MOF-Based 3D Ion-Conducting Network Enables High-Voltage All-Solid-State Lithium Metal Batteries at Room Temperature AITranslate

South China Normal University; South China Normal University; South China Normal University; South China Normal University; South China Normal University; South China Normal University; South China Normal University; South China Normal University; South China Normal University; South China Normal University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metal–organic frameworks (MOFs) with high surface area, tunable porous structure, and versatile functionality hold great prospects for manipulating ion transport and designing high-performance composite solid electrolytes (CSEs). However, the discontinuous ion transport and poor mechanical support arising from the randomly distributed MOF particles lead to insufficient ionic conductivity and inferior mechanical strength. Herein, a highly efficient and robust MOF-based 3D ion conducting network was rationally designed by in situ grown MOF nanocrystals on the 3D polyimide fiber network, where (1) the optimized MOF with appropriate pore sizes and abundant open metal sites can effectively restrict the movement of the anion to homogenize the Li+ flux, (2) the in situ growth of densely packed MOFs builds continuous ion channels to promote the rapid transport of Li+, and (3) the mechanically and chemically robust polyimide network bestows the CSE with superior mechanical strength and high oxidation stability. Consequently, the resulting CSE demonstrates high ionic conductivity, a high Li+ transference number, excellent Li compatibility, a wide potential window, and excellent mechanical robustness, which enables the stable cycling of high-voltage all-solid-state Li-metal batteries at room temperature.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00077

Chinese Library Classification Number:

Citation Information:

Metal–organic frameworks (MOFs) with high surface area, tunable porous structure, and versatile functionality hold great prospects for manipulating ion transport and designing high-performance composite solid electrolytes (CSEs). However, the discontinuous ion transport and poor mechanical support arising from the randomly distributed MOF particles lead to insufficient ionic conductivity and inferior mechanical strength. Herein, a highly efficient and robust MOF-based 3D ion conducting network was rationally designed by in situ grown MOF nanocrystals on the 3D polyimide fiber network, where (1) the optimized MOF with appropriate pore sizes and abundant open metal sites can effectively restrict the movement of the anion to homogenize the Li+ flux, (2) the in situ growth of densely packed MOFs builds continuous ion channels to promote the rapid transport of Li+, and (3) the mechanically and chemically robust polyimide network bestows the CSE with superior mechanical strength and high oxidation stability. Consequently, the resulting CSE demonstrates high ionic conductivity, a high Li+ transference number, excellent Li compatibility, a wide potential window, and excellent mechanical robustness, which enables the stable cycling of high-voltage all-solid-state Li-metal batteries at room temperature.

quote

GB/T 7714-2015 [1] Siyan Zheng, Zhongliang Li, Luyi Chen, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00077.
MLA [1] Siyan Zheng, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00077.
APA [1] Siyan Zheng, Zhongliang Li, Luyi Chen, Yutong Huang, Junkai Shi, Shuxian Wang, Yang Liu, Yan Liu, YuePeng Cai, & Qifeng Zheng. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00077