A New Technology for Ammonium Heptamolybdate AITranslate

Anhui Provincial Institute of Metallurgical Science;Anhui Provincial Institute of Metallurgical Science;Anhui Provincial Institute of Metallurgical Science;Anhui Provincial Institute of Metallurgical Science;Anhui Provincial Institute of Metallurgical Science
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The solution of acidic ammonium molybdate is precipitated with the hexamine. Its precipitate is employed to generate the ammonium heptamolybdate in basic condition and the hexamine can be completely recovered.

KeyWords AITranslate

hexamine ammonium heptamolybdate precipitation crystallization

1张宝,夏晓梅,李倩.单相仲钼酸铵制备与表征[J].稀有金属材料与工程,2012,41(S2):781-785. 被引量:2

2曹璇,张宝.七钼酸铵的制备及进展[J].铜业工程,2008(4):29-31. 被引量:7

3厉学武,崔玉青,唐丽霞,唐军利,罗建海.结晶工艺与钼酸铵品质的对比研究[J].中国钼业,2011,35(2):33-35. 被引量:4

4马素娟,刘锦锐.用二钼酸铵制备仲钼酸铵的实验研究[J].中国钼业,2011,35(5):31-33. 被引量:6

5孙凯学,厉学武.高浓度氨氮废水处理应用研究[J].中国钼业,2013,37(6):46-48.

6徐志昌,张萍.模块化合成化学在制备系列钼酸铵工艺中的应用[J].中国钼业,2019,43(6):38-43. 被引量:2

1张亨.钼酸铵的生产研究进展[J].中国钼业,2013,37(2):49-54. 被引量:5

2张金莲,张要军,黄进献.七钼酸铵制备新工艺的研究[J].现代矿业,2015,0(10):89-90. 被引量:4

3张旭,郭军刚,白佩,员汝娜,李冬,李稳宏.七钼酸铵制备工艺优化及热力学分析研究[J].西北大学学报:自然科学版,2017,47(6):852-858. 被引量:2

4郭军刚,白佩,崔玉青.七钼酸铵连续式结晶工艺优化研究[J].中国钼业,2018,42(1):34-39. 被引量:2

5刘锦锐.钼酸铵生产工艺流程综述[J].云南冶金,2018,47(4):48-57. 被引量:4

6郭株辉.四钼酸铵转化成七钼酸铵的工艺研究[J].铜业工程,2018(6):46-52. 被引量:1

7徐志昌,张萍.系列钼酸铵合成工艺的研究[J].中国钼业,2019,43(2):31-36. 被引量:2

8徐志昌,张萍.模块化合成化学在制备系列钼酸铵工艺中的应用[J].中国钼业,2019,43(6):38-43. 被引量:2

9杨利群,周秋生,彭志宏,刘桂华,齐天贵,李小斌.易热分解易水溶性金属铵盐的一步法制备[J].中国有色金属学报,2021,31(12):3634-3644.

10刘蕾.二钼酸铵中钙含量控制的研究[J].四川化工,2022,25(2):17-19.

1林潜德,徐孝德.仲钼酸铵生产线简介[J].中国钼业,1996,20(3):26-28.

2秦文峰,彭金辉,樊希安,肖新志,袁茂强.微波辐射法干燥仲钼酸铵新工艺[J].中国钼业,2002,26(6):28-31. 被引量:12

3赵延霞.以聚乙二醇为模板制备纳米MoO_3微粉[J].中国钨业,2013,28(1):34-38.

4李天锁.钾对仲钼酸铵直接还原成二氧化钼的影响[J].中国钼业,1997,21(6):28-32. 被引量:4

5周晓平,马琳,徐旭耀,冯宗财.仲钼酸铵热分解过程及热力学分析[J].稀有金属与硬质合金,2015,43(3):25-28. 被引量:4

6钼盐文摘[J].无机盐技术,2012(3):54-54.

7谢东.重结晶法提纯生产试剂钼酸铵[J].湖北化工,2002,19(2):29-29. 被引量:3

8易永鹏.仲钼酸铵(APM)生产过程质量控制[J].中国钼业,1998,22(5):45-46.

9赵延霞.水热法合成一维纳米级MoO_3微粉[J].中国钨业,2012,27(3):25-29. 被引量:2

10高纯仲钼酸铵的制备方法[J].中国钼业,2006,30(5):49-49.

Basic Information:

DOI:

Chinese Library Classification Number:TQ136.12[化学工程—无机化工];TQ113.79[化学工程—无机化工]

Citation Information:

The solution of acidic ammonium molybdate is precipitated with the hexamine. Its precipitate is employed to generate the ammonium heptamolybdate in basic condition and the hexamine can be completely recovered.

quote

GB/T 7714-2015 [1] ZHOU Chao-hui, HUA Dong-fa, DING Zhi-hu, et al. A New Technology for Ammonium Heptamolybdate[J]. Rare Metals and Cemented Carbides, 1998(3): 1-4.
MLA [1] ZHOU Chao-hui, et al., "A New Technology for Ammonium Heptamolybdate." Rare Metals and Cemented Carbides, no. 3, 1998, pp. 1-4.
APA [1] ZHOU Chao-hui, HUA Dong-fa, DING Zhi-hu, ZHANG Zhi-jie, & ZHAO Ye-song. (1998). A New Technology for Ammonium Heptamolybdate. Rare Metals and Cemented Carbides(3), 1-4.
IEEE [1] ZHOU Chao-hui, HUA Dong-fa, DING Zhi-hu, ZHANG Zhi-jie, and ZHAO Ye-song, "A New Technology for Ammonium Heptamolybdate," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 1998. keywords: {hexamine;ammonium heptamolybdate;precipitation;crystallization}