daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Ambient Synthesis of Metal–Organic Framework-Derived Bimetallic Layered Double Hydroxide Nanosheets by the Composition Inheritance Strategy for Efficient Microwave Attenuation Applications Ambient Synthesis of Metal–Organic Framework-Derived Bimetallic Layered Double Hydroxide Nanosheets by the Composition Inheritance Strategy for Efficient Microwave Attenuation Applications AITranslate

China|Hangzhou Dianzi University Shangyu Institute of Science and Engineering; Hangzhou Dianzi University; Hangzhou Dianzi University; Nanjing University of Science & Technology; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; China|Hangzhou Dianzi University Shangyu Institute of Science and Engineering; Nanjing University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Layered double hydroxide (LDH) materials have attracted much attention in electromagnetic (EM) wave absorption applications due to their flaky texture and adjustable bimetallic composition. However, the construction of 2D LDH materials, especially metal–organic framework (MOF)-derived LDHs, is usually demanded with high-energy and multi-step processes. Here, the 2D bimetallic Co, Ni-LM nanosheets have been readily prepared by a one-step room-temperature reaction using 2-methylimidazole as an inducer molecule and the interlayer equilibrium substance. The precise molar ratio of Co2+ and Ni2+ in water/methanol is the controlling factor for the formation of MOF-derived LDH nanosheets. In addition, the well-tuned molar ratio can be extended to the preparation of 2D bimetallic Zn, Ni-LM nanosheets by only changing the Co2+ ions to Zn2+ ions, using the same feeding ratio. Then, we apply a temperature-controlled pyrolysis strategy under air to convert Co, Ni-LM and Zn, Ni-LM into their derivatives of Co, Ni-LMc and Zn, Ni-LMc, respectively. Based on the synergistic effects of multi-components and 2D structure, the Co, Ni-LMc material achieves remarkable electromagnetic absorption (EMA) performance, where its maximum width reaches 4.76 GHz with a thickness of 1.9 mm. For Zn, Ni-LMc material, a resonant absorption peak appears around 14.04 GHz for different absorber thicknesses. This work enlightens a facile, green, and environmentally friendly strategy for constructing MOF-derived LDH nanosheets. The unique EM response behavior of the two derivatives also provides us with a positive guidance for the subsequent design of EMA composites to meet the requirements of different application environments.

KeyWords AITranslate

2D nanosheet layer double hydroxides pyrolysis electromagnetic wave absorption metal−organic frameworks
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00718

Chinese Library Classification Number:

Citation Information:

Layered double hydroxide (LDH) materials have attracted much attention in electromagnetic (EM) wave absorption applications due to their flaky texture and adjustable bimetallic composition. However, the construction of 2D LDH materials, especially metal–organic framework (MOF)-derived LDHs, is usually demanded with high-energy and multi-step processes. Here, the 2D bimetallic Co, Ni-LM nanosheets have been readily prepared by a one-step room-temperature reaction using 2-methylimidazole as an inducer molecule and the interlayer equilibrium substance. The precise molar ratio of Co2+ and Ni2+ in water/methanol is the controlling factor for the formation of MOF-derived LDH nanosheets. In addition, the well-tuned molar ratio can be extended to the preparation of 2D bimetallic Zn, Ni-LM nanosheets by only changing the Co2+ ions to Zn2+ ions, using the same feeding ratio. Then, we apply a temperature-controlled pyrolysis strategy under air to convert Co, Ni-LM and Zn, Ni-LM into their derivatives of Co, Ni-LMc and Zn, Ni-LMc, respectively. Based on the synergistic effects of multi-components and 2D structure, the Co, Ni-LMc material achieves remarkable electromagnetic absorption (EMA) performance, where its maximum width reaches 4.76 GHz with a thickness of 1.9 mm. For Zn, Ni-LMc material, a resonant absorption peak appears around 14.04 GHz for different absorber thicknesses. This work enlightens a facile, green, and environmentally friendly strategy for constructing MOF-derived LDH nanosheets. The unique EM response behavior of the two derivatives also provides us with a positive guidance for the subsequent design of EMA composites to meet the requirements of different application environments.

quote

GB/T 7714-2015 [1] Kun Zhang, Zhizhen Xu, Yuting Li, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00718.
MLA [1] Kun Zhang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00718.
APA [1] Kun Zhang, Zhizhen Xu, Yuting Li, Siyao Cheng, Xiaoyu Zhao, Yaxin Wang, Fengyi Zhang, Xiaojie Guo, Yongjun Zhang, & Aming Xie. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00718
IEEE [1] Kun Zhang, Zhizhen Xu, Yuting Li, Siyao Cheng, Xiaoyu Zhao, Yaxin Wang, Fengyi Zhang, Xiaojie Guo, Yongjun Zhang, and Aming Xie, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00718. keywords: {2D nanosheet layer double hydroxides pyrolysis electromagnetic wave absorption metal−organic frameworks}