Hydrothermal Synthesis and Luminescent Properties of Co2+ Doped YPO_4:Eu3+ Phosphors AITranslate

School of Chemistry and Materials Science, Guizhou Normal University;School of Chemistry and Materials Science, Guizhou Normal University;School of Chemistry and Materials Science, Guizhou Normal University;School of Chemistry and Materials Science, Guizhou Normal University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Co2+doped YPO4:Eu3+phosphors were successfully synthesized with hydrothermal method.The crystal structure,element valence state and luminescent properties of the as-synthesized samples were investigated by XRD,XPS,FT-IR and FL.The results show that all the samples from hydrothermal synthesis are single-phase Co2+doped YPO4:Eu3+crystals with tetragonal xenotime structure,they can effectively emit characteristic orange-red luminescence of Eu3+with UV light excitation,and the fluorescence lifetime is approximately 4.6ms.A small amount of Co2+and Eu3+codoping has less influence on phase composition and crystal structure of product matrix,but has a significant impact on its luminescent properties.The intensity of emission peak located at 595 nm of YPO4:2%Eu3+,0.10 %Co2+sample is about 21.1%higher than that of YPO4:2%Eu3+sample.

KeyWords AITranslate

YPO4:Eu3+ Co2+ doping hydrothermal synthesis luminescent property

1Ye S, Xiao F, Pan Y X, et al. Phosphors in phosphor- converted white light-emitting diodes= Recent advances in materials, techniques and properties[J]. Materials Sci- ence & Engineering R,2010,71(1):1-34.

2Rodriguez-Liviano Sonia, Aparicio Francisco J, Rojas Te- resa C,et al. Microwave-assisted synthesis and lumines- cence of mesoporous RE-doped YPO4 (RE=Eu,Ce,Tb, and Ceq-Tb) nanophosphors with lenticular shape[J]. Crystal Growth & Design,2011,12(2) :635-645.

3Chen Jiangchao, Meng Qingguo, May P Stanley, et al. Sensitization of Eu3+ luminescence in Eu: YPO4 nano- crystals[J]. The Journal of Physical Chemistry C, 2013, 117(11) :5 953-5 962.

4杨锦瑜,罗林,苏玉长,申婧.高分子凝胶法合成YPO4:Sm^(3+)纳米荧光材料的结构与光学性能[J].粉末冶金材料科学与工程,2014,19(3):493-498. 被引量:6

5Zheng Wei,Zhu Haomiao,Li Renfu, et al. Visible-to-in- frared quantum cutting by phonon-assisted energy trans- fer in YPO4 :Tm3+ ,Yb3: phosphors[J]. Physical Chem- istry Chemical Physics,2012,14(19) :6 974-6 980.

6Angiuli F, Cavalli E, Belletti A. Synthesis and spectro- scopic characterization of YPOactivated with Tb3+ and effect of Bia+ co-doping on [J]. Journal of Solid State the luminescence properties Chemistry, 2012,192: 289-295.

7Huang Jinsong, Gao Rui, Lu Zhouguang, et al. Sol- gel preparation and photoluminescence enhancement of Li+ and Eu3+ Co- doped YPO4 nanophosphors[J]. Optical Materials, 2010,32(9) :857-861.

8Balakrishnaiah R,Kim Dong Woo, Yi Soung Soo,et al. Effect of AP+ ions on fluorescence properties of YPO4 Eu3+ phosphors[J]. Materials Letters, 2009, 63 (23) : 2 063-2 066.

9Parchur A K, Ningthoujam R S. Preparation, microstruc- ture and crystal structure studies of Li+ co- doped YPO4 : Eu3+[J]. RSC Advances, 2012,2 (29) : 10 854- 10 858.

10王达君,夏上达,尹民.Ab initio calculation of electronic structures and 4f-5d transitions of some rare earth ions doped in crystal YPO_4[J].稀土学报:英文版,2008,26(3):439-442. 被引量:1

1付兵,欧娅,刘欢,顾曼琦,陈卓,杨锦瑜.Ba^(2+)共掺杂YPO_4∶Tb^(3+)荧光材料的水热合成与荧光性能[J].材料导报,2017,31(18):16-20. 被引量:4

2刘欢,陈健,付兵,杨锦瑜.Sr^(2+)共掺杂YPO_4:Eu^(3+)发光材料的水热合成及其性能[J].有色金属工程,2018,8(2):54-58. 被引量:3

3付兵,郑义.LaPO_(4):Eu^(3+)/Ba^(2+)荧光材料的制备及其性能探究[J].山东化工,2023,52(10):27-29.

4郑义,付兵.Sr^(2+)共掺杂LaPO_(4):Tb^(3+)发光材料的水热合成与性能[J].山东化工,2023,52(10):50-53.

5欧娅,付兵,朱莉萍,陈雪羽,杨锦瑜.共沉淀法制备Eu^(3+)掺杂La_3PO_7荧光材料及其性能[J].中国有色金属学报,2017,27(5):974-980. 被引量:7

1孟晓燕,彭思艳,王学军,罗伟,孙宇杰,杨流赛.YPO_4:Ln^(3+)(Ln=Eu,Tb)球形荧光粉的合成及其发光性能优化[J].光电子.激光,2018,29(11):1187-1193. 被引量:5

2李娟,黄一男,李蓝苹,李慧玲,陈雪羽,杨锦瑜.共沉淀法制备Y_3PO_7∶Tb^(3+)荧光材料及其性能[J].人工晶体学报,2018,47(11):2344-2349. 被引量:1

3薛同站,李卫华,伍鲧,申慧彦,薛莉娉.污水厂尾水及受纳河流样品溶解有机物(DOM)的分子光谱解析及识别[J].生态与农村环境学报,2018,34(12):1131-1138. 被引量:4

4黄婷,许广西,连景宝,吴念初,张雪,何娇.Gd2O2SO4:Tb3+纳米荧光粉的共沉淀合成及光致发光[J].有色金属工程,2019,9(6):17-23.

5赵文华,魏智强,梁家浩,马龙,张旭东,姜金龙.Cr掺杂SnS2纳米花的微观结构与光学性能[J].中国有色金属学报,2019,29(8):1693-1700.

6李蓝苹,李慧玲,张玲,饶啟亮,张丽君,杨锦瑜.Y2P4O13:Eu^3+荧光材料的制备及其性能[J].有色金属工程,2020,10(3):7-12.

7李慧玲,李蓝苹,饶啟亮,张玲,陈雪羽,邹海凤,杨锦瑜.Er^3+/Yb^3+共掺杂YPO4上转换发光材料的制备与性能[J].中国有色金属学报,2020,30(6):1349-1357. 被引量:2

8张玲,饶啟亮,郭海瑞,朱浩天,朱莉萍,杨锦瑜.单基质白光荧光粉Gd3PO7∶Dy3+的制备及其性能研究[J].稀有金属与硬质合金,2020,48(5):41-47.

9鲁雅,张敏芝,梁刚锋,李春霞,赵国良.LiSrBO_(3):Bi^(3+)/RE^(3+)(RE=Sm,Eu,Tb)荧光粉的合成与发光性能[J].中国有色金属学报,2021,31(7):1879-1890. 被引量:1

10付兵.Ca^(2+)共掺杂LaPO_(4)∶Tb^(3+)荧光材料的水热合成与性能[J].山东化工,2021,50(17):70-71. 被引量:1

1崔丽华,王岩,舒霞,崔接武,张勇,吴玉程.MnO_2/TiO_2复合物电极的制备及超级电容性能[J].复合材料学报,2016,33(8):1794-1802. 被引量:5

2适合摄影的绝佳时刻[J].新青年:珍情,2014,0(10):64-64.

3杨锦瑜,罗林,苏玉长,申婧.高分子凝胶法合成YPO4:Sm^(3+)纳米荧光材料的结构与光学性能[J].粉末冶金材料科学与工程,2014,19(3):493-498. 被引量:6

4胡正龙,顾豪爽,胡永明,周迪,邹亚囡.Bi_(3.15)Nd_(0.85)Ti_3O_(12)纳米结构的制备与XPS研究[J].压电与声光,2009,31(6):868-870.

5杨锦瑜,罗林,刘雪颖,苏玉长.Eu^(3+)掺杂RE_2Sn_2O_7(RE=La,Gd,Y)纳米荧光材料的水热合成与发光性能[J].中国有色金属学报,2014,24(4):1036-1040. 被引量:3

6杨锦瑜,罗林,刘雪颖.Eu3+掺杂Re2Sn207(Re=La,Gd,Y)纳米荧光材料的水热合成与发光性能[J].纳米科技,2013,10(5):56-60.

7吴敏涛.相机[J].年轻人:B版(魅力校园),2015,0(11):124-124.

8刘晓明,李洪涛,李美成,赵连城.低温退火对InAsSb材料结构特性的影响[J].稀有金属材料与工程,2009,38(A02):606-608.

9张效华,辛凤,胡跃辉,陈义川,杨丰.不同衬底温度下生长的Bi_(1.5)Zn_(1.0)Nb_(1.5)O_(7.0)薄膜的XPS研究[J].真空科学与技术学报,2013,33(5):415-418. 被引量:2

10王海斗,卢晓亮,李国禄,徐滨士,邢志国.超音速等离子喷涂BaTiO_3涂层的制备及表征[J].功能材料,2013,44(5):731-735. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]

Citation Information:

Co2+doped YPO4:Eu3+phosphors were successfully synthesized with hydrothermal method.The crystal structure,element valence state and luminescent properties of the as-synthesized samples were investigated by XRD,XPS,FT-IR and FL.The results show that all the samples from hydrothermal synthesis are single-phase Co2+doped YPO4:Eu3+crystals with tetragonal xenotime structure,they can effectively emit characteristic orange-red luminescence of Eu3+with UV light excitation,and the fluorescence lifetime is approximately 4.6ms.A small amount of Co2+and Eu3+codoping has less influence on phase composition and crystal structure of product matrix,but has a significant impact on its luminescent properties.The intensity of emission peak located at 595 nm of YPO4:2%Eu3+,0.10 %Co2+sample is about 21.1%higher than that of YPO4:2%Eu3+sample.

quote

GB/T 7714-2015 [1] CENG Xiao-dao, JIA Xiao-hui, ZHU Li-ping, et al. Hydrothermal Synthesis and Luminescent Properties of Co2+ Doped YPO_4:Eu3+ Phosphors[J]. Rare Metals and Cemented Carbides, 2016(1): 50-55.
MLA [1] CENG Xiao-dao, et al., "Hydrothermal Synthesis and Luminescent Properties of Co2+ Doped YPO_4:Eu3+ Phosphors." Rare Metals and Cemented Carbides, no. 1, 2016, pp. 50-55.
APA [1] CENG Xiao-dao, JIA Xiao-hui, ZHU Li-ping, & YANG Jin-yu. (2016). Hydrothermal Synthesis and Luminescent Properties of Co2+ Doped YPO_4:Eu3+ Phosphors. Rare Metals and Cemented Carbides(1), 50-55.
IEEE [1] CENG Xiao-dao, JIA Xiao-hui, ZHU Li-ping, and YANG Jin-yu, "Hydrothermal Synthesis and Luminescent Properties of Co2+ Doped YPO_4:Eu3+ Phosphors," Rare Metals and Cemented Carbides, no. 1, pp. 50-55, 2016. keywords: {YPO4:Eu3+;Co2+ doping;hydrothermal synthesis;luminescent property}