Inorganic Lead Halide Perovskite Micro-/Nanostructures: From Self-Assembly to Applications Inorganic Lead Halide Perovskite Micro-/Nanostructures: From Self-Assembly to Applications AITranslate
Abstract AITranslate
Inorganic lead halide perovskites (ILHPs), an emerging class of semiconductors, hold great potential for a broad spectrum of applications, ranging from solar cells and light-emitting diodes (LEDs) to scintillators and lasers, due to ILHPs’ exceptional optical/electronic properties. The properties of ILHPs are closely related to their micro-/nanostructures, and thus controlling the micro-/nanostructures of ILHPs is highly desired to promote further development. Self-assembly, a common but powerful method, has recently been explored for the synthesis and control of the micro-/nanostructures of ILHPs. In this Review, we first summarize recent advances in the self-assembly of ILHPs into micro-/nanostructures and pay attention to main factors that can influence the self-assembly process. We then illustrate representative applications of the self-assembled micro-/nanostructures of ILHPs, including photodetectors, LEDs, lasers, and X-ray imaging. And last, we offer our perspectives on the self-assembled micro-/nanostructures of ILHPs, particularly their applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00189
Chinese Library Classification Number:
Citation Information:
Inorganic lead halide perovskites (ILHPs), an emerging class of semiconductors, hold great potential for a broad spectrum of applications, ranging from solar cells and light-emitting diodes (LEDs) to scintillators and lasers, due to ILHPs’ exceptional optical/electronic properties. The properties of ILHPs are closely related to their micro-/nanostructures, and thus controlling the micro-/nanostructures of ILHPs is highly desired to promote further development. Self-assembly, a common but powerful method, has recently been explored for the synthesis and control of the micro-/nanostructures of ILHPs. In this Review, we first summarize recent advances in the self-assembly of ILHPs into micro-/nanostructures and pay attention to main factors that can influence the self-assembly process. We then illustrate representative applications of the self-assembled micro-/nanostructures of ILHPs, including photodetectors, LEDs, lasers, and X-ray imaging. And last, we offer our perspectives on the self-assembled micro-/nanostructures of ILHPs, particularly their applications.
quote
| GB/T 7714-2015 | [1] Weiqiu Kang, Yangyang Niu, Min Lu, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00189. |
| MLA | [1] Weiqiu Kang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00189. |
| APA | [1] Weiqiu Kang, Yangyang Niu, Min Lu, Yang Wei, Hongbo Li, & Xiaoji Xie. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00189 |