Abstract AITranslate
The influences of sintering aids Al2O3-Y2O3on sintering performance of B4C/B-Al composites were studied in vacuum carbon tube furnace under argon atmosphere at 1 850 ℃ holding 1.5 h.The results indicated that physical mechanical properties of B4C/B-Al composites are improved through adding Al2O3-Y2O3.Comparing to samples without sintering aids the volume density of the samples increase 26.94%,porosity decreases 32.1%,and compression increases 85.81% averagely.At the same time it was pointed out that the sin...
KeyWords AITranslate
1李文辉,李文新.碳化硼陶瓷的液相烧结试验研究[J].哈尔滨理工大学学报,2002,7(2):73-75. 被引量:15
2汪德宁,徐颖,徐东,吴建生,王家敏,张澜庭,毛大立.金属间化合物FeAl与α-Al_2O_3的界面润湿行为及合金元素Y和Nb的作用[J].材料科学与工艺,1996,4(1):5-9. 被引量:17
1张其土.利用外加SiC改善Si_3N_4陶瓷材料的抗氧化性能[J].佛山陶瓷,1995(3):19-23.
2曾新强.Al2O3—Y2O3—SiO2系统的相平衡和玻璃的分相及结晶化[J].玻璃译林,1992(2):35-41.
3尚俊玲,陈维平,刘城,李元元.助烧剂和造孔剂对真空烧结SiC多孔陶瓷性能的影响[J].耐火材料,2006,40(6):450-452. 被引量:5
4张阳,韩亚苓,王辰,白兴亮,吴哲.SiC加入量对Sialon/SiC复合陶瓷显微组织的影响[J].中国陶瓷,2015,51(2):37-40. 被引量:5
5孙洋,陈树江,田琳,李国华.埋炭烧成MgO-Al复合材料中MgAlON的形成[J].耐火材料,2016,50(6):428-431. 被引量:3
6侯铁翠,韩东方,郑英姿,张锐,卢红霞.Al_2O_3/Al复合材料的制备及性能研究[J].佛山陶瓷,2008,18(3):1-3.
7李国星,陈昌平,郭兰静,李玮,刘安,卢红霞.用真空碳管炉烧结结构陶瓷[J].河南建材,2003(3):15-16. 被引量:1
8李文辉,李文新.碳化硼陶瓷的液相烧结试验研究[J].哈尔滨理工大学学报,2002,7(2):73-75. 被引量:15
9司文捷,林仕伟.不同α—SiC粉料液相烧结特性的研究[J].材料导报,2000(Z10):48-50. 被引量:1
10徐超,王忠,周辉,田先明,李家虎,龚仕顺.SiC-Al_2O_3-Y_2O_3体系陶瓷料浆的制备与性能研究[J].武汉工程职业技术学院学报,2013,25(1):13-16. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TQ174[化学工程—陶瓷工业]
Citation Information:
The influences of sintering aids Al2O3-Y2O3on sintering performance of B4C/B-Al composites were studied in vacuum carbon tube furnace under argon atmosphere at 1 850 ℃ holding 1.5 h.The results indicated that physical mechanical properties of B4C/B-Al composites are improved through adding Al2O3-Y2O3.Comparing to samples without sintering aids the volume density of the samples increase 26.94%,porosity decreases 32.1%,and compression increases 85.81% averagely.At the same time it was pointed out that the sin...
quote
| GB/T 7714-2015 | [1] WANG Dong-shan, XUE Xiang-xin. Influence of Sintering Aids on Sintering Performance of B_4C/B-Al[J]. Rare Metals and Cemented Carbides, 2008(1): 20-23. |
| MLA | [1] WANG Dong-shan, and XUE Xiang-xin. "Influence of Sintering Aids on Sintering Performance of B_4C/B-Al." Rare Metals and Cemented Carbides, no. 1, 2008, pp. 20-23. |
| APA | [1] WANG Dong-shan, & XUE Xiang-xin. (2008). Influence of Sintering Aids on Sintering Performance of B_4C/B-Al. Rare Metals and Cemented Carbides(1), 20-23. |
| IEEE | [1] WANG Dong-shan and XUE Xiang-xin, "Influence of Sintering Aids on Sintering Performance of B_4C/B-Al," Rare Metals and Cemented Carbides, no. 1, pp. 20-23, 2008. keywords: {sintering aids;B-Al compound;B4C;sintering performance;mechanical properties} |