daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Determination of Trace Impurity Elements in the Li-Pb Alloy AITranslate

Institute of Nuclear Physics and Chemistry, China Institute of Engineering Physics;Institute of Nuclear Physics and Chemistry, China Institute of Engineering Physics;Institute of Nuclear Physics and Chemistry, China Institute of Engineering Physics
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The content of trace impurity elements-Fe,Na,Al, Mg-in the alloy Li17 Pb83 was measured by inductively coupled plasma emission spectroscopy (ICP-AES). The optimization of measuring parameters was explored as well as the type and dosage of acid. And the interference effect of coexistent elements on the analysis result was also studied. The results show that the mass fractions of Fe,Na,AI,Mg in Li17Pb83 are respectively 0. 003%,0. 005 8%,0. 002 6% and 0. 002% ,when carrier gas pressure is 0.25 MPa,generator power 1.3 k W,observation height 10 mm above the coil, the volume ratio of hydrochloric acid to nitric acid 4 : 1 and the total acid concentration 10%.

KeyWords AITranslate

Li17 Pb83 alloy impurity element ICP-AES measuring condition

1吴宜灿,汪卫华,刘松林,李静惊,王红艳,陈红丽,陈明亮,张士杰,黄群英,黄德所,郑善良,曾勤,胡丽琴,柏云清,章毛连,李艳芬,李春京,冯岩,宋勇,龙鹏成,FDS课题组.聚变发电反应堆概念设计研究[J].核科学与工程,2005,25(1):76-85. 被引量:47

2谢波,杨通在,胡睿.液态锂锡合金氚增殖行为的理论分析[J].核技术,2008,31(8):608-612. 被引量:7

3李静惊,曾勤,吴宜灿.聚变发电反应堆双冷液态锂铅包层氚增殖中子学分析研究[J].核科学与工程,2005,25(1):86-90. 被引量:3

1谢波,古梅,肖成建.锂铅合金样品的初步活化理论分析[J].稀有金属与硬质合金,2011,39(2):47-49.

2谢波,吴宜灿,陈晓军,翁葵平,刘俊,肖成建,FDS团队.锂铅合金释氚实验研究[J].原子核物理评论,2011,28(3):371-376. 被引量:2

1梅华平,魏世平,何梅生.聚变堆氚材料衡算测量系统研究初探[J].核安全,2021,20(4):51-55.

2韩佳佳,汪卫华,浦文婧,江海燕,储德林,史博.矩形管道载氚热磁流体输运特性的数值模拟研究[J].核聚变与等离子体物理,2023,43(2):161-168.

1蔡翠侨,吴天良.ICP—AES法测定氧化钴中主成分Co和杂质元素Fe、Ni、Mn、Cu含量[J].光谱仪器与分析,2001(4):1-6. 被引量:5

2杨晶秋,孙晓红.ICP-AES法测定工业硅中杂质含量[J].中国新技术新产品,2009(16):18-18. 被引量:3

3侯列奇,李洁,王树安,卢菊生.电感耦合等离子体-原子发射光谱法测定银中22种微量元素[J].光谱实验室,2007,24(3):299-302. 被引量:14

4靳芳,李吉生,杨生宏,邢红.ICP-MS测定碳酸锂中微量元素[J].光谱实验室,2011,28(4):1710-1712. 被引量:3

5顾战平,徐建平,丁溪萍,储燕萍,夏琴.石墨炉原子吸收分光光度法测定地表水中的锑[J].环境监测管理与技术,2010,22(6):64-65. 被引量:5

6王昌钊,张遴.ICP-AES法测定玻璃器皿中铅、镉、砷、锑溶出量的研究[J].化学分析计量,2012,21(4):50-52. 被引量:10

7王铁,亢德华,于媛君,闫晓军.ICP-AES法测定铅合金中的Cu、As、Bi、Sn、Sb[J].鞍钢技术,2013(4):37-39.

8墨淑敏.原子发射光谱法直接测定焦炭中的15种微量杂质元素[J].光谱实验室,2009,26(2):367-369. 被引量:6

9鲁琳.精硒中微量杂质元素的发射光谱法测定[J].铜业工程,1998,0(2):58-60.

10郝原芳,刘新,宋丽华,李丽君,徐英奎.电感耦合等离子体质谱法测定铅合金中的微量杂质元素镉和锡[J].岩矿测试,2016,35(4):378-383. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:O657.2[理学—分析化学]

Citation Information:

The content of trace impurity elements-Fe,Na,Al, Mg-in the alloy Li17 Pb83 was measured by inductively coupled plasma emission spectroscopy (ICP-AES). The optimization of measuring parameters was explored as well as the type and dosage of acid. And the interference effect of coexistent elements on the analysis result was also studied. The results show that the mass fractions of Fe,Na,AI,Mg in Li17Pb83 are respectively 0. 003%,0. 005 8%,0. 002 6% and 0. 002% ,when carrier gas pressure is 0.25 MPa,generator power 1.3 k W,observation height 10 mm above the coil, the volume ratio of hydrochloric acid to nitric acid 4 : 1 and the total acid concentration 10%.

quote

GB/T 7714-2015 [1] XIE Bo, WU Xi, WENG Kui-ping. Determination of Trace Impurity Elements in the Li-Pb Alloy[J]. Rare Metals and Cemented Carbides, 2009(3): 29-32.
MLA [1] XIE Bo, et al., "Determination of Trace Impurity Elements in the Li-Pb Alloy." Rare Metals and Cemented Carbides, no. 3, 2009, pp. 29-32.
APA [1] XIE Bo, WU Xi, & WENG Kui-ping. (2009). Determination of Trace Impurity Elements in the Li-Pb Alloy. Rare Metals and Cemented Carbides(3), 29-32.
IEEE [1] XIE Bo, WU Xi, and WENG Kui-ping, "Determination of Trace Impurity Elements in the Li-Pb Alloy," Rare Metals and Cemented Carbides, no. 3, pp. 29-32, 2009. keywords: {Li17 Pb83 alloy;impurity element;ICP-AES;measuring condition}