Study on Grain Growth kinetics of Ti(C,N)-based Cermets during Sintering AITranslate

Lingnan Normal University Business School;School of Mechanical and Electrical Engineering, Guangdong University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The sintered samples of Ti(C,N)-based cermets were prepared by vacuum sintering at different heating temperature for different holding time.The grain size was measured with metallographic quantitative method.The grain growth kinetic model of Ti(C,N)-based cermets during sintering was established based on Sellars model and Anelli model,and the grain growth kinetic equation was determined by nonlinear regression analysis of the experimental data.The results show that when the temperature is lower than1 300 ℃,the average grain size of Ti(C,N)-based cermets increases with the increase of the holding time,but the growth rate is slow.When the temperature is higher than 1 300℃,the grain growth rate rapidly increases at first to reach the maximum value and then decreases.The crystal grain growth apparent activation energy of Ti(C,N)-based cermets during sintering is 493.67 kJ/mol,and the kinetic equation is d^2.82=d^2.820+2.75×10^23 t^ 1.373 exp[-493 670/(RT)].

KeyWords AITranslate

Ti (C N)-based cermet vacuum sintering grain growth grain size kinetic equation apparent activation energy

1李鹏南,唐思文,张厚安,张永忠.Ti(C,N)基金属陶瓷刀具的高速切削性能与磨损机理[J].中国有色金属学报,2008,18(7):1286-1291. 被引量:15

2董广彪,熊计,郭智兴,万维财,易成红.Mo_2C对Ti(C,N)基金属陶瓷腐蚀性能的影响[J].硬质合金,2012,29(3):160-166. 被引量:9

3孙万昌,佘晓林,张磊,李攀.烧结工艺和粘结相对Ti(C,N)基金属陶瓷微观组织的影响[J].热加工工艺,2013,42(8):1-5. 被引量:8

4郑勇,汪胜祥,袁泉,石增敏.纳米复合Ti(C,N)基陶瓷烧结晶粒长大的特性[J].三峡大学学报:自然科学版,2003,25(2):105-107. 被引量:2

5刘建涛,刘国权,胡本芙,陈焕铭,宋月鹏,张义文.FGH96合金晶粒长大规律的研究[J].材料热处理学报,2004,25(6):25-29. 被引量:38

6李伟,陈文琳,吴跃,杨栋,周香.42CrMo钢加热时奥氏体晶粒长大演化规律[J].材料热处理学报,2015,36(1):104-108. 被引量:27

7李立新,汪凌云,周家林,唐力.等温条件下晶粒长大模型研究[J].武汉科技大学学报,2002,25(4):335-336. 被引量:7

8杨小红,张士宏,王忠堂,张路宁,冯斌.GH4169合金等温条件下晶粒长大数学模型研究[J].沈阳理工大学学报,2007,26(3):64-68. 被引量:5

9岳重祥,张立文,廖舒纶,裴继斌,高惠菊,贾元伟,廉晓洁.GCr15钢奥氏体晶粒长大规律研究[J].材料热处理学报,2008,29(1):94-97. 被引量:37

10肖水清,程利霞,伍尚华.Ti(C,N)基金属陶瓷烧结过程的显微组织演化[J].稀有金属与硬质合金,2016,44(3):37-41. 被引量:3

1王坤.Mo对Ti(C,N)金属陶瓷组织结构和力学性能影响[J].陶瓷,2019,0(12):29-40.

2刘锦,梁炳亮,方财生,何文,张建军,艾云龙.0.6Ca0.61La0.26TiO3-0.4La(Mg0.5Ti0.5)O3介质陶瓷微波烧结的晶粒生长动力学研究[J].人工晶体学报,2020,49(7):1300-1307.

3肖水清,伍尚华.Ti(C,N)基金属陶瓷显微结构演化的蒙特卡罗模拟研究[J].硬质合金,2020,37(4):257-265.

1肖和,张立,傅又红,张华栋.固相阶段烧结气氛对Ti(C,N)基金属陶瓷成分、组织和性能的影响[J].硬质合金,2017,34(3):143-149. 被引量:4

2汪建新,吴永刚,陈肖洁.LSSVM的特征选择算法在烧结过程的应用[J].机械设计与制造,2018,0(3):75-77. 被引量:1

3王程明,王福明,肖寄光,吴丹,陈曦,李长荣.Cr-Mo-V高铁制动盘用钢的奥氏体晶粒长大行为[J].金属热处理,2017,42(12):14-19. 被引量:3

4李剑,代雨航,朱忠丽.铥镱双掺氧化钆钇透明陶瓷的制备与发光性能[J].硅酸盐学报,2017,45(10):1474-1480.

5申笑天,孙方宏.新型碳化硅基体单层CVD金刚石磨盘的制备[J].超硬材料工程,2017,29(6):1-6.

6寇凌霄.真空烧结粘片芯片脱落失效分析[J].微处理机,2018,39(1):5-8.

7章天金,周东祥,姜胜林.Al_2O_3掺杂ZnO压敏陶瓷的晶粒生长研究[J].功能材料,2000,31(5):519-521. 被引量:7

8王伟,陈可,袁晓,余传贵,马广旭.Mg-Zn-Ca-Ti非晶合金的非等温晶化动力学[J].材料科学与工程学报,2017,35(5):810-814. 被引量:1

9张道礼,曹明贺,周东祥,欧阳世翕.微波场中BaTiO_3陶瓷的烧结及施、受主掺杂对晶粒生长的影响[J].功能材料,2000,31(5):528-530. 被引量:5

10高温熔融型UV玻璃发泡油墨[J].丝网印刷,2018,0(1):55-55.

Basic Information:

DOI:

Chinese Library Classification Number:TG148[金属学及工艺—金属材料]

Citation Information:

The sintered samples of Ti(C,N)-based cermets were prepared by vacuum sintering at different heating temperature for different holding time.The grain size was measured with metallographic quantitative method.The grain growth kinetic model of Ti(C,N)-based cermets during sintering was established based on Sellars model and Anelli model,and the grain growth kinetic equation was determined by nonlinear regression analysis of the experimental data.The results show that when the temperature is lower than1 300 ℃,the average grain size of Ti(C,N)-based cermets increases with the increase of the holding time,but the growth rate is slow.When the temperature is higher than 1 300℃,the grain growth rate rapidly increases at first to reach the maximum value and then decreases.The crystal grain growth apparent activation energy of Ti(C,N)-based cermets during sintering is 493.67 kJ/mol,and the kinetic equation is d^2.82=d^2.820+2.75×10^23 t^ 1.373 exp[-493 670/(RT)].

quote

GB/T 7714-2015 [1] XIAO Shui-qing, WU Shang-hua. Study on Grain Growth kinetics of Ti(C,N)-based Cermets during Sintering[J]. Rare Metals and Cemented Carbides, 2018(1): 56-60.
MLA [1] XIAO Shui-qing, and WU Shang-hua. "Study on Grain Growth kinetics of Ti(C,N)-based Cermets during Sintering." Rare Metals and Cemented Carbides, no. 1, 2018, pp. 56-60.
APA [1] XIAO Shui-qing, & WU Shang-hua. (2018). Study on Grain Growth kinetics of Ti(C,N)-based Cermets during Sintering. Rare Metals and Cemented Carbides(1), 56-60.
IEEE [1] XIAO Shui-qing and WU Shang-hua, "Study on Grain Growth kinetics of Ti(C,N)-based Cermets during Sintering," Rare Metals and Cemented Carbides, no. 1, pp. 56-60, 2018. keywords: {Ti (C, N)-based cermet;vacuum sintering;grain growth;grain size;kinetic equation;apparent activation energy}