Current Development and Preparation Methods of Rapidly Solidified High-silicon Aluminum Alloys AITranslate
Abstract AITranslate
The current development and preparation methods of rapidly solidified high-silicon aluminum loys are introduced,and their development trend is prospected.
KeyWords AITranslate
1王祝堂,田荣璋.铝合金加工手册[M].长沙:中南工业大学出版社,2001.
2甘卫平,陈招科,杨伏良,周兆锋.高硅铝合金轻质电子封装材料研究现状及进展[J].材料导报,2004,18(6):79-82. 被引量:45
3佟林松,樊建中,肖伯律.低热膨胀铝基复合材料的研究进展[J].稀有金属,2008,32(3):375-380. 被引量:23
4李坤,石南林,孙超.碳纤维增强镁基复合材料界面研究进展[J].材料导报,2005,19(F11):425-427. 被引量:9
5张济山.新型喷射成形轻质、高导热、低膨胀Si-Al电子封装材料[J].材料导报,2002,16(9):1-4. 被引量:36
6Jacobsen D M. Spray-formed silicon-aluminum[J]. Ad- vanced Materials Processes, 2000,3 : 36-39.
7German R M,Hens K F,Johnson J L. Powder metal- lurgy processing of thermal management materials for microelectronic applications [J]. International Journal Powder Metallurgy, 1994,30 (2) : 205-215.
8杨培勇,郑子樵,蔡杨,李世晨,冯曦.Si-Al电子封装材料粉末冶金制备工艺研究[J].稀有金属,2004,28(1):160-165. 被引量:28
9黄强,顾明元,金燕萍.电子封装材料的研究现状[J].材料导报,2000,14(9):28-32. 被引量:59
10陈美英.喷射成形新型轻量化电子封装材料Si-A1合金的研究[D].北京:北京科技大学,2003.
1李承娣,沈岩,王永彬,朱峰,金梅,徐久军.化学刻蚀高硅铝合金缸套的摩擦磨损性能[J].中国表面工程,2014,27(6):104-109. 被引量:4
2唐立超,魏子伟,翟彦博.磁场对Al-19wt%Si高硅铝合金离心铸造组织的影响[J].热加工工艺,2018,47(19):101-105. 被引量:2
3董屹盛,吕洪玉.高硅铝合金的研究现状及展望[J].轻合金加工技术,2021,49(2):11-16. 被引量:1
1李承娣,徐佳子,沈岩,金梅,徐久军.表面硅颗粒整形对高硅铝合金缸套摩擦磨损性能的影响[J].中国表面工程,2016,29(6):8-14. 被引量:4
2曾志强,张博,王俊元,祝锡晶,贵凯.Ni基+WC等离子喷焊涂层性能研究[J].粉末冶金工业,2017,27(1):37-41. 被引量:7
3李承娣,金梅,徐久军,沈岩.激光光整对高硅铝合金缸套材料摩擦磨损性能的影响[J].中国表面工程,2017,30(5):89-94. 被引量:1
4刘善勇,王玉玲,孙树峰,邵晶,刘庆玉,王津.高温化学腐蚀加工多孔碳化硅陶瓷的表征及机理[J].航空材料学报,2019,39(2):16-24. 被引量:3
5王旭,冯阳,赵利辉,王正洋,吕启文,董天顺,李国禄.重熔处理对高硅铝涂层组织和性能的影响[J].轻合金加工技术,2020,48(1):40-44. 被引量:3
6李波,刘卓毅,何锦航,苏剑锋,施艳,张志清,刘施峰,卢金科,邵春.电磁铸造对Al-Si12.6%共晶合金微观组织的影响[J].精密成形工程,2023,15(6):62-69.
7马鸿量,符寒光.耐磨材料悬浮铸造技术的研究现状[J].中国铸造装备与技术,2023,58(4):5-13.
1周多三,胡荫森,蒋向阳,陈振华.喷射沉积Al—8Fe—2V—2Si合金的结构和性能研究[J].湖南冶金,1993(4):3-8.
2Maech.,R,周细应.喷射沉积700系列高强铝合金的组织,机械性能及应力...[J].国外金属加工,1992(5):42-46.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.21[金属学及工艺—金属材料]
Citation Information:
The current development and preparation methods of rapidly solidified high-silicon aluminum loys are introduced,and their development trend is prospected.
quote
| GB/T 7714-2015 | [1] ZHANG Li-jun, XIE Jing-pei, WANG Ai-qin. Current Development and Preparation Methods of Rapidly Solidified High-silicon Aluminum Alloys[J]. Rare Metals and Cemented Carbides, 2012(6): 64-67. |
| MLA | [1] ZHANG Li-jun, et al., "Current Development and Preparation Methods of Rapidly Solidified High-silicon Aluminum Alloys." Rare Metals and Cemented Carbides, no. 6, 2012, pp. 64-67. |
| APA | [1] ZHANG Li-jun, XIE Jing-pei, & WANG Ai-qin. (2012). Current Development and Preparation Methods of Rapidly Solidified High-silicon Aluminum Alloys. Rare Metals and Cemented Carbides(6), 64-67. |
| IEEE | [1] ZHANG Li-jun, XIE Jing-pei, and WANG Ai-qin, "Current Development and Preparation Methods of Rapidly Solidified High-silicon Aluminum Alloys," Rare Metals and Cemented Carbides, no. 6, pp. 64-67, 2012. keywords: {high-silicon aluminum alloy;rapid solidification;powder metallurgy;spray deposition} |