Treatment of Cyanide Tailings with Persulfate Oxidizers at Different Temperatures AITranslate

1.School of Metallurgical Engineering,Xi'an University of Architectural Science and Technology,Xi'an 710055,China
2.Shaanxi Gold and Resources Key Laboratory,Xi'an 710055,China
3.Jiangxi Chemical Industry Design Institute,Nanchang 330000,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cyanidation is still the main gold extraction process,but it is accompanied by a large number of cyanide tailings,whose composition is complex and difficult to deal with. If it is directly stored without treatment,it will occupy a large amount of land,bring environmental pollution problems and a serious waste of resources,so the study of its harmlessness,minimization,resource comprehensive treatment process is crucial for the ecological environment and metal resources recycling. Compared with the fire method,the wet reaction conditions are more moderate and controllable,the reaction speed is fast,and the adaptability to the raw ore is strong,etc. It has a wider development prospect. At present,the advanced oxidation technology of persulfate (PS)has attracted extensive attention from researchers,which has the advantages of high stability,easy operation,low price,etc. The activation of SO4·− radicals has the characteristics of long half-life,wide pH application range,and strong oxidizability,etc. In this paper,persulfate was used as the oxidant,persulfate was used as an oxidizing agent to treat cyanide tailings,focusing on the effect of temperature on the leaching process and the oxidation reaction mechanism of pyrite. Through chemical analysis,X-ray diffraction analysis (XRD),scanning electron microscopy (SEM)and other means,the changes in the leaching rate of ferric ions during the oxidation process,the enrichment of gold,the changes in the main mineral types before and after leaching,and the types of free radicals and their contributions were systematically analyzed. The results showed that the iron leaching rate gradually increased with the increase of reaction temperature,and the leaching rate reached 93.69% at 90 ℃. Macrokinetic analysis showed that the leaching process conformed to the pseudo-primary kinetic model,with a reaction rate constant of 0.0897 h−1,an apparent activation energy of 41.177 kJ·mol−1,and a chemical reaction as the main rate-controlling step. XRD and SEM results showed that the cratering and corrosion cracking of the pyrite surface worsened with the increase of temperature,but no diffraction peaks of other iron minerals appeared at the end of the leaching process,which indicated that the leaching process was mainly the dissolution reaction of FeS2,not a simple oxidation and desulfurization reaction. At 90 ℃,cyanide tailings quality loss rate of 52.8%,the gold content of 1.19 g·t−1 enriched to 2.88 g·t−1,the aggravation of corrosion of pyrite was conducive to the exposure of the gold and silver wrapped in pyrite,and to increase the subsequent leach agent and its contact area,which contributed to the subsequent recovery of gold and silver treatment,contributing to the subsequent recovery of gold and silver processing. Methanol (MeOH)and tert-butanol (TBA)were added as active species bursting agents in the persulfate oxidation system to investigate the free radical species and their contributions in the system. The results showed that the decomposition of pyrite in cyanide tailings under ambient conditions was mainly attributed to the direct oxidation of S2O82−,but the oxidation potential of PS itself was low,and pyrite could not be oxidized effectively. With the increase of leaching temperature,persulfate absorbed external energy to induce the homolytic decomposition of O–O bonds,and the contribution of oxidation by SO4·− and HO· radicals increased,and the contribution of HO· oxidation could reach 94.13% at 90 ℃. At the same time,the significant decrease in pH during the oxidation process was favorable for the generation of free radicals through HSO4− decomposition pathway. During the oxidation process,the oxidation mechanisms of SO4·− and HO· radicals on pyrite were similar,both preferentially reacted with S atoms,but due to the coordination number limitation of S atoms,the neighboring Fe atoms at this time had a stronger affinity compared to the radicals,and the preferential oxidation of Fe atoms would further promote the deep oxidation of S atoms. This might be the fundamental reason why the physical phase of FeS2 remained unchanged during the oxidation process. During the experiment,phosphoric acid was used to mask Fe3+,and it could be seen that at lower temperatures,the lower Fe3+ content of iron ions had less influence on the leaching rate,but when the temperature increased,the large amount of Fe3+ production was conducive to the destruction of the S–S bond,and at the same time realized the cyclic conversion between Fe2+/Fe3+,which promoted the generation of free radicals and further enhances the leaching rate. However,the activation mode of energy transfer was still dominant in the whole oxidation process,supplemented by the activation mode of electron transfer with Fe2+ as the electron donor. This indicated that the effect of temperature on PS treatment of cyanide tailings was mainly reflected in the change of the reaction rate constant (k)and Gibbs free energy (ΔG)in the radical generation reaction,which in turn affected pH of the reaction system and the composition of the oxidized substances.

KeyWords AITranslate

cyanide tailings sodium persulfate free radicals oxidation

[1]袁嘉声,畅永锋,郑春龙,杨新华,王伟,谢锋. 氰化尾渣脱氰技术综述[J].中国有色金属学报,2021,31(6):1568.

J S Yuan,Y F Chang,C L Zheng,X H Yang,W Wang,F Xie. Review on treatment technologies of cyanide tailing[J].The Chinese Journal of Nonferrous Metals,2021,31(6):1568.

[2]Donato D B,Nichols O,Possingham H,Moore M,Ricci P F ,Noller B N. A critical review of the effects of gold cyanide-bearing tailings solutions on wildlife[J].Environment International,2007,33(7):974.

[3]Li H Y,Ma A Y,Srinivasakannan C,Zhang L B,Li S W ,Yin S H. Investigation on the recovery of gold and silver from cyanide tailings using chlorination roasting process[J].Journal of Alloys and Compounds,2018,763:241.

[4]Lv C C,Ding J,Qian P,Li Q C,Ye S F ,Chen Y F. Comprehensive recovery of metals from cyanidation tailing[J].Minerals Engineering,2015,70:141.

[5]刘志建,金哲男,王保仁,杨洪英,董准勤,陈涛. 黄金冶炼氰渣火法处理研究现状及展望[J].有色金属(冶炼部分),2021,(1):84.

Z J Liu,Z N Jin,B R Wang,H Y Yang,Z Q Dong,T Chen. Research status and prospect of pyrometallurgical treatment of cyanide residue from gold smelting[J].Nonferrous Metals (Extractive Metallurgy),2021,(1):84.

[6]任传裕,武彪,尚鹤,温建康,邓静娴,张其东. 酸性生物预氧化渣硫脲浸金过程动力学[J].稀有金属,2024,48(11):1661.

C Y Ren,B Wu,H Shang,J K Wen,J X Deng,Q D Zhang. Kinetics study on gold leaching with thiourea from acid bio-oxidation slag[J].Chinese Journal of Rare Metals,2024,48(11):1661.

[7]杨鹏,王杰,周元浩,李玉玺. 氰渣浮选尾矿回收硫试验研究[J].黄金,2023,44(11):35.

P Yang,J Wang,Y H Zhou,Y X Li. Experimental study ons ulfur recovery from cyanide residue flotationtailings[J].Gold,2023,44(11):35.

[8]马红周,杨志祥,郭运生,建海顺,赵兵,毋鹏先. 焙烧氰化尾渣中氧化铁的磁化焙烧研究[J].稀有金属,2012,36(3):507.

H Z Ma,Z X Yang,Y S Guo,H S Jian,B Zhao,P X Wu. Magnetization roasting of Fe2O3 in tailings of roasting-cyaniding process[J].Chinese Journal of Rare Metals,2012,36(3):507.

[9]陈潮方,邱仙辉,邱廷省,张春菊,谢泽政,董浩,赖瑞森. 氰化尾渣的性质特点与综合利用研究现状[J].有色金属科学与工程,2022,13(4):107.

C F Chen,X H Qiu,T S Qiu,C J Zhang,Z Z Xie,H Dong,R S Lai. Research status of properties and comprehensive utilization of cyanide tailings[J].Nonferrous Metals Science and Engineering,2022,13(4):107.

[10]Zhao D,Liao X Y,Yan X L,Huling S G,Chai T,Tao H. Effect and mechanism of persulfate activated by different methods for PAHs removal in soil[J].Journal of Hazardous Materials,2013,254-255:228.

[11]Zheng X X,Niu X J,Zhang D Q,Lv M Y,Ye X Y,Ma J L,Lin Z,Fu M L. Metal-based catalysts for persulfate and peroxymonosulfate activation in heterogeneous ways:a review[J].Chemical Engineering Journal,2021,429:132323.

[12]Han W W,Yang H Y,Tong L L. Removal of cyanide in gold cyanide residues through persulfate-advanced oxidation process[J].Minerals,2023,13(5):613.

[13]Chen S H,Xiong P,Zhan W,Xiong L. Degradation of ethylthionocarbamate by pyrite-activated persulfate[J]. Minerals Engineering,2018,122:38.

[14]Liao L,Song Y H,Zhang P P,Li Y F,Bao J ,Zhou J M. Treatment of actual cyanide gold extraction wastewater by persulfate oxidation and its reaction mechanism[J].Research on Chemical Intermediates,2023,49:3705.

[15]Héctor I L,Brian L B,Luis B B,Efraím A S G,Ricardo A T P,Fiderman M M,Samir F C A. Degradation of hexacyanoferrate (Ⅲ)ion by the coupling of the ultraviolet light and the activation of persulfate at basic pH[J].Journal of Environmental Chemical Engineering,2021,9:106233.

[16]Miao D,Peng J B,Zhou X H,Qian L,Wang M J,Zhai L,Gao S X. Oxidative degradation of atenolol by heat-activated persulfate:kinetics,degradation pathways and distribution of transformation intermediates[J].Chemosphere,2018,207:174.

[17]Zrinyi N,Pham A L T. Oxidation of benzoic acid by heat-activated persulfate:effect of temperature on transformation pathway and product distribution[J]. Water Research,2017,120:43.

[18]王勇,张远琴,但娟,施宗友. EDTA络合滴定法测量高炉渣中铁(Ⅲ)和铁(Ⅱ)[J].冶金分析,2017,37(8):49.

Y Wang,Y Q Zhang,J Dan,Z Y Shi. Determination of ferric iron and ferrous iron in blast furnace slag by EDTA complexometric titration[J].Metallurgical Analysis,2017,37(8):49.

[19]Tang Y,Li G H,Yang Y,Ma J,Zhi Y X,Yao Y Y,Zheng L L,Tuo B Y. Oxidation of gold-bearing pyrite by ammonium persulfate[J].Journal of Sustainable Metallurgy,2021,7:1280.

[20]Neta P,Huie R E,Ross A B. Rate constants for reactions of inorganic radicals in aqueous solution[J].Journal of Physical and Chemical Reference Data,1988,17(3):1027.

[21]Nasseri S,Mahvi A H,Seyedsalehi M,Yaghmaeian K,Nabizadeh R,Alimohammadi M ,Safari G H. Degradation kinetics of tetracycline in aqueous solutions using peroxydisulfate activated by ultrasound irradiation:effect of radical scavenger and water matrix[J].Journal of Molecular Liquids,2017,241:704.

[22]Peng W Y,Dong Y X,Fu Y,Wang L L,Li Q C,Liu Y J,Fan Q Y,Wang Z H. Non-radical reactions in persulfate-based homogeneous degradation processes:a review[J]. Chemical Engineering Journal,2020,421:127818.

[23]王健行,张青青,曾亦婷,谢心怡,王赵鹏,王春英. 热活化过硫酸盐降解典型选矿药苯甲羟肟酸[J].有色金属工程,2024,14(5):143.

J X Wang,Q Q Zhang,Y T Zang,X Y Xie,Z P Wang,C Y Wang. Degradation of typical mineral processing agent benzohydroxamicacid by heat-activated persulfate[J]. Nonferrous Metals Engineering,2024,14(5):143.

[24]Kim C,Ahn J Y,Kim T Y,Shin W S,Hwang I. Activation of persulfate by nanosized zero-valent iron (NZVI):mechanisms and transformation products of NZVI[J].Environmental Science & Technology,2018,52(6):3625.

[25]Liu Z B,Ren X,Duan X Y,Sarmah A K ,Zhao X S. Remediation of environmentally persistent organic pollutants (POPs)by persulfates oxidation system (PS):a review[J].Science of the Total Environment,2022,863:160818.

[26]Tu Z H,Guo C L,Zhang T,Lu G N,Wan J J,Liao C J,Dang Z. Investigation of intermediate sulfur species during pyrite oxidation in the presence and absence of acidithiobacillus ferrooxidans[J].Hydrometallurgy,2017,167:58.

[27]符志强,罗玲玲,王超. 四川典型废弃硫铁矿地块环境调查研究[J].铜业工程,2023,(2):122.

Z Q Fu,L L Luo,C Wang. Environmental investigation of typical abandoned pyrites mine land in Sichuan[J]. Copper Engineering,2023,(2):122.

[28]Dong H Y,Qiang Z M,Hu J,Sans C. Accelerated degradation of iopamidol in iron activated persulfate systems:roles of complexing agents[J].Chemical Engineering Journal,2017,316:288.

[29]Lin K Y A,Lin J Y,Jochems A P. Oxidation of amaranth dye by persulfate and peroxymonosulfate activated by ferrocene[J].Journal of Chemical Technology and Biotechnology,2016,92(1):163.

[30]Zhang T,Wang Y Q,Hu Y N,Wang Z,Chen J H,Niu X P,Li Y Q,Gong X Z. HO selective cleavage FeS bond for FeS2 electrolysis in alkaline solution[J]. Electrochimica Acta,2019,306:327.

[31]He P,Zhu J Y,Chen Y Z,Chen F,Zhu J L,Liu M F,Zhang K,Gan M. Pyrite-activated persulfate for simultaneous 2,4-DCP oxidation and Cr(Ⅵ)reduction[J]. Chemical Engineering Journal,2020,406:126758.

[32]Jing B H,Li J,Nie C Y,Zhou J H,Li D D,Ao Z M. Flow line of density functional theory in heterogeneous persulfate-based advanced oxidation processes for pollutant degradation:a review[J].Critical Reviews in Environmental Science and Technology,2022,53(4):483.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY23080004

Chinese Library Classification Number:TF09

Citation Information:

Cyanidation is still the main gold extraction process,but it is accompanied by a large number of cyanide tailings,whose composition is complex and difficult to deal with. If it is directly stored without treatment,it will occupy a large amount of land,bring environmental pollution problems and a serious waste of resources,so the study of its harmlessness,minimization,resource comprehensive treatment process is crucial for the ecological environment and metal resources recycling. Compared with the fire method,the wet reaction conditions are more moderate and controllable,the reaction speed is fast,and the adaptability to the raw ore is strong,etc. It has a wider development prospect. At present,the advanced oxidation technology of persulfate (PS)has attracted extensive attention from researchers,which has the advantages of high stability,easy operation,low price,etc. The activation of SO4·− radicals has the characteristics of long half-life,wide pH application range,and strong oxidizability,etc. In this paper,persulfate was used as the oxidant,persulfate was used as an oxidizing agent to treat cyanide tailings,focusing on the effect of temperature on the leaching process and the oxidation reaction mechanism of pyrite. Through chemical analysis,X-ray diffraction analysis (XRD),scanning electron microscopy (SEM)and other means,the changes in the leaching rate of ferric ions during the oxidation process,the enrichment of gold,the changes in the main mineral types before and after leaching,and the types of free radicals and their contributions were systematically analyzed. The results showed that the iron leaching rate gradually increased with the increase of reaction temperature,and the leaching rate reached 93.69% at 90 ℃. Macrokinetic analysis showed that the leaching process conformed to the pseudo-primary kinetic model,with a reaction rate constant of 0.0897 h−1,an apparent activation energy of 41.177 kJ·mol−1,and a chemical reaction as the main rate-controlling step. XRD and SEM results showed that the cratering and corrosion cracking of the pyrite surface worsened with the increase of temperature,but no diffraction peaks of other iron minerals appeared at the end of the leaching process,which indicated that the leaching process was mainly the dissolution reaction of FeS2,not a simple oxidation and desulfurization reaction. At 90 ℃,cyanide tailings quality loss rate of 52.8%,the gold content of 1.19 g·t−1 enriched to 2.88 g·t−1,the aggravation of corrosion of pyrite was conducive to the exposure of the gold and silver wrapped in pyrite,and to increase the subsequent leach agent and its contact area,which contributed to the subsequent recovery of gold and silver treatment,contributing to the subsequent recovery of gold and silver processing. Methanol (MeOH)and tert-butanol (TBA)were added as active species bursting agents in the persulfate oxidation system to investigate the free radical species and their contributions in the system. The results showed that the decomposition of pyrite in cyanide tailings under ambient conditions was mainly attributed to the direct oxidation of S2O82−,but the oxidation potential of PS itself was low,and pyrite could not be oxidized effectively. With the increase of leaching temperature,persulfate absorbed external energy to induce the homolytic decomposition of O–O bonds,and the contribution of oxidation by SO4·− and HO· radicals increased,and the contribution of HO· oxidation could reach 94.13% at 90 ℃. At the same time,the significant decrease in pH during the oxidation process was favorable for the generation of free radicals through HSO4− decomposition pathway. During the oxidation process,the oxidation mechanisms of SO4·− and HO· radicals on pyrite were similar,both preferentially reacted with S atoms,but due to the coordination number limitation of S atoms,the neighboring Fe atoms at this time had a stronger affinity compared to the radicals,and the preferential oxidation of Fe atoms would further promote the deep oxidation of S atoms. This might be the fundamental reason why the physical phase of FeS2 remained unchanged during the oxidation process. During the experiment,phosphoric acid was used to mask Fe3+,and it could be seen that at lower temperatures,the lower Fe3+ content of iron ions had less influence on the leaching rate,but when the temperature increased,the large amount of Fe3+ production was conducive to the destruction of the S–S bond,and at the same time realized the cyclic conversion between Fe2+/Fe3+,which promoted the generation of free radicals and further enhances the leaching rate. However,the activation mode of energy transfer was still dominant in the whole oxidation process,supplemented by the activation mode of electron transfer with Fe2+ as the electron donor. This indicated that the effect of temperature on PS treatment of cyanide tailings was mainly reflected in the change of the reaction rate constant (k)and Gibbs free energy (ΔG)in the radical generation reaction,which in turn affected pH of the reaction system and the composition of the oxidized substances.

quote

GB/T 7714-2015 [1] Rongyan Zhu, Yonghui Song, Ping Dong, et al. Treatment of Cyanide Tailings with Persulfate Oxidizers at Different Temperatures[J]. Chinese Journal of Rare Metals, 2025, 49(5): 648-656. DOI:10.13373/j.cnki.cjrm.XY23080004.
MLA [1] Rongyan Zhu, et al., "Treatment of Cyanide Tailings with Persulfate Oxidizers at Different Temperatures." Chinese Journal of Rare Metals, vol. 49, no. 5, 2025, pp. 648-656, https://doi.org/10.13373/j.cnki.cjrm.XY23080004.
APA [1] Rongyan Zhu, Yonghui Song, Ping Dong, Long Liao, Ya Wang, & Liang Zhang. (2025). Treatment of Cyanide Tailings with Persulfate Oxidizers at Different Temperatures. Chinese Journal of Rare Metals, 49(5), 648-656. https://doi.org/10.13373/j.cnki.cjrm.XY23080004
IEEE [1] Rongyan Zhu, Yonghui Song, Ping Dong, Long Liao, Ya Wang, and Liang Zhang, "Treatment of Cyanide Tailings with Persulfate Oxidizers at Different Temperatures," Chinese Journal of Rare Metals, vol. 49, no. 5, pp. 648-656, 2025, doi: 10.13373/j.cnki.cjrm.XY23080004. keywords: {cyanide tailings;sodium persulfate;free radicals;oxidation}