Effect of Various Parameters on Specific Electric Capacity of Ta Powder with High Specific Capacity AITranslate
Abstract AITranslate
Influences of various parameters, such as average particle size, green density, sintering temperature, on the specific electric capacity of tantalum powder with high specific capacity were studied. The regression equation between the capacity and parameters was obtained. The temperature dependent characteristics of tantalum powder, furthermore, were investigated,by a comparison of some domestic powders with PL 22. The results show that the loss of the specific capacity during sintering increases with decreasing Ta powder particle size. Each paritcle size has an optimum sintering temperature for lowest loss of the capacity. The poor temperature characteristics of domestic Ta powder was due to non homogeneous distribution of the powder particles and their complicated shape.
KeyWords AITranslate
1邱向东.稀有金属冶金学会1996年年会论文集[M].宜昌:稀有金属冶金学会,1996.17.
2宁夏有色金属冶炼厂.超高比容钽粉(16V-30000μF·V/g)的技术鉴定报告[M].,1997..
1刘勇刚,易金锋.35 V47 μF固体钽电容器制备工艺的改进[J].电子工艺技术,2008,29(2):98-101. 被引量:4
1徐云飞,李春光,安涛,吴华.0603型钽电容器氧化膜的生长工艺[J].稀有金属材料与工程,2013,42(1):190-193. 被引量:1
2乔建伟,徐云飞.硝酸锰溶液添加硝酸铵对钽电容器电性的影响[J].科技视界,2013(5):71-73. 被引量:1
3熊晓莉,黄诚,耿嘎,陆胜,方鸣,李宁.乙醇对硝酸锰热分解的影响[J].重庆工商大学学报:自然科学版,2014,31(2):70-73. 被引量:4
4杜利蓉,祝呈捷,吴薄,张芳芳,唐先忠.过氧乙酸等添加剂对钽电容阴极被覆液性能的影响[J].电子元件与材料,2018,37(7):59-62. 被引量:1
1刘红东,潘伦桃,卢振达,郑爱国,程越伟,马跃忠,王春翔,李慧.高比容钽粉的新进展[J].稀有金属,2003,27(1):35-38. 被引量:10
2何季麟,刘红东,卢振达,马春红.高比容钽粉关键技术及应用开发研究[J].材料导报,2000,14(5):8-9. 被引量:4
3晏志凡.高比容钽粉用钙除氧的研究[J].稀有金属,1997,21(5):346-349. 被引量:5
4梁雅丽,王英红.高比容钽粉在电容器中的应用[J].电子元件与材料,2006,25(5):46-48. 被引量:6
5张春雷,陈学清,赵德强.电容器级中压高比容钽粉的特性[J].材料导报,2004,18(F10):330-331. 被引量:2
6张红丽,黎粤凌.高比容钽粉应用工艺[J].电子元件,1993(4):37-41.
7李慧,雒国清,程越伟,马跃忠,杨国启,柏林,马海燕.高比容钽粉的微观结构及电性能特性的研究[J].湖南有色金属,2017,33(1):48-52. 被引量:4
8程越伟,郑爱国,潘伦桃,李慧,任萍.电容器用钽粉的高比容化[J].宁夏工程技术,2006,5(1):99-101. 被引量:12
9冯颖芳.电容器用高比容钽粉的开发[J].稀有金属快报,2003(10):15-15.
10胡武将.高压变频器在球团高压电机上的应用研究[J].酒钢科技,2014(1):49-54.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料];TM535.1[电气工程—电器]
Citation Information:
Influences of various parameters, such as average particle size, green density, sintering temperature, on the specific electric capacity of tantalum powder with high specific capacity were studied. The regression equation between the capacity and parameters was obtained. The temperature dependent characteristics of tantalum powder, furthermore, were investigated,by a comparison of some domestic powders with PL 22. The results show that the loss of the specific capacity during sintering increases with decreasing Ta powder particle size. Each paritcle size has an optimum sintering temperature for lowest loss of the capacity. The poor temperature characteristics of domestic Ta powder was due to non homogeneous distribution of the powder particles and their complicated shape.
quote
| GB/T 7714-2015 | [1] CAO Han-song. Effect of Various Parameters on Specific Electric Capacity of Ta Powder with High Specific Capacity[J]. Rare Metals and Cemented Carbides, 1999(4): 6-10. |
| MLA | [1] CAO Han-song. "Effect of Various Parameters on Specific Electric Capacity of Ta Powder with High Specific Capacity." Rare Metals and Cemented Carbides, no. 4, 1999, pp. 6-10. |
| APA | [1] CAO Han-song. (1999). Effect of Various Parameters on Specific Electric Capacity of Ta Powder with High Specific Capacity. Rare Metals and Cemented Carbides(4), 6-10. |
| IEEE | [1] CAO Han-song, "Effect of Various Parameters on Specific Electric Capacity of Ta Powder with High Specific Capacity," Rare Metals and Cemented Carbides, no. 4, pp. 6-10, 1999. keywords: {Ta powder with high specific capacity;physical parameters;specific electric capacity;regression equation} |