daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study of the Crack Detection Defect of Tungsten Wire and its Causes AITranslate

School of Materials Engineering, Central South University;School of Materials Engineering, Central South University;School of Materials Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The basic requirements for tungsten wire from lighting industry are introduced.Eddy current crack detection is performed for D0.39 mm tungsten wire.Based on sampling crack detection defect part and observing microstructure,some typical defect types are summarized and their formation causes and influence factors are briefly analyzed.

KeyWords AITranslate

D0.39 mm tungsten wire eddy current crack detection defect type metallographic analysis crack

1李家伟,陈积懋.无损探伤手册[M].北京:机械工业出版社,2002.

2王铁虎,杨斌,谢秀松.涡流探伤在钨丝生产中的应用[J].中国钨业,2008,23(3):43-45. 被引量:6

3白淑文.钨钼丝压力加工原理[M].北京:轻工业出版社,1984.

1严剑刚,高鸣,罗俊.涡流技术在钨杆自动检测中的应用[J].无损检测,2018,40(6):6-8. 被引量:3

1郭平,陈念蓉,黄庆德.自动涡流检测技术在民航发动机维修检测中的应用[J].自动化与信息工程,2020,41(2):44-48. 被引量:1

2严剑刚,高鸣,罗俊.短钨杆自动无心磨削工艺研究[J].制造技术与机床,2020,0(6):119-121.

3严剑刚,高鸣,罗俊.行星式球磨加工钨杆的工艺实验研究[J].制造技术与机床,2020(11):72-74. 被引量:2

1刘富国,齐增生,解海滨.平整机支承辊辊面裂纹分析[J].重型机械,2010(3):64-66.

2刘敏,黄海娥,王俊霖,孙宜强.中厚板探伤检测不合格的原因分析[J].物理测试,2015,33(2):26-30. 被引量:5

3埃默.,PJ,周忠善.应用自动超声波探伤检测铸件[J].五金科技,1991(4):38-40.

4李春华,林海鹏,胥良.提升钢丝绳探伤检测的研究[J].煤矿机械,2001,22(4):33-34. 被引量:5

5李玉胜,翟虎,马宝民,袁伟波,冯志军,曲选辉.高强度ZL205A合金大型铸件“白点”偏析研究[J].铸造,2007,56(2):185-187. 被引量:17

6巴顿菲尔TechBEX小型材挤出生产线[J].橡塑技术与装备,2006,32(6):6-6.

7巴顿菲尔TechBEX小型材挤出生产线[J].国外塑料,2006,24(4):78-78.

82012年模具检测新技术应用与检测案例分析会议即将召开[J].金属加工:冷加工,2012(10):77-77.

9杨林涛,张虎.超声波探伤检测的影响因素[J].中国石油和化工标准与质量,2013,33(16):18-18. 被引量:4

10胡现龙,张青,王静妹.锻钢冷轧工作辊表面草状波原因分析[J].现代冶金,2014,41(6):14-17. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

The basic requirements for tungsten wire from lighting industry are introduced.Eddy current crack detection is performed for D0.39 mm tungsten wire.Based on sampling crack detection defect part and observing microstructure,some typical defect types are summarized and their formation causes and influence factors are briefly analyzed.

quote

GB/T 7714-2015 [1] MOU Bing, WANG De-zhi, LUO Zhen-zhong. Study of the Crack Detection Defect of Tungsten Wire and its Causes[J]. Rare Metals and Cemented Carbides, 2011(2): 60-62.
MLA [1] MOU Bing, et al., "Study of the Crack Detection Defect of Tungsten Wire and its Causes." Rare Metals and Cemented Carbides, no. 2, 2011, pp. 60-62.
APA [1] MOU Bing, WANG De-zhi, & LUO Zhen-zhong. (2011). Study of the Crack Detection Defect of Tungsten Wire and its Causes. Rare Metals and Cemented Carbides(2), 60-62.
IEEE [1] MOU Bing, WANG De-zhi, and LUO Zhen-zhong, "Study of the Crack Detection Defect of Tungsten Wire and its Causes," Rare Metals and Cemented Carbides, no. 2, pp. 60-62, 2011. keywords: {D0.39 mm tungsten wire;eddy current crack detection;defect type;metallographic analysis;crack}