Preparation of Small Size and High Total Cerium Carbonate AITranslate
Abstract AITranslate
Small size and high total cerium carbonate with the total >70 % and the particle size D50<15 μm was prepared by one-step precipitation using ammonium bicarbonate as precipitant.By using laser particle size analyzer,scanning electron microscope and EDTA titration methods,the effects of cerium chloride concentration,molar ratio of ammonium bicarbonate to cerium chloride,reaction temperature and pH value on the particle size and total of cerium carbonate were investigated.The results show that under the condition of cerium chloride concentration of 0.6~0.8 mol/L,molar ratio of ammonium bicarbonate to cerium chloride of 4 :1,reaction temperature of 80℃ and pH of 4,the precipitated cerium carbonate achieving good crystalline form,with particle size D50~15 μm and total >72M can be obtained.
KeyWords AITranslate
1冷忠义,马莹,许延辉,张丽萍,郝先库,范明洋,白彦,王文斌,孟祥,黄继民.用碳酸氢铵作沉淀剂制取碳酸钕和氧化钕[J].稀土,2000,21(6):26-29. 被引量:14
2李永绣,胡平贵,何小彬,辜子英,黎敏.碳酸钇铵复盐结晶的形成及影响因素[J].中国稀土学报,2000,18(1):79-81. 被引量:17
3王嵩龄,刘艳,程福祥,吴声,廖春生.碳酸钠作沉淀剂制备碳酸稀土的研究[J].矿冶,2015,24(2):44-46. 被引量:22
4李慧琴,李健,赵永志,张瑞祥,郝先库,马显东.碳酸氢铵沉淀法制备大颗粒球形氧化钇的研究[J].稀土,2014,35(3):77-81. 被引量:12
1尹贺军,柴帅东.EDTA在水泥稳定碎石滴定中的误差分析——以商丘黄河路改建工程为例[J].河南科技,2018,37(34):111-112. 被引量:2
2一种多段格式螺旋排焦阀[J].燃料与化工,2019,50(1):61-61.
3蓝桥发,邱小英,朱宸,肖敏,叶春生.正交实验法优化高纯氧化钕制备工艺参数[J].有色冶金设计与研究,2018,39(6):47-50.
4温俊峰,王超,李瑞,张敏娜,高立国.沙柳纤维素提取工艺研究与结构表征[J].榆林学院学报,2019,29(2):17-21. 被引量:4
5桑兆虎,李明.不同乳化体系对氯乙烯聚合影响研究[J].中国氯碱,2018(12):13-17.
6张保明.含钯废活性炭催化剂中金属钯的回收[J].中国资源综合利用,2019,37(2):27-29. 被引量:1
7刘建国,苏石晶,姚传凯,朱虎.鞘氨醇单胞杆菌Sphigomonas sp.WG产威兰胶的提取工艺研究[J].山东科技大学学报:自然科学版,2019,38(2):44-48. 被引量:3
8张千,刘向阳,陈旺,吴恒,肖芃颖,吉芳英,李宸,念海明.新型除磷填料的制备及除磷吸附床运行参数的优化[J].化工学报,2019,70(3):1099-1110. 被引量:5
9周玉新,王健,朱成,刘一林.撞击流反应器制备电池级超细磷酸铁[J].化学工程与装备,2019(3):4-7. 被引量:2
10李庆磊,刘艳茹,孙瑶,党光耀.极化石墨毡电极膜电吸附去除并回收乙酸[J].泰山医学院学报,2019,40(3):182-186.
Basic Information:
DOI:
Chinese Library Classification Number:TF845.6[冶金工程—有色金属冶金]
Citation Information:
Small size and high total cerium carbonate with the total >70 % and the particle size D50<15 μm was prepared by one-step precipitation using ammonium bicarbonate as precipitant.By using laser particle size analyzer,scanning electron microscope and EDTA titration methods,the effects of cerium chloride concentration,molar ratio of ammonium bicarbonate to cerium chloride,reaction temperature and pH value on the particle size and total of cerium carbonate were investigated.The results show that under the condition of cerium chloride concentration of 0.6~0.8 mol/L,molar ratio of ammonium bicarbonate to cerium chloride of 4 :1,reaction temperature of 80℃ and pH of 4,the precipitated cerium carbonate achieving good crystalline form,with particle size D50~15 μm and total >72M can be obtained.
quote
| GB/T 7714-2015 | [1] LU Mei, QIU Guang-huai, MA Yong, et al. Preparation of Small Size and High Total Cerium Carbonate[J]. Rare Metals and Cemented Carbides, 2019(1): 16-18. |
| MLA | [1] LU Mei, et al., "Preparation of Small Size and High Total Cerium Carbonate." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 16-18. |
| APA | [1] LU Mei, QIU Guang-huai, MA Yong, ZHANG Xiang-biao, & GAO Wei-zheng. (2019). Preparation of Small Size and High Total Cerium Carbonate. Rare Metals and Cemented Carbides(1), 16-18. |
| IEEE | [1] LU Mei, QIU Guang-huai, MA Yong, ZHANG Xiang-biao, and GAO Wei-zheng, "Preparation of Small Size and High Total Cerium Carbonate," Rare Metals and Cemented Carbides, no. 1, pp. 16-18, 2019. keywords: {small size;high total;cerium carbonate;ammonium bicarbonate;cerium chloride;one-step precipitation} |