Research on Diamond Coating Preparation and Milling Characteristics of Cemented Carbide Tools with Complex Shape AITranslate

School of Mechanical and Power Engineering, Henan University of Technology;School of Mechanical and Power Engineering, Henan University of Technology;School of Mechanical and Power Engineering, Henan University of Technology;School of Mechanical and Power Engineering, Henan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Micron-sized diamond films were uniformly deposited on the surface of cemented carbide vertical keyway milling tools with complex shape by hot filament chemical vapor deposition,where parallel hot filament arrangement and optimized processes of pretreatment and deposition were adopted.SEM and Raman spectra were employed to study morphology and composition of the diamond films.Milling experiments were carried out with high volume fraction(65%)SiCP/Al composite as the workpiece material.And milling characteristics were investigated and compared between diamond film coated milling tools and uncoated milling tools.The results show that with the same milling parameters,cutting force of diamond film coated milling tools is reduced by 20%~60% compared with uncoated milling tools.With high surface adhesion strength,diamond films effectively reduce tool wear and increase tool life by 3~5 times.During early processing,surface quality of the workpieces from uncoated tools is better,but rapidly deteriorates during later processing.In contrast,surface quality of the workpieces from diamond film coated tools is more stable.

KeyWords AITranslate

cemented carbide tool with complex shape diamond coating hot filament chemical vapor deposition SiCP/Al composite milling characteristic

1薛宏国,孙方宏,马玉平,陈明.高性能超细晶粒金刚石涂层刀具制备及试验研究[J].人工晶体学报,2006,35(6):1251-1256. 被引量:7

2孙方宏,陈明,张志明,沈荷生.高性能CVD金刚石薄膜涂层刀具的制备和试验研究[J].机械工程学报,2003,39(7):101-106. 被引量:25

3Sun F H,Zhang Z M,Chen M,etal. Improvement of ad- hesive strength and surface roughness of diamond films on Co-cemented tungsten carbide tools[J]. Diamond and Related Materials, 2003,12 ( 3-7 ), 711-718.

4许幸新,张晓辉,张春林,郑友益.硬质合金成形铣刀的金刚石涂层热应力分析[J].金刚石与磨料磨具工程,2013,33(5):48-52. 被引量:4

5沈彬,孙方宏,薛宏国,陈明,张志明.高性能复杂形状金刚石薄膜涂层刀具的制备和切削性能研究[J].中国机械工程,2008,19(19):2287-2291. 被引量:11

1徐银超,陈康华,王社权,陈响明,李园园,陈送义.金刚石涂层硬质合金刀具涂层的研究和应用进展[J].硬质合金,2015,32(2):136-146. 被引量:16

1刘士嘉,鞠洪博,许俊华,喻利花.涂层技术与硬质涂层材料的研究现状[J].上海电气技术,2022,15(1):66-69. 被引量:1

2刘战强,杨东,王兵.高效切削与高完整性加工技术[J].航空制造技术,2016,59(7):36-43. 被引量:1

3汪兵兵,周建平,许燕,姜宏.短电弧铣削工具电极材料的放电性能研究[J].制造技术与机床,2016(5):94-98. 被引量:9

4臧健,赵军,李安海,王福增.导热系数对钛合金切削绝热剪切影响的有限元模拟[J].硬质合金,2016,33(3):181-187. 被引量:2

5孙轼龙,朱学明,任保民.金刚石涂层刀具铣削氧化锆义齿性能研究[J].硬质合金,2016,33(5):342-349.

6晏超仁,陈燕,郑凯,梁宇红.钎焊金刚石铣磨刀具磨粒粒度尺寸与排布间距对CFRP磨削质量的影响[J].金刚石与磨料磨具工程,2017,37(4):6-10. 被引量:1

7刘伟,满卫东,吕继磊,孙洁,曹阳,江南.植晶工艺对金刚石涂层硬质合金刀具切削性能的影响[J].硬质合金,2017,34(3):167-173. 被引量:5

8熊超,李烈军,苏东艺,彭继华.预处理对金刚石薄膜质量及结合力的影响[J].表面技术,2018,47(1):203-210. 被引量:9

9曹阳,满卫东,吕继磊,刘伟,孙洁,江南.碳化硅衬底沉积高取向金刚石薄膜[J].硬质合金,2017,34(6):407-412. 被引量:1

10闫广宇,吴玉厚,赵德宏,王贺,陆峰.CVD金刚石涂层刀具高效铣削天然理石的切削特性实验研究[J].润滑与密封,2018,43(7):52-57. 被引量:2

1张晓辉,许幸新,张春林,向道辉,郑友益.YT15硬质合金成形铣刀的金刚石涂层制备及应用研究[J].制造技术与机床,2014(10):107-111. 被引量:2

2李刚,王扬渝,周浩东.拼接淬硬钢铣削特性有限元模拟[J].工具技术,2014,48(5):24-27.

3张晓辉,许幸新,张春林,向道辉,郑友益.YT类硬质合金金刚石涂层成形刀具对高体积分数SiC_P/Al复合材料的铣削特性研究[J].稀有金属与硬质合金,2014,42(5):60-64. 被引量:1

4许幸新,张晓辉,向道辉,赵波.复杂形状硬质合金刀具沉积金刚石薄膜涂层过程的热丝分布研究[J].稀有金属与硬质合金,2016,44(6):68-72. 被引量:2

5新型键槽铣刀[J].工具技术,1996,30(10):27-27. 被引量:1

6舒彪,何宁,武凯.氮气介质下钛合金铣削特性的分析研究[J].航空精密制造技术,2002,38(6):16-19. 被引量:1

7宋亚林,程敏.热丝化学气相沉积(HFCVD)制备金刚石薄膜涂层刀具[J].鄂州大学学报,2013,20(3):78-80. 被引量:5

8唐华生.金刚石薄膜涂层技术的发展[J].润滑与密封,1990(5):58-61.

9赵齐,代明江,韦春贝,邱万奇,侯惠君.钨丝到基体表面距离对HFCVD金刚石薄膜质量的影响[J].材料导报,2013,27(22):22-25. 被引量:2

10许幸新,张晓辉,张春林,郑友益.CVD金刚石涂层刀具铣削高体分SiCp/Al复合材料特性研究[J].现代制造工程,2014(7):71-76. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG711[金属学及工艺—刀具与模具]

Citation Information:

Micron-sized diamond films were uniformly deposited on the surface of cemented carbide vertical keyway milling tools with complex shape by hot filament chemical vapor deposition,where parallel hot filament arrangement and optimized processes of pretreatment and deposition were adopted.SEM and Raman spectra were employed to study morphology and composition of the diamond films.Milling experiments were carried out with high volume fraction(65%)SiCP/Al composite as the workpiece material.And milling characteristics were investigated and compared between diamond film coated milling tools and uncoated milling tools.The results show that with the same milling parameters,cutting force of diamond film coated milling tools is reduced by 20%~60% compared with uncoated milling tools.With high surface adhesion strength,diamond films effectively reduce tool wear and increase tool life by 3~5 times.During early processing,surface quality of the workpieces from uncoated tools is better,but rapidly deteriorates during later processing.In contrast,surface quality of the workpieces from diamond film coated tools is more stable.

quote

GB/T 7714-2015 [1] XU Xing-xin, ZHANG Xiao-hui, ZHANG Chun-lin, et al. Research on Diamond Coating Preparation and Milling Characteristics of Cemented Carbide Tools with Complex Shape[J]. Rare Metals and Cemented Carbides, 2014(3): 63-68.
MLA [1] XU Xing-xin, et al., "Research on Diamond Coating Preparation and Milling Characteristics of Cemented Carbide Tools with Complex Shape." Rare Metals and Cemented Carbides, no. 3, 2014, pp. 63-68.
APA [1] XU Xing-xin, ZHANG Xiao-hui, ZHANG Chun-lin, & ZHENG You-yi. (2014). Research on Diamond Coating Preparation and Milling Characteristics of Cemented Carbide Tools with Complex Shape. Rare Metals and Cemented Carbides(3), 63-68.
IEEE [1] XU Xing-xin, ZHANG Xiao-hui, ZHANG Chun-lin, and ZHENG You-yi, "Research on Diamond Coating Preparation and Milling Characteristics of Cemented Carbide Tools with Complex Shape," Rare Metals and Cemented Carbides, no. 3, pp. 63-68, 2014. keywords: {cemented carbide tool with complex shape;diamond coating;hot filament chemical vapor deposition;SiCP/Al composite;milling characteristic}