Enhanced Durability of an All-Solid-State WO3 Based Electrochromic Device on a Single Substrate by Using a Complementary Anodically Coloring Poly(o-ethoxyaniline) Enhanced Durability of an All-Solid-State WO3 Based Electrochromic Device on a Single Substrate by Using a Complementary Anodically Coloring Poly(o-ethoxyaniline) AITranslate
Abstract AITranslate
Electrochromic (EC) devices represent one of the most promising energy-saving and solar control technologies for the market of energy-efficient building and optoelectronic devices by offering dynamic control of the optical transmission of visible and near-infrared light. Although notable results are achieved in terms of material and EC performance, a continuous and intense effort is currently devoted to the development of effective solid-state systems capable of providing excellent durability. Here, poly(o-ethoxyaniline) (POEA), a derivative of PANI capable of being more easily processed by solution deposition techniques than PANI, is used as both anodic EC and protective layer to fabricate a complementary all-solid-state WO3/POEA based EC device on a single-glass substrate. The introduction of POEA, synthesized by chemical oxidative polymerization, enabled a more marked protection against the degradative processes occurring at the anode side, promoting at the same time a more effective conversion between the different WO3 redox states, fast switching dynamics, and a high coloration efficiency (η = 150 cm2 C–1). Besides determining a significant gain in EC performance, POEA permits us to maintain a good optical response and electrochemical stability after 1000 CV cycles, conferring an enhanced durability with respect to similar monolithic all-solid-state WO3 based EC devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c01079
Chinese Library Classification Number:
Citation Information:
Electrochromic (EC) devices represent one of the most promising energy-saving and solar control technologies for the market of energy-efficient building and optoelectronic devices by offering dynamic control of the optical transmission of visible and near-infrared light. Although notable results are achieved in terms of material and EC performance, a continuous and intense effort is currently devoted to the development of effective solid-state systems capable of providing excellent durability. Here, poly(o-ethoxyaniline) (POEA), a derivative of PANI capable of being more easily processed by solution deposition techniques than PANI, is used as both anodic EC and protective layer to fabricate a complementary all-solid-state WO3/POEA based EC device on a single-glass substrate. The introduction of POEA, synthesized by chemical oxidative polymerization, enabled a more marked protection against the degradative processes occurring at the anode side, promoting at the same time a more effective conversion between the different WO3 redox states, fast switching dynamics, and a high coloration efficiency (η = 150 cm2 C–1). Besides determining a significant gain in EC performance, POEA permits us to maintain a good optical response and electrochemical stability after 1000 CV cycles, conferring an enhanced durability with respect to similar monolithic all-solid-state WO3 based EC devices.
quote
| GB/T 7714-2015 | [1] Vitantonio Primiceri, Marco Pugliese, Roberto Giannuzzi, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01079. |
| MLA | [1] Vitantonio Primiceri, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01079. |
| APA | [1] Vitantonio Primiceri, Marco Pugliese, Roberto Giannuzzi, Marco Esposito, Giuseppe Gigli, Vincenzo Maiorano, & Pierluigi Cossari. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01079 |
| IEEE | [1] Vitantonio Primiceri, Marco Pugliese, Roberto Giannuzzi, Marco Esposito, Giuseppe Gigli, Vincenzo Maiorano, and Pierluigi Cossari, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01079. keywords: {poly(oethoxyaniline) WO3 solidstate electrochromic device cyclic voltammetry durability} |