Study on Improvement of Paraffin as the Molding Agent of Cemented Carbide AITranslate
Abstract AITranslate
Type selection and amount of paraffin molding agent were studied,and improvements were made for the shortcomings of the paraffin.There are two main ways to improve paraffin:one is adding the right amount of higher fatty acids into paraffin and the other is adding the right amount of surfactants into paraffin.Paraffin viscosity and pellet rigidity are improved by improving paraffin molding agent,so that the pressing pressure is reduced,the strength of compacts increases,and the cracks are effectively reduced without significant effect on the magnetic saturation,coercivity and flexural strength of the products,resulting in very good applications of the improved paraffin in cemented carbide production and research.
KeyWords AITranslate
1陈双琳,付坤,周建华.树脂基成形剂的开发与应用研究[J].凿岩机械气动工具,2013,39(1):46-49. 被引量:1
2吴玉霜,孙宝琦,吴国龙.不同种类合成橡胶作为硬质合金成形剂的实验研究[J].稀有金属与硬质合金,1998,26(1):21-24. 被引量:7
3吴玉霜,孙宝琦.新型成形剂的开发与应用研究[J].粉末冶金技术,1993,11(4):266-270. 被引量:5
4唐楷,颜杰,黄新,姜宁.新型石蜡基成形剂的应用性实验研究[J].硬质合金,2008,25(1):28-31. 被引量:12
5郑国梁,郑郴.硬质合金成形剂的现状与发展趋势[J].稀有金属与硬质合金,1992,20(2):39-41. 被引量:11
6Zaky M T,Soliman F S,Farag A S. Influence of paraffin wax characteristics on the formulation of wax- based binders and their debinding fromgreen molded parts using two comparative techniques [J]. J Mater Proc Techn,2009,209(18-19):5 981-5 989.
1韩亚刚,时凯华,顾金宝,董凯林,曾伟.硬质合金模压成型剂的研究进展[J].四川冶金,2019,41(5):2-5.
2刘娟,刘安虎,刘雅璇,罗丹.56#石蜡和PEG4000对硬质合金数控刀片成型性能的影响[J].硬质合金,2023,40(2):134-139.
3陈成艺.石蜡成形剂改性对硬质合金影响的研究[J].福建冶金,2016,45(5):42-45. 被引量:1
1韩亚刚,时凯华,顾金宝,董凯林,曾伟.硬质合金模压成型剂的研究进展[J].四川冶金,2019,41(5):2-5.
1张梅琳,朱世根,朱守星.超细及纳米硬质合金中碳含量的变化及对组织性能的影响[J].材料导报,2006,20(8):65-68. 被引量:24
2郭幸华.硬质合金挤压成形剂及生产技术研究进展[J].稀有金属与硬质合金,2014,42(6):46-48.
3刘秋萍.钼粉的形貌与粒度分布对压坯强度的影响[J].铸造技术,2012,33(11):1270-1272. 被引量:9
4孙丹,张鹤年,孙卫权,李广生.一种新型超细硬质合金棒料挤压成形剂的设计[J].硬质合金,2009,26(3):176-179. 被引量:5
5付胜,易军,戴湘平.高压坯强度钨粉工艺研究[J].中国钨业,2012,27(5):32-35. 被引量:5
6张立,吴冲浒,王振波,单成,熊湘君.硬质合金常用模压成形剂的热分解特性[J].粉末冶金材料科学与工程,2010,15(6):674-678. 被引量:7
7康新婷,汤慧萍,王建永,迟煜頔,杨保军,王建,李亚宁.成形压力对Fe16Al2Cr多孔材料性能的影响[J].稀有金属材料与工程,2011,40(10):1732-1736. 被引量:5
8林信平,曹顺华,李炯义.温压工艺在硬质合金制备中的应用[J].中国钼业,2004,28(3):29-33. 被引量:3
9Jin-ChunKim Sung-SooRyu Hyoklee In-HyungMoon.纳米结构W—Cu复合粉末的金属注射成形[J].国外难熔金属与硬质材料,1999,15(2):55-61.
10王小路,黄晋,龙威,张友寿,夏露.铸钢用新型保温补贴材料研究[J].铸造,2016,65(10):945-949.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Type selection and amount of paraffin molding agent were studied,and improvements were made for the shortcomings of the paraffin.There are two main ways to improve paraffin:one is adding the right amount of higher fatty acids into paraffin and the other is adding the right amount of surfactants into paraffin.Paraffin viscosity and pellet rigidity are improved by improving paraffin molding agent,so that the pressing pressure is reduced,the strength of compacts increases,and the cracks are effectively reduced without significant effect on the magnetic saturation,coercivity and flexural strength of the products,resulting in very good applications of the improved paraffin in cemented carbide production and research.
quote
| GB/T 7714-2015 | [1] CHEN Shuang-lin, FU Kun, ZHOU Jian-hua, et al. Study on Improvement of Paraffin as the Molding Agent of Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2014(3): 58-62. |
| MLA | [1] CHEN Shuang-lin, et al., "Study on Improvement of Paraffin as the Molding Agent of Cemented Carbide." Rare Metals and Cemented Carbides, no. 3, 2014, pp. 58-62. |
| APA | [1] CHEN Shuang-lin, FU Kun, ZHOU Jian-hua, & SUN Bao-qi. (2014). Study on Improvement of Paraffin as the Molding Agent of Cemented Carbide. Rare Metals and Cemented Carbides(3), 58-62. |
| IEEE | [1] CHEN Shuang-lin, FU Kun, ZHOU Jian-hua, and SUN Bao-qi, "Study on Improvement of Paraffin as the Molding Agent of Cemented Carbide," Rare Metals and Cemented Carbides, no. 3, pp. 58-62, 2014. keywords: {paraffin;molding agent;mixture;cemented carbide;compact strength} |