Study on Process and Mechanism of Extraction Separation of Sc and P in Zirconium Residue Wash Water AITranslate

Hunan Rare-Earth Metal Materials Reseach Institute;Hunan Rare-Earth Metal Materials Reseach Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The extraction properties and mechanism of three different extraction systems (P350, P507 and P20:l) for P and Sc were studied. Based on comparison, P204-TBP-kerosene system is the best extraction system for separation of Sc and Pb. The ideal organic phase composition is 25% P204+4% TBP+ 71% kerosene, and the suitable feed liquid acidity is 5.4 mol/L. Under the above conditions, Sc extraction rate is 98.78% and P extraction rate is 20.99%. P204 extraction system is suitable for a wide range of feed liquid acidity and P content,and the recovered products can be used directly as a raw material into a high-purity scandium oxide production line. This method has simple and economical process and high recovery rate with the value of popularization and application.

KeyWords AITranslate

zirconium residue wash water scandium phosphorus extraction separation P204 process mechanism

1黄奇,张月英,余守慧.从锆英石提取钪的研究[J].上海金属:有色分册,1989,10(2):36-40. 被引量:7

2杨革.从钨渣中提取高纯氧化钪[J].湖南有色金属,2001,17(1):18-20. 被引量:33

3谢丽娜.钪锆的萃取分离[J].稀土,1991,12(5):68-69. 被引量:9

4宋金如,郑全伟,刘英,蒋小良.从高纯氧化钪中分离微量铁、锆的研究[J].湿法冶金,2004,23(3):151-156. 被引量:9

5Ishiwatari,M Kimura,E.用离子交换法从稀土金属中分离锆[J].离子交换与吸附,1990,6(3):222-222. 被引量:3

6傅玉琴,周移,李龙泉.PMBP萃淋树脂分离钪中微量锆[J].化学试剂,1999,21(1):44-46. 被引量:7

7赵云岭,李德谦.甲基膦酸二(1-甲庚)酯萃取钪的机理[J].应用化学,1990,7(2):1-5. 被引量:2

8侯利生.P_(507)和P_(204)在稀土分离中的应用[J].包钢科技,2005,31(S1):26-29. 被引量:9

9谢丽娜.从氯化物介质中萃取钪[J].稀有金属,1992,16(2):89-92. 被引量:2

10李正安.利用钛白粉生产的废酸提取高纯氧化钪[J].河南化工,1996,15(2):32-33. 被引量:9

1孙帅,孙宏骞,宋静,曲景奎,齐涛.钪资源现状及溶剂萃取在钪提取过程中的应用研究进展[J].过程工程学报,2020,20(8):877-886. 被引量:7

1葛阳阳,孟建卫,张凯熙,郭静粉.含氟助剂两段酸浸提取钒钛磁铁矿尾矿中的钪[J].稀土,2022,43(4):73-80. 被引量:2

2刘国栋,付勇,何伟,唐波,龙珍,杨颖,龙克树.中国铝土岩系中伴生钪资源富集规律及富集机制初探[J].地质论评,2021,67(4):952-972. 被引量:2

3李望,王雯博,段理哲,朱晓波.伯胺7101萃取分离钒及有机相乳化分析[J].矿冶工程,2021,41(4):76-78.

4邱叶红,董惠,朱刘.钪回收提取技术发展现状[J].中国资源综合利用,2021,39(10):145-147. 被引量:1

5冯艳虎,庄故章,周平,李子豪,晋艳玲,张培.西昌三圆石材厂废料中高钪矿物的浮选试验[J].矿冶,2021,30(6):20-28.

6潘思呈,徐红彬,张红玲,董玉明,张宏军,娄太平.赤泥硫酸铵焙烧浸出液水解制备偏钛酸的研究[J].无机盐工业,2023,55(2):85-91.

7邓冰,王晓慧,梁友伟,肖军辉.攀枝花地区含钪钒钛磁铁矿尾矿提钪关键技术研究[J].矿产综合利用,2023(4):50-54.

1李金华.国际科技活动测度体系群的演化与发展[J].国外社会科学,2018,0(3):116-125. 被引量:3

2郑汝伟,包申旭,张一敏.P204-TBP浸渍树脂的制备及对钒(Ⅳ)的吸附研究[J].有色金属:冶炼部分,2018(1):39-43. 被引量:3

3梁协池,刘学斌,杨燕生.2-乙基已基膦酸单2-乙基已基酯(P_(507))在水—癸醇体系中两相电离常数的测定[J].中山大学学报:自然科学版,1985,0(1):85-89.

Basic Information:

DOI:

Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]

Citation Information:

The extraction properties and mechanism of three different extraction systems (P350, P507 and P20:l) for P and Sc were studied. Based on comparison, P204-TBP-kerosene system is the best extraction system for separation of Sc and Pb. The ideal organic phase composition is 25% P204+4% TBP+ 71% kerosene, and the suitable feed liquid acidity is 5.4 mol/L. Under the above conditions, Sc extraction rate is 98.78% and P extraction rate is 20.99%. P204 extraction system is suitable for a wide range of feed liquid acidity and P content,and the recovered products can be used directly as a raw material into a high-purity scandium oxide production line. This method has simple and economical process and high recovery rate with the value of popularization and application.

quote

GB/T 7714-2015 [1] WU Xi-tao, WANG Zhi-jian. Study on Process and Mechanism of Extraction Separation of Sc and P in Zirconium Residue Wash Water[J]. Rare Metals and Cemented Carbides, 2018(3): 1-5.
MLA [1] WU Xi-tao, and WANG Zhi-jian. "Study on Process and Mechanism of Extraction Separation of Sc and P in Zirconium Residue Wash Water." Rare Metals and Cemented Carbides, no. 3, 2018, pp. 1-5.
APA [1] WU Xi-tao, & WANG Zhi-jian. (2018). Study on Process and Mechanism of Extraction Separation of Sc and P in Zirconium Residue Wash Water. Rare Metals and Cemented Carbides(3), 1-5.
IEEE [1] WU Xi-tao and WANG Zhi-jian, "Study on Process and Mechanism of Extraction Separation of Sc and P in Zirconium Residue Wash Water," Rare Metals and Cemented Carbides, no. 3, pp. 1-5, 2018. keywords: {zirconium residue wash water;scandium;phosphorus;extraction separation;P204;process;mechanism}