Sequential Infiltration Synthesis with Organic Co-reactants for Extensively Swollen Organic–Inorganic Hybrid Thin Films AITranslate

Chungnam National University; Korea Institute of Machinery and Materials (KIMM); Chungnam National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We demonstrate the growth of polymer–Al–O(−R) hybrid thin films via a sequential infiltration synthesis (SIS). SIS using an organic coreactant resulted in the expansion of the hybrid thin films with a highly uniform distribution of the chemical composition. This behavior stems from the large free volumes created by the long and flexible chains of the organic coreactant, enabling the continued incorporation of SIS precursors into the structures. The proposed method will be a valuable addition to vacuum deposition techniques for both organic–inorganic hybrid thin films and porous inorganic films with tunable porosity, pore morphology, and film thickness.

KeyWords AITranslate

sequential infiltration synthesis organic−inorganic hybrid alucone porous films in situ FTIR spectroscopy
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01645

Chinese Library Classification Number:

Citation Information:

We demonstrate the growth of polymer–Al–O(−R) hybrid thin films via a sequential infiltration synthesis (SIS). SIS using an organic coreactant resulted in the expansion of the hybrid thin films with a highly uniform distribution of the chemical composition. This behavior stems from the large free volumes created by the long and flexible chains of the organic coreactant, enabling the continued incorporation of SIS precursors into the structures. The proposed method will be a valuable addition to vacuum deposition techniques for both organic–inorganic hybrid thin films and porous inorganic films with tunable porosity, pore morphology, and film thickness.

quote

GB/T 7714-2015 [1] Minkyung Ko, HyeongU Kim, Nari Jeon. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01645.
MLA [1] Minkyung Ko, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01645.
APA [1] Minkyung Ko, HyeongU Kim, & Nari Jeon. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01645
IEEE [1] Minkyung Ko, HyeongU Kim, and Nari Jeon, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01645. keywords: {sequential infiltration synthesis;organic−inorganic hybrid;alucone;porous films;in situ FTIR spectroscopy}