Pezhman Darabi,Sirvan Naderi.Ti Impurity Effect on the Optical Coefficients in 2D Cu_2Si: A DFT Study[J].理论物理通讯:英文版,2018,69(1):101-106.
5孟昭瑞,李红立,廖璐.某含银低品位铁锰矿石选矿工艺研究[J].矿冶,2018,27(1):14-17. 被引量:1
6韩国研究团队成功研发超高速运转磁性存储器核心技术[J].新材料产业,2017,0(12):70-71.
7杜亚星,王广,王静松,薛庆国.含钛铌铁精矿含碳球团直接还原试验研究[J].烧结球团,2017,42(6):51-56. 被引量:2
8丁志广,李博.甲烷作用下硅镁型红土镍矿低温还原焙烧—磁选镍铁精矿[J].矿冶,2018,27(1):30-36. 被引量:2
9张海培,刘宏银,丁志广.甲烷作用下硅镁型红土镍矿还原焙烧试验[J].河南科技大学学报:自然科学版,2018,39(3):99-104.
10龙雨,胡友红,伍从应,谢祥,刘立德,高长益.提高钒铌元素收得率的转炉冶炼脱氧工艺探讨[J].四川冶金,2017,39(3):30-33. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TD955[矿业工程—选矿]
Citation Information:
The effects were studied of additives on the separation of iron, rare earth and niobium from low grade rare earth-niobium-iron crude concentrate during reduction roasting. The results show that when the crude concentrate with 31.9% TFe,3.16G REO and 2.91~//00 Nb205 is processed by direct reduction roast- ing,the iron grade of magnetic material is only 54. 45% ,and the recoveries of rare earth and niobium are 44.28% and 62.65% ,respectively. The reduction roasting effect is the best when 15% Na2SO4 and 5% activated carbon powder are added,the iron grade of magnetic material in the product is 89. 32% ,the iron recovery is 91.47%, REO and Nb20s contents of the non-magnetic materials are 5. 36% and 4. 62%, and their recoveries reach 96.09% and 95.83% ,respectively. The microstructure research results indicate that in the product from reduction roasting without additives, the iron granules are fine and have no clear boundary with other minerals, the aggregation degree of most rare earth and niobium granules are low, the grains are not well-knit, and the separation is not effective. In the product from reduction roasting added with Na2SO4 and activated carbon powder,iron,rare earth and niobium granules aggregate and grow up, and boundary between iron, rare earth, niobium and other minerals is clear, which is benefit for separation.
quote
| GB/T 7714-2015 | [1] LIU Mu-dan, LIU Yong, LIU Zhen-zhen. Effect of Additives on the Micro Separation Mechanism of Low Grade Rare Earth-Niobium-Iron Crude Concentrate During Reduction Roasting[J]. Rare Metals and Cemented Carbides, 2018(2): 6-10. |
| MLA | [1] LIU Mu-dan, et al., "Effect of Additives on the Micro Separation Mechanism of Low Grade Rare Earth-Niobium-Iron Crude Concentrate During Reduction Roasting." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 6-10. |
| APA | [1] LIU Mu-dan, LIU Yong, & LIU Zhen-zhen. (2018). Effect of Additives on the Micro Separation Mechanism of Low Grade Rare Earth-Niobium-Iron Crude Concentrate During Reduction Roasting. Rare Metals and Cemented Carbides(2), 6-10. |
| IEEE | [1] LIU Mu-dan, LIU Yong, and LIU Zhen-zhen, "Effect of Additives on the Micro Separation Mechanism of Low Grade Rare Earth-Niobium-Iron Crude Concentrate During Reduction Roasting," Rare Metals and Cemented Carbides, no. 2, pp. 6-10, 2018. keywords: {rare earth-niobium-iron associated ore;additive;reduction roasting;microstructure;Na2SO1;activated carbon} |