Abstract AITranslate
Ni60-WC composite coatings were prepared on Cr12 MoV steel surface by sintering cladding of Ni60-WC alloy powder.The phase composition,microstructure,interfacial structure and cross-sectional hardness distribution of Ni60-WC composite coatings were analyzed by metallographic microscope,X-ray diffractometer and Rockwell hardness tester.The effects of sintering temperature,insulation time and heat treatment process on microstructure and properties of the composite coatings were studied.The results show that Ni60-WC composite coatings mainly consist of γ-Ni-based solid solution and hard phases such as WC,W2C,B6Fe23,BNi3 and FeNi.When sintering temperature is 1 050 ℃ and insulation time is 30 min,the composite coating is compact with few pores and good metallurgical bond at the interface.Heat treatment promotes the diffusion of alloying elements between the coating and the substrate.The hardness of the substrate and the coating is effectively improved also by heat treatment,and the hardness value of the coating is increased from 59 HRC to 65 HRC.
KeyWords AITranslate
1雍耀维,傅卫,张翔,邓琦林,杨建国.原位生成WC/TaC复合激光熔覆层组织研究(英文)[J].稀有金属材料与工程,2017,46(11):3176-3181. 被引量:5
2赵健,刘光,马冰,郑子云,贾利,崔烺,徐建江.铜表面激光合金化和激光熔覆制备Ni/NiCrBSi梯度涂层[J].兵器材料科学与工程,2018,41(2):53-57. 被引量:9
3余廷,陈杰,饶锡新,张子翔.激光熔覆NiCrBSi涂层的高温摩擦行为[J].激光与光电子学进展,2019,56(10):233-238. 被引量:4
4曹佑青,蒋朋,吕玉廷,徐金富.有氧烧结Ni60-WC/Cr12MoV双金属复合材料的组织和性能[J].热加工工艺,2012,41(8):109-111. 被引量:3
5韩小云,王贤瑞,丁小芹,游航,梁翠,徐金富.有氧烧结Ni60/WC合金涂层的组织和性能[J].兵器材料科学与工程,2011,34(2):64-66. 被引量:3
6肖逸锋,曾凡检,匡雯慧,吴靓,许艳飞,钱锦文,贺跃辉.真空烧结熔覆Ni60涂层的组织和性能[J].金属热处理,2017,42(7):83-87. 被引量:9
7许祥平,王怡,刘兆龙,黄晓龙,邹家生.WC-NiCrBSi复合涂层的制备与耐磨性能研究[J].江苏科技大学学报:自然科学版,2018,32(6):778-782. 被引量:3
8赵志平,李新勇.重熔处理对火焰热喷涂Ni60A涂层件疲劳性能的影响[J].粉末冶金技术,2015,33(4):285-289. 被引量:5
9李朋洋,余新泉,黄怡,潘徐杰.火焰喷焊和等离子堆焊制备Ni60及Ni60-WC涂层的组织与性能[J].机械工程材料,2017,41(10):38-43. 被引量:7
10雷靖峰,祁文军,谢亚东,韩会.U71Mn钢表面激光熔覆Ni60-25%WC涂层工艺参数优化的研究[J].表面技术,2018,47(3):66-71. 被引量:25
1杨效田,周俊,王新华,魏亨利,曾荣,杨强斌,李文生.Cu含量对Ni基定向合金涂层组织与摩擦学性能的影响[J].稀有金属材料与工程,2022,51(4):1420-1426. 被引量:1
2何晓荣,黎秋萍,刘少鹏,沈明学.Cr12MoV模具钢渗氮层服役过程中不同磨损阶段的摩擦学特性[J].表面技术,2022,51(8):243-251. 被引量:1
1林犀灵,杨卯生,周晓龙.M50钢高应力高温摩擦磨损行为与微观机制[J].钢铁研究学报,2023,35(3):332-346.
2杨效田,曾荣,王新华,余伦,曹天翔,安国升.Ni60/Cu定向结构涂层在不同浓度H_(2)SO_(4)中的耐蚀性能[J].稀有金属材料与工程,2023,52(4):1311-1320.
1申井义,林晨(指导),姚永强,刘佳,徐欢欢.Ni60合金包覆WC粉激光熔覆涂层的组织与性能[J].机械工程材料,2020,44(7):18-22. 被引量:6
2李洋城,程晓农,罗锐,韦家波,张洁,高天明.热疲劳对B/M复相H13钢组织及力学性能的影响[J].金属热处理,2020,45(8):17-21.
3王俊杰,杨军,邹德宁,李新涛,米小雨.堆焊工艺参数与碳化钨含量对镍基碳化钨涂层性能的影响研究[J].矿冶工程,2020,40(4):130-134. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TB331[一般工业技术—材料科学与工程]
Citation Information:
Ni60-WC composite coatings were prepared on Cr12 MoV steel surface by sintering cladding of Ni60-WC alloy powder.The phase composition,microstructure,interfacial structure and cross-sectional hardness distribution of Ni60-WC composite coatings were analyzed by metallographic microscope,X-ray diffractometer and Rockwell hardness tester.The effects of sintering temperature,insulation time and heat treatment process on microstructure and properties of the composite coatings were studied.The results show that Ni60-WC composite coatings mainly consist of γ-Ni-based solid solution and hard phases such as WC,W2C,B6Fe23,BNi3 and FeNi.When sintering temperature is 1 050 ℃ and insulation time is 30 min,the composite coating is compact with few pores and good metallurgical bond at the interface.Heat treatment promotes the diffusion of alloying elements between the coating and the substrate.The hardness of the substrate and the coating is effectively improved also by heat treatment,and the hardness value of the coating is increased from 59 HRC to 65 HRC.
quote
| GB/T 7714-2015 | [1] LI Xin-xing, WANG Hong-xia, SHI Jian-feng, et al. Research on Microstructure and Properties of Ni60-WC Composite Coatings on Cr12MoV Steel Surface Prepared by Sintering Cladding[J]. Rare Metals and Cemented Carbides, 2020(4): 24-27. |
| MLA | [1] LI Xin-xing, et al., "Research on Microstructure and Properties of Ni60-WC Composite Coatings on Cr12MoV Steel Surface Prepared by Sintering Cladding." Rare Metals and Cemented Carbides, no. 4, 2020, pp. 24-27. |
| APA | [1] LI Xin-xing, WANG Hong-xia, SHI Jian-feng, XU Yan, CUI Lei, & HAN Bo-Qun. (2020). Research on Microstructure and Properties of Ni60-WC Composite Coatings on Cr12MoV Steel Surface Prepared by Sintering Cladding. Rare Metals and Cemented Carbides(4), 24-27. |
| IEEE | [1] LI Xin-xing, WANG Hong-xia, SHI Jian-feng, XU Yan, CUI Lei, and HAN Bo-Qun, "Research on Microstructure and Properties of Ni60-WC Composite Coatings on Cr12MoV Steel Surface Prepared by Sintering Cladding," Rare Metals and Cemented Carbides, no. 4, pp. 24-27, 2020. keywords: {composite coating;Ni60-WC;sintering cladding;microstructure;hardness distribution} |