Research Progress of Porous Titanium and Titanium Alloy AITranslate
Abstract AITranslate
Preparation methods,special properties and application of porous metal materials are briefly introduced.The latest research progress of porous titanium and its alloys are emphatically reviewed.Some problems existing in preparation and application of porous titanium and its alloy are summarized,and their future development directions are proposed.
KeyWords AITranslate
1肖逸锋,刘艳,汤智,吴靓,许艳飞,钱锦文,贺跃辉.Ni-Cr-Fe多孔材料的制备及抗氧化性能[J].中国有色金属学报,2017,27(2):295-304. 被引量:6
2Mechanical properties of porous titanium with different distributions of pore size[J].中国有色金属学报:英文版,2013,0(8):2317-2322. 被引量:11
3李虎,虞奇峰,张波,王辉,范红松,张兴栋.浆料发泡法制备生物活性多孔钛及其性能[J].稀有金属材料与工程,2006,35(1):154-157. 被引量:37
4王哲君,强洪夫,王学仁.新型亚稳β钛合金Ti2448的温变形行为及本构模型[J].中国有色金属学报,2013,23(5):1295-1300. 被引量:2
5胡海波,刘会群,王杰恩,易丹青,傅上,孙武令.生物医用多孔钛及钛合金的研究进展[J].材料导报:纳米与新材料专辑,2012,26(1):262-266. 被引量:23
6颉芳霞,何雪明,俞经虎,武美萍,何新波,曲选辉.生物医用多孔Ti-6Mo合金选择性激光烧结的结构特征和力学行为[J].稀有金属材料与工程,2016,45(6):1477-1482. 被引量:10
7刘洁,刘旭燕,刘芳,王飞,潘登.纳米多孔铜钛合金的制备及其超级电容器性能[J].材料研究学报,2015,29(12):913-920. 被引量:5
8沈宏飞,尤德强,张鹏,李卫.以NH_4HCO_3为造孔剂制备的多孔钛及其力学性能[J].特种铸造及有色合金,2016,36(3):291-294. 被引量:3
1刘卓萌,刘忠军,姬帅,雒设计.Ti5Si3的制备与应用研究进展[J].材料导报,2019,33(S02):175-180. 被引量:1
2张兰,王翔,刘军,张春秋,叶金铎,刘璐.3D打印钛合金骨小梁多孔结构的拉伸性能[J].中国组织工程研究,2020,24(22):3498-3503. 被引量:14
3吴小玉,汪涛,周苗,黄文静,黄卫星.植酸/氢氧化钙改性对3D打印纯钛多孔结构生物矿化的影响[J].稀有金属,2020,44(7):680-686. 被引量:6
4胡勇,李申申,吴栋,李英新,康文江,张昊,张会莹.聚多巴胺接枝纳米氧化锌复合涂层对TC4合金表面修饰的影响[J].稀有金属材料与工程,2021,50(8):2876-2882.
5刘卓萌,刘忠军,姬帅.Ti-Si金属间化合物多孔膜材料的制备[J].中国有色金属学报,2021,31(9):2490-2498.
6王建忠,敖庆波,荆鹏,王建.多孔钛的制备及应用[J].稀有金属材料与工程,2022,51(5):1907-1918. 被引量:3
7胡勇,胡永淇,李申申,张会莹,褚成,王力华.钛合金表面GO/纳米ZnO复合涂层的制备及性能[J].稀有金属材料与工程,2022,51(8):2915-2922.
8王建忠,敖庆波,马军,李爱君.钛合金纤维多孔材料制备及压缩性能[J].粉末冶金技术,2023,41(2):125-130.
9刘坤,马北越,周萍,昝文宇,余超,邓承继,王周福.钛合金熔炼用Y_(2)O_(3)–Al_(2)O_(3)–MgO–CaO系耐火材料的设计与制备[J].硅酸盐学报,2023,51(3):628-634.
1王丁,李宁.基于微推出实验评价选择性激光烧结多孔桩的粘接强度[J].中国医药导报,2021,18(30):84-87.
2Hua-Fang Li,Jin-Yan Huang,Gui-Cai Lin,Peng-Yu Wang.Recent advances in tribological and wear properties of biomedical metallic materials[J].稀有金属:英文版,2021,40(11):3091-3106.
3He Li,Yong-Sheng Liu,Yan-Song Liu,Qing-Feng Zeng,Jing-Jing Liang.Microstructure and mechanical properties of 3D printed ceramics with different vinyl acetate contents[J].稀有金属:英文版,2021,40(11):3241-3250. 被引量:1
4李天海.金属材料拉伸性能及测试方法研究[J].中国金属通报,2021(18):124-125.
5刘曙光,许奎雪,夏超群,姜红江,李强,张朝锋,王振国,史春宝.3D打印多孔钛合金植入物髌腱重建愈合效果动物实验研究[J].河北工业大学学报,2022,51(1):42-53.
6Chun-Sheng Shao,Liang-Jian Chen,Rui-Min Tang,Bo Zhang,Jiang-Jie Tang,Wei-Na Ma.Polarized hydroxyapatite/BaTiO_(3) scaffolds with bio-inspired porous structure for enhanced bone penetration[J].稀有金属:英文版,2022,41(1):67-77.
7Chun-Sheng Shao,Liang-Jian Chen,Rui-Min Tang,Bo Zhang,Jiang-Jie Tang,Wei-Na Ma.Degradation and biological performance of porous osteomimetic biphasic calcium phosphate in vitro and in vivo[J].稀有金属:英文版,2022,41(2):457-468.
8Yao Ding,Zhang Yuan,Jin-Wei Hu,Kun Xu,Hong Wang,Peng Liu,Kai-Yong Cai.Surface modification of titanium implants with micro–nanotopography and NIR photothermal property for treating bacterial infection and promoting osseointegration[J].稀有金属:英文版,2022,41(2):673-688. 被引量:1
9Huan-Ming Chen,Hao-Yu Huang,Yang Xue,Kai Li,Tie-Xin Ding,Xiao-Jun Cai,Jun Chen,Lan Zhang.Immobilization of pegylated AMP on hydroxyapatite nanorods for antibiosis[J].稀有金属:英文版,2022,41(2):713-722.
10张强,杜俊炜,戴志兵,武峻申,江仁兵.3D打印定制半骨盆假体置换治疗原发性髋臼周围恶性肿瘤的疗效评估[J].实用骨科杂志,2022,28(3):203-208. 被引量:4
1施兰,杨立军,代文豪,李宁宁,闫程程.沉积温度对多孔钛表面仿生制备羟基磷灰石的影响[J].材料科学与工艺,2017,25(6):27-33. 被引量:1
2李栋.3D打印技术在生物医用多孔钛合金的研究进展[J].当代化工研究,2017(8):103-105. 被引量:2
3罗洪峰,张先满.多孔金属激光增材制造研究进展[J].铸造技术,2018,39(1):236-239. 被引量:2
4章辉,夏荣,朱一铭,刘春,闵曦,肖楠楠,刘芮.选择性激光熔覆制备微孔钛试件及体内实验研究[J].安徽医科大学学报,2017,52(12):1800-1805.
5曹阳阳,王焕钦,秦飞虎,桂华侨,刘建国,余同柱,孙强,吕亮,王杰,程寅.用于颗粒物监测仪的小型法拉第杯的优化设计[J].仪表技术与传感器,2018,0(2):48-51. 被引量:1
6刘兆平,周旭峰.石墨烯发展,浙江蓝图已绘[J].经贸实践,2017,0(12):24-25.
7曹凤,张文彦,张思思,燕阳天,杨瑞锋.多孔金属材料的化学制备方法及性能研究进展[J].材料导报,2017,31(21):139-145. 被引量:7
8纳米多孔金属催化材料进展[J].科学中国人,2017,0(10Z):11-11.
9唐新明.浅谈血液制品的制备及临床应用[J].中外健康文摘:医药月刊,2007,4(5):177-179.
10关磊,张力嫱.新型多孔碳泡沫材料的制备及其应用研究[J].化工新型材料,2018,46(1):25-28. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]
Citation Information:
Preparation methods,special properties and application of porous metal materials are briefly introduced.The latest research progress of porous titanium and its alloys are emphatically reviewed.Some problems existing in preparation and application of porous titanium and its alloy are summarized,and their future development directions are proposed.
quote
| GB/T 7714-2015 | [1] REN Xin-ming, MA Bei-yue, ZHANG Bo-wen, et al. Research Progress of Porous Titanium and Titanium Alloy[J]. Rare Metals and Cemented Carbides, 2018(1): 61-64. |
| MLA | [1] REN Xin-ming, et al., "Research Progress of Porous Titanium and Titanium Alloy." Rare Metals and Cemented Carbides, no. 1, 2018, pp. 61-64. |
| APA | [1] REN Xin-ming, MA Bei-yue, ZHANG Bo-wen, ZHANG Ya-ran, YU Jing-kun, & QU Xuan-hui. (2018). Research Progress of Porous Titanium and Titanium Alloy. Rare Metals and Cemented Carbides(1), 61-64. |
| IEEE | [1] REN Xin-ming, MA Bei-yue, ZHANG Bo-wen, ZHANG Ya-ran, YU Jing-kun, and QU Xuan-hui, "Research Progress of Porous Titanium and Titanium Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 61-64, 2018. keywords: {porous metal material;titanium;titanium alloy;biocompatibility;research progress} |