Historical Perspectives and Recent Research on DNA Hydrogel-Based Stimuli-Responsive Systems and Bioengineering Applications AITranslate

China|Youjiang Medical University for Nationalities; The Third Affiliated Hospital of Southern Medical University; Dongguan University of Technology; Affiliated Hospital of Youjiang Medical University for Nationalities; Affiliated Hospital of Youjiang Medical University for Nationalities; Shanghai Jiao Tong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Soft hydrogel materials have attracted increasing attention from scientists due to the programmability of nucleic acids. DNA hydrogels are increasingly used in biomedicine due to their natural biocompatibility and degradation properties. Moreover, the addition of various molecules to these hydrogels can enhance the superiority and utility of DNA hydrogels. Therefore, the present study aimed to provide a timely overview of historical perspectives and recent research advances in DNA hydrogels and their applications in bioengineering and stimulus-responsive systems. The state-of-the-art problems and future prospects of DNA hydrogels were also discussed.

KeyWords AITranslate

artificial extracellular matrix bioengineering DNA hydrogels stimuliresponsive
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01528

Chinese Library Classification Number:

Citation Information:

Soft hydrogel materials have attracted increasing attention from scientists due to the programmability of nucleic acids. DNA hydrogels are increasingly used in biomedicine due to their natural biocompatibility and degradation properties. Moreover, the addition of various molecules to these hydrogels can enhance the superiority and utility of DNA hydrogels. Therefore, the present study aimed to provide a timely overview of historical perspectives and recent research advances in DNA hydrogels and their applications in bioengineering and stimulus-responsive systems. The state-of-the-art problems and future prospects of DNA hydrogels were also discussed.

quote

GB/T 7714-2015 [1] Zhifu Cao, Kai Li, Chong Wang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01528.
MLA [1] Zhifu Cao, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01528.
APA [1] Zhifu Cao, Kai Li, Chong Wang, Jia Liu, Yujin Tang, & Liqiang Wang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01528
IEEE [1] Zhifu Cao, Kai Li, Chong Wang, Jia Liu, Yujin Tang, and Liqiang Wang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01528. keywords: {artificial extracellular matrix;bioengineering;DNA;hydrogels;stimuliresponsive}