In-Situ Synthesization of WC-6Co Cemented Carbides by SPS AITranslate
Abstract AITranslate
The WC-6Co cemented carbides were rapidly prepared by the in-situ synthesis during sintering by applying the SPS technology, using WO3,Co3O4 and carbon mixed powders as the raw powder material.The effects of the sintering temperature and the pressure on the degree of compactness, the grain microstructure and the mechanical properties of the alloy were studied. The pure phases of WC and Co were obtained when the sintering temperature of 1 270℃and the pressure of 90 MPa were used. The prepared samples have the relative density as 99%,the hardness HRA≥93 and HV≥1 900.
KeyWords AITranslate
1解迎芳,王兴庆,陈立东,李晓东,郭海亮.放电等离子烧结纳米硬质合金的研究[J].硬质合金,2003,20(3):138-142. 被引量:24
2王国栋.硬质合金原理[M].北京:冶金工业出版社,1988.
3张久兴,刘科高,周美玲.放电等离子烧结技术的发展和应用[J].粉末冶金技术,2002,20(3):129-134. 被引量:142
4罗锡裕.放电等离子烧结材料的最新进展[J].粉末冶金工业,2001,11(6):7-16. 被引量:50
5冯海波,周玉,贾德昌.放电等离子烧结技术的原理及应用[J].材料科学与工艺,2003,11(3):327-331. 被引量:61
6Cynthia L.Dow finds cost effective route to fine WC powders[J].Metal Powder Report,1997,52(12):27.
7曹顺华,高海燕,李元元,李炯义,曲选辉.利用反应热处理制备纳米晶WC-10Co复合粉末[J].中南工业大学学报,2003,34(5):480-483. 被引量:3
8晏洪波,张丽英,吴成义,吴庆华,崔萍.直接还原碳化法制备超细WC-Ni-Fe合金粉的研究[J].粉末冶金技术,2001,19(3):144-147. 被引量:6
9饶岩岩,张久兴,王澈,张国珍.钨/钴氧化物SPS直接碳化原位合成超细WC-Co硬质合金[J].稀有金属与硬质合金,2006,34(1):18-21. 被引量:13
10Schubert W D,et al.Hardness to toughness relationship of fine-grained WC-Co hardmetal[J].International Journal of Refactory Metals and Hard Materials,1998,16:133.
1郭圣达,易健宏,鲍瑞.放电等离子烧结制备钨钴硬质合金的研究现状[J].中国钨业,2015,30(6):35-41. 被引量:6
2文彦,张钦英,郭圣达,苏伟,黄柱,陈颢.WC-6Co硬质合金SPS烧结工艺[J].有色金属科学与工程,2017,8(3):74-78. 被引量:11
1杨大锦.2015年云南冶金年评[J].云南冶金,2016,45(2):54-80. 被引量:1
2郭圣达,鲍瑞,易健宏,羊建高.SPS原位碳化合成WC-6Co硬质合金[J].中国钨业,2016,31(6):13-17. 被引量:1
3文彦,张钦英,郭圣达,苏伟,黄柱,陈颢.WC-6Co硬质合金SPS烧结工艺[J].有色金属科学与工程,2017,8(3):74-78. 被引量:11
4郭圣达,鲍瑞,易健宏,羊建高,刘亮,杨平.SPS制备含钼WC-6Co硬质合金的工艺性能[J].中国有色金属学报,2018,28(3):556-564. 被引量:6
5朱二涛,张久兴,羊建高.喷雾转化法制备WC-Co复合粉末制备硬质合金的研究进展[J].稀有金属与硬质合金,2019,47(3):70-78. 被引量:2
6段柏华,张钊,杨栋林,王德志.微波烧结工艺对6%Al2O3/Mo复合材料结构和性能的影响[J].有色金属科学与工程,2019,10(4):59-65. 被引量:2
7吴杰,王忠华,吕健.HVOF喷涂超细结构WC-12Co涂层磨粒磨损性能[J].稀有金属与硬质合金,2019,47(4):24-29.
8汪艳亮,王云,谢小豪,陈林芳,陈颢.稀土硬质合金研究进展[J].有色金属科学与工程,2019,10(5):106-112. 被引量:9
9朱二涛,张久兴,杨新宇,潘亚飞,羊建高.Co对原位合成WC-6Co复合粉末制备高性能硬质合金的影响[J].有色金属科学与工程,2019,10(6):31-39. 被引量:1
10韩翠柳,沈学峰,王衍,杨新宇,潘亚飞,张久兴.放电等离子烧结新技术新材料研究现状与发展趋势[J].航空制造技术,2019,62(22):43-51. 被引量:10
1谢宏,肖逸锋,贺跃辉,丰平,黄自谦.低压烧结对硬质合金组织和性能的影响[J].中国钨业,2006,21(6):27-31. 被引量:25
2江莞,王连军,陈立东,秦超.SPS制备Ti-Si-C系纳米复合材料[J].稀有金属材料与工程,2005(z1):367-370.
3谢兴铖,林晨光,贾成厂,曹瑞军.超细WC-6Co硬质合金注射参数的优化[J].稀有金属材料与工程,2015,44(12):3202-3207. 被引量:4
4李炯义,曹顺华,林信平,高海燕,李元元.反应热处理技术制备纳米晶WC-6Co硬质合金复合粉末[J].金属热处理,2005,30(7):56-59. 被引量:2
5董学泉,孔德军,王进春.海洋平台用S355钢表面电弧喷涂Al涂层组织及性能[J].材料热处理学报,2015,36(4):215-220.
6闵学刚,余新泉,孙扬善,冯文博,孙建荣.铁铝混合粉热喷涂及扩散处理组织分析[J].金属热处理,2001,26(5):4-7. 被引量:2
7朱丽慧,胡涛,彭笑,倪旺阳,刘一雄.Al含量对TiAlN涂层结合强度的影响[J].材料热处理学报,2015,36(3):154-158. 被引量:21
8肖逸锋,贺跃辉,丰平,谢宏,马自省,张丽娟,黄自谦,黄伯云.WC-Co梯度硬质合金的制备及渗碳对其组织的影响[J].材料热处理学报,2008,29(1):116-119. 被引量:8
9范亮,刘丹敏,张久兴.大块非晶的性能及其制备技术[J].功能材料,2007,38(A10):4051-4054. 被引量:3
10张国栋,洪敏,张建强,张富巨.基于SPS技术的异种钢焊接[J].焊接学报,2009,30(2):141-144. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The WC-6Co cemented carbides were rapidly prepared by the in-situ synthesis during sintering by applying the SPS technology, using WO3,Co3O4 and carbon mixed powders as the raw powder material.The effects of the sintering temperature and the pressure on the degree of compactness, the grain microstructure and the mechanical properties of the alloy were studied. The pure phases of WC and Co were obtained when the sintering temperature of 1 270℃and the pressure of 90 MPa were used. The prepared samples have the relative density as 99%,the hardness HRA≥93 and HV≥1 900.
quote
| GB/T 7714-2015 | [1] WANG Kai, SONG Xiao-yan, ZHANG Jiu-xing, et al. In-Situ Synthesization of WC-6Co Cemented Carbides by SPS[J]. Rare Metals and Cemented Carbides, 2006(4): 17-21. |
| MLA | [1] WANG Kai, et al., "In-Situ Synthesization of WC-6Co Cemented Carbides by SPS." Rare Metals and Cemented Carbides, no. 4, 2006, pp. 17-21. |
| APA | [1] WANG Kai, SONG Xiao-yan, ZHANG Jiu-xing, & LIU Wen-bin. (2006). In-Situ Synthesization of WC-6Co Cemented Carbides by SPS. Rare Metals and Cemented Carbides(4), 17-21. |
| IEEE | [1] WANG Kai, SONG Xiao-yan, ZHANG Jiu-xing, and LIU Wen-bin, "In-Situ Synthesization of WC-6Co Cemented Carbides by SPS," Rare Metals and Cemented Carbides, no. 4, pp. 17-21, 2006. keywords: {SPS;in-situ synthesis;degree of compactness;WC-6Co cemented carbides} |