Corrosion Behavior of Annealed Ti35 Alloy in Concentrated Nitric Acid AITranslate

School of Metallurgy Engineering, Xi'an University of Architecture and Technology;School of Metallurgy Engineering, Xi'an University of Architecture and Technology;School of Metallurgy Engineering, Xi'an University of Architecture and Technology;School of Metallurgy Engineering, Xi'an University of Architecture and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ti35alloy bar was annealed at 700 ℃for 8h,and then investigated by full immersion corrosion tests and polarization curves and electrochemical impedance spectroscopy in 8mol/L nitric acid.The experimental results show that through a long time of annealing,the grain size of Ti35 alloy bar obviously increases,its corrosion current density decreases,impedance arc radius significantly increases,phase angle platform broadens and modulus value increases,resulting in its corrosion resistance greatly improved in concentrated nitric acid.

KeyWords AITranslate

titanium alloy annealing corrosion resistance concentrated nitric acid

1Yamamot T, Tsukul S, Okamoto S, et al. Gamma-ray ir- radiation effect on corrosion rates of stainless steel, Ti and Ti-5Ta in boiling 9N nitric acid[J]. Journal of Nu- clear Materials, 1996,228(2) : 162-167.

2Sano Y, Takeuchi M, Nakajima Y, et al. Effect of metal ions in a heated nitric acid solution on the corrosion be- havior of a titanium-5% tantalum alloy in the hot nitric acid condensate[J]. Journal of Nuclear Materials, 2013, 432(1-3) :475-481.

3吴志林,吴多祥,袁人枢,赵磊,赵言宝.热处理对静液挤压AZ80镁合金管材腐蚀行为的影响[J].中国有色金属学报,2015,25(2):301-307. 被引量:8

4朱梅生,刘建章,李中奎,宋启忠.热处理对新锆合金在蒸汽中腐蚀性能的影响[J].稀有金属材料与工程,1997,26(4):40-44. 被引量:8

5Mardare A I,Savan A, Ludwig A,et al. A combinatorial passivation study of Ta-Ti alloys[J]. Corrosion Science, 2009,51(7) :1 519-1 527.

6Shankar A R, Dayal R K, Balasubramaniam R, et al. Effect of heat treatment on the corrosion behaviour of Ti-5Ta-1.8 Nb alloy in boiling concentrated nitric acid [J]. Journal of Nuclear Materials, 2008,372 (2-3) : 277- 284.

7杨英丽,赵彬,林桥,殷京瓯,苏航标.冷加工率对Ti-35合金组织性能的影响[J].钛工业进展,2004,21(6):22-24. 被引量:11

1霍东兴,梁精龙,李慧,谢珊珊,杨宇.钛合金腐蚀的研究进展[J].热加工工艺,2017,46(20):29-31. 被引量:1

2杨帆,吴金平,郭荻子,赵彬,罗媛媛.Ti-Ta合金在硝酸中电化学腐蚀研究[J].钛工业进展,2018,35(2):22-25. 被引量:6

3徐建平,苏航标,郭荻子,吴金平,王晓,赵永庆,许并社.核乏燃料后处理设备用钛合金腐蚀性能研究进展[J].稀有金属与硬质合金,2019,47(3):36-41. 被引量:2

4郝晓博,刘茵琪,李渤渤,张强.船舶用Ti70合金在人工海水中的腐蚀行为研究[J].腐蚀科学与防护技术,2019,31(1):27-32. 被引量:3

5洪圆,王倜嘉,徐磊.Ti35钛合金焊接接头在硝酸中腐蚀电化学研究[J].山西化工,2022,42(3):16-18.

1王浩楠,李争显,王彦峰,姬寿长,刘林涛.钛表面钛钯合金层耐蚀性能及耐蚀机理研究[J].钛工业进展,2018,35(6):41-45.

2熊艳杰,徐大鹏,程赵辉,魏敬鹏.铸态和烧结态AlCoCrFeNi高熵合金模拟海水腐蚀性能研究[J].西安工业大学学报,2020,40(1):76-81. 被引量:2

3郝晓博,李渤渤,刘茵琪,张强,李洋.Ti70合金板的组织与力学性能的各向异性[J].金属热处理,2020,45(8):34-38. 被引量:7

4王帆,李娟,李金灵,鱼涛,屈撑囤,朱世东,李彦.金属管道在CO_(2)/H_(2)S环境中的腐蚀行为[J].热加工工艺,2021,50(4):1-7. 被引量:16

5张银,康敏,李恒征,刘运通,金美付,Nyambura Samuel Mbugua.Ni-Co-P合金镀层显微硬度及其耐海水腐蚀性[J].材料科学与工程学报,2021,39(3):384-392. 被引量:3

6刘星,冉斗,孟惠民,李全德,巩秀芳,隆彬.表面状态对TC4钛合金的耐蚀性影响[J].中国腐蚀与防护学报,2021,41(6):828-836. 被引量:2

7许瑾璐.框架结构用螺纹钢中温锌锰系磷化及封闭处理[J].兵器材料科学与工程,2021,44(6):15-20. 被引量:1

8张春龙,董永昌,吕丹,宋凤丽,陈思喆,徐春艳,刘新华.日本乏燃料后处理厂设备腐蚀研究及启示[J].核化学与放射化学,2022,44(6):575-588.

9李文桔,张慧霞,张宏泉,郝福耀,仝宏韬.温度对钛合金应力腐蚀行为的影响[J].中国腐蚀与防护学报,2023,43(1):111-118.

10李博,史新鑫,齐风华,田德厚,张玉国,王照国.Ti70合金板热成型组织性能研究[J].科技创新与应用,2023,13(9):69-72.

1阮健,毛小南,杨义,冯亮.固溶温度对Ti35合金显微组织的影响[J].热加工工艺,2012,41(20):209-211. 被引量:1

2杨英丽,罗媛媛,吴金平,郭荻子,赵彬,赵恒章,苏航标.耐蚀钛合金Ti35管材微观结构分析[J].钛工业进展,2010,27(6):20-23. 被引量:5

3宋飞飞,吴金平,杨英丽,赵彬,罗媛媛,郭荻子.Ti35合金管材数控弯曲成形规律有限元模拟研究[J].钛工业进展,2015,32(4):17-21.

4陈锋,王煜.Sn、Zr、Mo对Ti35Nb基合金组织与力学性能的影响[J].中国有色金属学报,2013,23(6):1560-1566. 被引量:3

5李培友,王永善,孟凡莹,任晓妮,刘锦.Ti_(35.37)Cu_(45.11)Ni_(8.88)Zr_(10.64)金属玻璃锯齿流变应力降对剪切带扩展的影响[J].陕西理工学院学报:自然科学版,2015,31(5):1-4. 被引量:3

6商佳程,王晓敏,盛钟琦.Ti35钛合金与低碳不锈钢在硝酸溶液中的电化学腐蚀对比研究[J].中国核科技报告,2006(1):14-20. 被引量:2

7郭荻子,杨英丽,赵彬,赵恒章,吴金平,苏航标.Ti35合金在沸腾硝酸中钝化膜及过渡层形成及组成分析[J].钛工业进展,2015,32(1):38-41. 被引量:2

8林建国,张云飞,马蓦.Preparation of porous Ti35Nb alloy and its mechanical properties under monotonic and cyclic loading[J].中国有色金属学报:英文版,2010,20(3):390-394. 被引量:2

9杨专钊,刘道新,张晓化.钛及钛合金的缝隙腐蚀行为[J].腐蚀与防护,2013,34(4):295-297. 被引量:11

10王玉会,张晖,张旺峰,颜孟奇,李野.TiNbTaZr钛合金冷加工塑性行为研究[J].航空材料学报,2014,34(4):147-152. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]

Citation Information:

Ti35alloy bar was annealed at 700 ℃for 8h,and then investigated by full immersion corrosion tests and polarization curves and electrochemical impedance spectroscopy in 8mol/L nitric acid.The experimental results show that through a long time of annealing,the grain size of Ti35 alloy bar obviously increases,its corrosion current density decreases,impedance arc radius significantly increases,phase angle platform broadens and modulus value increases,resulting in its corrosion resistance greatly improved in concentrated nitric acid.

quote

GB/T 7714-2015 [1] YANG Fan, JU Jian-hui, MAO Xiao-nan, et al. Corrosion Behavior of Annealed Ti35 Alloy in Concentrated Nitric Acid[J]. Rare Metals and Cemented Carbides, 2016(1): 47-49.
MLA [1] YANG Fan, et al., "Corrosion Behavior of Annealed Ti35 Alloy in Concentrated Nitric Acid." Rare Metals and Cemented Carbides, no. 1, 2016, pp. 47-49.
APA [1] YANG Fan, JU Jian-hui, MAO Xiao-nan, & WU Jin-ping. (2016). Corrosion Behavior of Annealed Ti35 Alloy in Concentrated Nitric Acid. Rare Metals and Cemented Carbides(1), 47-49.
IEEE [1] YANG Fan, JU Jian-hui, MAO Xiao-nan, and WU Jin-ping, "Corrosion Behavior of Annealed Ti35 Alloy in Concentrated Nitric Acid," Rare Metals and Cemented Carbides, no. 1, pp. 47-49, 2016. keywords: {titanium alloy;annealing;corrosion resistance;concentrated nitric acid}