Microstructure and Properties of Porous Medical Titanium Alloy Implanted in Bones with Different Mo Contents AITranslate

College of Materials Science and Engineering,Chongqing University of Technology,Chongqing 400054,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the development of human biomedical level,requirements for medical materials have been enhanced. It requires high mechanical properties and outstanding corrosion resistance,etc. Titanium and titanium alloys are widely utilized in the fields of shipbuilding,aerospace,biomedical and chemical industries because of high specific strengths and good fatigue properties,low elastic modulus,excellent bio-compatibility and great corrosion resistance. However,the elastic modulus of titanium alloys that have been implanted into the host bone as a load-bearing material is much higher than that of host bones. It results in insufficient bearing of the host bones which triggers off the phenomenon of "stress shielding" and the atrophy and resorption of host bones. Eventually,it will lead to the failure of operation and implantation. Thereby,to solve the problem of mismatch of mechanical properties caused by elastic modulus of titanium alloy,researchers have carried out a variety of studies on the descent of elastic modulus of titanium alloy. It is mainly employed in accordance with such two aspects. Firstly,the design optimization of porous structures in titanium alloys. The introduction of pore structure could significantly reduce the elastic modulus of titanium alloys,and the connected porous structure with appropriate pore sizes was conducive to fluid exchange and the adhesion,proliferation and differentiation of osteoblasts on the surfaces of alloys. Consequently,new bone tissues that grow into pores would strengthen the connection between titanium alloys and bone,which would further improve the biocompatibility of titanium alloys. Additionally,the addition of β stabilizer could take an advantage of low elastic modulus of β-Ti,which promoted the development of a novel titanium alloy. As a β stabilizer,Mo can not only dramatically stabilize β phase,improve the mechanical properties of the alloys,but also improve the corrosion resistance of titanium alloys. However,most of the current studies focued on the influence of Mo on the microstructure and mechanical properties of dense titanium alloys. Meanwhile,there were few studies on the microstructure,mechanical properties and corrosion resistance of porous Ti-Mo alloys. As a consequence,pore structures,microstructures,mechanical properties and corrosion resistances of porous Ti-Mo alloys prepared by powder metallurgy were studied by multi-scale characterization methods such as optical microscopy (OM),scanning electron microscopy (SEM)and X-ray diffraction (XRD)in this research. Firstly,the complete porous Ti-Mo alloy samples were prepared by ball milling,cold pressing,desalination and sintering of Ti and Mo powders,and then the pore structures of porous Ti-Mo alloys were determined by Archimedes drainage methods and line intercept methods. The results demonstrated that with the increase of Mo element content from 5 at% to 20 at%,the number of tiny Kirkendall pores distributed on the skeleton of porous Ti-Mo alloys soared,the porosity of porous Ti-Mo alloys increased slightly from 38.06% to 41.36%,and the pore sizes were enhanced from 289.34 to 323.11 µm. Meanwhile,the microstructure characterization illustrated that the porous Ti-Mo alloys were mainly composed of α phase and β phase,the volume fraction of the α phase gradually plunged and the volume fraction of the β phase gradually ascended with the increase of Mo element contents. The α phase within grains gradually transformed from lamellae to needle-like shape and eventually disappeared. The ultimate compressive strength and elastic modulus of the porous Ti-Mo alloys gradually decreased as the content of Mo increased from 5 at% to 20 at% at room temperature. Finally,the results of corrosion resistance demonstrated that the self-corrosion potential increased from -281.8 to -225.8 mV and then decreased to-287.7 mV,and Ti-10Mo alloys exhibited better corrosion resistances.

KeyWords AITranslate

porous Ti-Mo alloy phase compositions elastic modulus compressive strengths electrochemical performance

[1]Ibrahim M K,Hamzah E,Saud S N,Nazim E M,Bahador A. Parameter optimization of microwave sintering porous Ti-23%Nb shape memory alloys for biomedical applications [J]. Transactions of Nonferrous Metals Society of China,2018,28(4):700.

[2]Kuroda P A B,Buzalaf M A R,Grandini C R. Effect of molybdenum on structure,microstructure and mechanical properties of biomedical Ti-20Zr-Mo alloys [J]. Mater Sci Eng C Mater Biol Appl,2016,67:511.

[3]Pitchi C S,Priyadarshini A,Sana G,Narala S K R. A review on alloy composition and synthesis of β-Titanium alloys for biomedical applications [J]. Materials Today:Proceedings,2020,26:3297.

[4]Meng Q K,Zhang J S,Huo Y F,Sui Y W,Zhang J Y,Guo S,Zhao X Q. Design of low modulus β-type titanium alloys by tuning shear modulus C44 [J]. Journal of Alloys and Compounds,2018,745:579.

[5]Geetha M,Singh A K,Asokamoni R,Gogia A K. Ti based biomaterials,the ultimate choice for orthopaedic implants-a review [J]. Progress in Materials Science,2009,54(3):397.

[6]Guerra C,Sancy M,Walczak M. Effect of added porosity on a novel porous Ti-Nb-Ta-Fe-Mn alloy exposed to simulated body fluid [J]. Mater Sci Eng C Mater Biol Appl,2020,111:110758.

[7]Ehtemam-Haghichi S,Attar H,Okulov I V,Dargusch M S,Kent D. Microstructural evolution and mechanical properties of bulk and porous low-cost Ti-Mo-Fe alloys produced by powder metallurgy [J]. Journal of Alloys and Compounds,2021,853:156768.

[8]Mohan P,Rajak D K,Pruncu C I,Ajit B,Vicente A B,Bakr E A. Influence of beta-phase stability in elemental blended Ti-Mo and Ti-Mo-Zr alloys [J]. Micron,2021,142:102992.

[9]Cardoso F F,Ferrandini P L,Lopes E S N,Cremasco A,Caram R. Ti-Mo alloys employed as biomaterials:effects of composition and aging heat treatment on microstructure and mechanical behavior [J]. J Mech Behav Biomed Mater,2014,32:31.

[10]Oliveira N T C,Aleixo G,Caram R,Guastaldi A C. Development of Ti-Mo alloys for biomedical applications:microstructure and electrochemical characterization [J]. Materials Science and Engineering:A,2007,452-453:727.

[11]Chen Y Y,Xu L J,Liu Z G,Kong F T,Chen Z Y. Microstructures and properties of titanium alloys Ti-Mo for dental use [J]. Transactions of Nonferrous Metals Society of China,2006,16:824.

[12]Zhou Y L,Luo D M. Microstructures and mechanical properties of Ti-Mo alloys cold-rolled and heat treated [J]. Materials Characterization,2011,62(10):931.

[13]Min X H,Emura S,Nishimura T,Zhang L,Tamilselvi S,Tsuchiya K,Tsuzaki K. Effects of α phase precipitation on crevice corrosion and tensile strength in Ti-15Mo alloy [J]. Materials Science and Engineering:A,2010,527(6):1480.

[14]Lu J W,Zhao Y Q,Ge P,Niu H Z. Microstructure and beta grain growth behavior of Ti-Mo alloys solution treated [J]. Materials Characterization,2013,84:105.

[15]Zhang W D,Liu Y,Wu H,Song M,Zhang T Y,Lan X D,Yao T H. Elastic modulus of phases in Ti-Mo alloys [J]. Materials Characterization,2015,106:302.

[16]Oliveira N T C,Guastaldi A C. Electrochemical stability and corrosion resistance of Ti-Mo alloys for biomedical applications [J]. Acta Biomater,2009,5(1):399.

[17]Ehtemam H S,Attar H,Okulov I V. Microstructural evolution and mechanical properties of bulk and porous low-cost Ti-Mo-Fe alloys produced by powder metallurgy [J]. Journal of Alloys and Compounds,2021,853:156768.

[18](尹胜. 多孔TiNb合金的腐蚀及其力学性能的影响[D].长沙:湘潭大学,2009. 1.)

S Yin. Corrosion of Porous TiNb Alloy and Its Influence on Mechanical Properties [D]. Changsha:Xiangtan University,2009. 1.

[19](赵朝勇,匡林,张雪峰. 细长孔的多孔Ti-5Nb合金制备及力学性能研究 [J]. 钢铁钒钛,2019,40(6):57.)

C Y Zhao,L Kuang,X F Zhang. Preparation and mechanical properties of porous Ti-5Nb alloy with slender holes [J]. Iron and Steel Vanadium Titanium,2019,40(6):57.

[20]Sequeira C A C,Amaral L. Role of Kirkendall effect in diffusion processes in solids [J]. Transactions of Nonferrous Metals Society of China,2014,24(1):1.

[21]Gao Z,Li Q Y,He F,Huang Y,Wan Y Z. Mechanical modulation and bioactive surface modification of porous Ti-10Mo alloy for bone implants [J]. Materials & Design,2012,42:13.

[22]Liu Y,Chen L F,Tang H P,Liu C T,Liu B,Huang B Y. Design of powder metallurgy titanium alloys and composites [J]. Materials Science and Engineering:A,2006,418(1-2):25.

[23]Mour M,Das D,Winkler T,Hoenig E,Mielke G,Morlock M M,Schilling A F. Advances in porous biomaterials for dental and orthopaedic applications [J]. Materials,2010,3(5):2947.

[24](徐丽娟. 牙科用钛合金组织与性能的研究 [D]. 哈尔滨:哈尔滨工业大学,2007. 1.)

L J Xu. Research on Themicrostructure and Properties of Titanium Alloy for Dentistry [D]. Harbin:Harbin Institute of Technology,2007. 1.

[25]Tang B,Kou H,Zhang X,Gao P Y,Li J S. Study on the formation mechanism of α lamellae in a near β titanium alloy [J]. Progress in Natural Science:Materials International,2016,26(4):385.

[26]Sadeghpour S,Abbasi S M,Morakabati M,Bruschi S. Correlation between alpha phase morphology and tensile properties of a new beta titanium alloy [J]. Materials & Design,2017,121:24.

[27]Zhao X F,Niinomi M,Nakai M,Hieda J. Beta type Ti-Mo alloys with changeable Young's modulus for spinal fixation applications [J]. Acta Biomater,2012,8(5):1990.

[28]Xie F X,He X B,Lu X,Cao S L,Qu X H. Preparation and properties of porous Ti-10Mo alloy by selective laser sintering [J]. Mater Sci Eng C Mater Biol Appl,2013,33(3):1085.

[29]Suri S,Viswanathan G B,Neeraj T,Hou D H,Mills M J. Room temperature deformation and mechanisms of slip transmission in oriented single-colony crystals of an α/β titanium alloy [J]. Acta Materialia,1999,47(3):1019.

[30]Mantri S A,Choudhuri D,Alam T,Viswanathan G B,Sosa J M,Fraser H L,Banerjee R. Tuning the scale of α precipitates in β-titanium alloys for achieving high strength [J]. Scripta Materialia,2018,154:139.

[31]Liu Y J,Li S J,Hou W T,Wang S G,Hao Y L,Yang R,Sercombe T B,Zhang L C. Electron beam melted beta-type Ti-24Nb-4Zr-8Sn porous structures with high strength-to-modulus ratio [J]. Journal of Materials Science & Technology,2016,32(6):505.

[32](李怀明,杨让. 回火索氏体钢轨钢循环应变行为与位错结构关系的研究 [J].钢铁研究学报,1995,(1):47.)

H M Li,R Yang. Study on the relationship between cyclic strain behavior and dislocation structure of tempered solitenite rail steel [J]. Journal of Iron and Steel Research,1995,(1):47.

[33]Xu W,Chen M,Lu X,Zhang D W,Singh H P,Shu Y J,Pan Y,Qu X H,Liu C Z. Effects of Mo content on corrosion and tribocorrosion behaviours of Ti-Mo orthopaedic alloys fabricated by powder metallurgy [J].Corrosion Science,2020,168:108557.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY24010037

Chinese Library Classification Number:TG135

Citation Information:

With the development of human biomedical level,requirements for medical materials have been enhanced. It requires high mechanical properties and outstanding corrosion resistance,etc. Titanium and titanium alloys are widely utilized in the fields of shipbuilding,aerospace,biomedical and chemical industries because of high specific strengths and good fatigue properties,low elastic modulus,excellent bio-compatibility and great corrosion resistance. However,the elastic modulus of titanium alloys that have been implanted into the host bone as a load-bearing material is much higher than that of host bones. It results in insufficient bearing of the host bones which triggers off the phenomenon of "stress shielding" and the atrophy and resorption of host bones. Eventually,it will lead to the failure of operation and implantation. Thereby,to solve the problem of mismatch of mechanical properties caused by elastic modulus of titanium alloy,researchers have carried out a variety of studies on the descent of elastic modulus of titanium alloy. It is mainly employed in accordance with such two aspects. Firstly,the design optimization of porous structures in titanium alloys. The introduction of pore structure could significantly reduce the elastic modulus of titanium alloys,and the connected porous structure with appropriate pore sizes was conducive to fluid exchange and the adhesion,proliferation and differentiation of osteoblasts on the surfaces of alloys. Consequently,new bone tissues that grow into pores would strengthen the connection between titanium alloys and bone,which would further improve the biocompatibility of titanium alloys. Additionally,the addition of β stabilizer could take an advantage of low elastic modulus of β-Ti,which promoted the development of a novel titanium alloy. As a β stabilizer,Mo can not only dramatically stabilize β phase,improve the mechanical properties of the alloys,but also improve the corrosion resistance of titanium alloys. However,most of the current studies focued on the influence of Mo on the microstructure and mechanical properties of dense titanium alloys. Meanwhile,there were few studies on the microstructure,mechanical properties and corrosion resistance of porous Ti-Mo alloys. As a consequence,pore structures,microstructures,mechanical properties and corrosion resistances of porous Ti-Mo alloys prepared by powder metallurgy were studied by multi-scale characterization methods such as optical microscopy (OM),scanning electron microscopy (SEM)and X-ray diffraction (XRD)in this research. Firstly,the complete porous Ti-Mo alloy samples were prepared by ball milling,cold pressing,desalination and sintering of Ti and Mo powders,and then the pore structures of porous Ti-Mo alloys were determined by Archimedes drainage methods and line intercept methods. The results demonstrated that with the increase of Mo element content from 5 at% to 20 at%,the number of tiny Kirkendall pores distributed on the skeleton of porous Ti-Mo alloys soared,the porosity of porous Ti-Mo alloys increased slightly from 38.06% to 41.36%,and the pore sizes were enhanced from 289.34 to 323.11 µm. Meanwhile,the microstructure characterization illustrated that the porous Ti-Mo alloys were mainly composed of α phase and β phase,the volume fraction of the α phase gradually plunged and the volume fraction of the β phase gradually ascended with the increase of Mo element contents. The α phase within grains gradually transformed from lamellae to needle-like shape and eventually disappeared. The ultimate compressive strength and elastic modulus of the porous Ti-Mo alloys gradually decreased as the content of Mo increased from 5 at% to 20 at% at room temperature. Finally,the results of corrosion resistance demonstrated that the self-corrosion potential increased from -281.8 to -225.8 mV and then decreased to-287.7 mV,and Ti-10Mo alloys exhibited better corrosion resistances.

quote

GB/T 7714-2015 [1] Junyi Liu, Ming'ao Li, Su Su, et al. Microstructure and Properties of Porous Medical Titanium Alloy Implanted in Bones with Different Mo Contents[J]. Chinese Journal of Rare Metals, 2025, 49(10): 1493-1502. DOI:10.13373/j.cnki.cjrm.XY24010037.
MLA [1] Junyi Liu, et al., "Microstructure and Properties of Porous Medical Titanium Alloy Implanted in Bones with Different Mo Contents." Chinese Journal of Rare Metals, vol. 49, no. 10, 2025, pp. 1493-1502, https://doi.org/10.13373/j.cnki.cjrm.XY24010037.
APA [1] Junyi Liu, Ming'ao Li, Su Su, Yu Gao, Wenwu Kang, & Bin Chen. (2025). Microstructure and Properties of Porous Medical Titanium Alloy Implanted in Bones with Different Mo Contents. Chinese Journal of Rare Metals, 49(10), 1493-1502. https://doi.org/10.13373/j.cnki.cjrm.XY24010037
IEEE [1] Junyi Liu, Ming'ao Li, Su Su, Yu Gao, Wenwu Kang, and Bin Chen, "Microstructure and Properties of Porous Medical Titanium Alloy Implanted in Bones with Different Mo Contents," Chinese Journal of Rare Metals, vol. 49, no. 10, pp. 1493-1502, 2025, doi: 10.13373/j.cnki.cjrm.XY24010037. keywords: {porous Ti-Mo alloy;phase compositions;elastic modulus;compressive strengths,electrochemical performance}