Recovery of Rare Earth from CeFeB Waste by Sulfation Roasting-Selective Decomposition-Water Leaching AITranslate

School of Materials&Metallurgy(School of Rare Earth),Inner Mongolia University of Science and Technology;School of Materials&Metallurgy(School of Rare Earth),Inner Mongolia University of Science and Technology;School of Materials&Metallurgy(School of Rare Earth),Inner Mongolia University of Science and Technology;School of Materials&Metallurgy(School of Rare Earth),Inner Mongolia University of Science and Technology;School of Materials&Metallurgy(School of Rare Earth),Inner Mongolia University of Science and Technology;School of Materials&Metallurgy(School of Rare Earth),Inner Mongolia University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The method of sulfation roasting-selective decomposition-water leaching was used to recover rare earth from CeFeB waste,and meanwhile the reaction mechanism of CeO2 and Ce valence change in the re-covery process were investigated.The results show that the optimal recovery process conditions are sulfuric acid concentration of 14.5mol/L,sulfuric acid dosage of 2times the theoretical amount,sulfation roasting temperature and time of 300℃and 60min,and selective decomposition temperature and time of 700℃and 120min.Under the above optimized conditions,the rare earth leaching rate reaches 95.46%,the impurity Fe enters into the filter residue in the form of Fe2O3,and the rare earth oxide Nd0.20Ce0.80O1.90is ob-tained after the leaching solution is precipitated with oxalic acid and the precipitate is roasted.The products of sulfation roasting process are Ce(SO4)2,RE2(SO4)3and Fe2(SO4)3.Ce2(SO4)3,Fe2O3and indecompo-sable other RE2(SO4)3are obtained in the selective decomposition process,and the decomposition product SO3further reacts with unreacted CeO2to form Ce2(SO4)3.During the water leaching process,the water-soluble Ce2(SO4)3and RE2(SO4)3dissolve into the leachate,and the water-insoluble Fe2O3enters into the filter residue,thereby realizing the effective separation and recovery of rare earth from CeFeB waste.

KeyWords AITranslate

rare earth recovery CeFeB waste sulfation roasting selective decomposition water leaching process optimization reaction mechanism

1李亚峰.磁性材料行业现状与发展前景分析[J].新材料产业,2018(7):51-54. 被引量:8

2李世健,崔振杰,李文韬,王东,王志.钕铁硼废料循环利用技术现状与展望[J].材料导报,2021,35(3):3001-3009. 被引量:12

3胡伯平.稀土永磁产业现状及展望[J].稀土信息,2018,0(11):14-17. 被引量:12

4郭小明.稀土永磁材料的发展及应用[J].江西化工,2018,34(6):242-243. 被引量:6

5刘勇,刘珍珍,刘牡丹.稀土粗精矿的低温硫酸化分解工艺[J].中国有色金属学报,2014,24(12):3147-3154. 被引量:12

6杨瑛,杨汝栋.硫酸铈水合物的热分解行为及动力学研究[J].中国稀土学报,1993,11(4):293-296. 被引量:3

1朱小龙.新型铈铁硼中铅含量的测定方法研究[J].岩石矿物学杂志,2023,42(4):591-595.

2邓永春,袁璐,李宇航,辛文彬,姜银举,王亮.硫酸化焙烧-水浸法回收钕铁硼和铈铁硼废料过程的对比分析[J].稀有金属与硬质合金,2023,51(4):1-7.

1陈荣升,龙伟,杨建广,徐文俊.采用硫酸化焙烧—水浸工艺从铜烟灰氧压酸浸渣中浸出铟[J].湿法冶金,2022,41(2):126-132. 被引量:2

2王明,杨勇,周洁英,赖兰萍,陈后兴.云南省某地区离子型稀土矿提取试验研究[J].有色金属:矿山部分,2022,74(1):10-14.

3罗利军,孟德梅,戴建辉,李俊红,郑丽波,夏丽红,蒋峰芝.TiO_(2)-NB/pg-C3N4可见光催化降解17α-乙炔雌二醇的机理[J].中国环境科学,2022,42(2):654-664. 被引量:2

4库尔班江·努尔麦提,热娜古丽·阿不都热合曼.废水中Cr(Ⅲ)的吸附热力学和动力学研究进展[J].化工时刊,2022,36(2):22-25. 被引量:1

5闫时雨,纪文涛,谢克强,黄海艺,袁晓磊.水洗—酸浸两步法回收黄磷电尘灰中的镓及浸出动力学[J].有色金属工程,2022,12(3):86-95.

6赵雨,吴喜龙,王彪,王欢,李勇,刘文,杨深宏.载体溶解法回收失效Pt/TiO_(2)催化剂中的铂[J].贵金属,2021,42(4):37-40.

7杜晗,陈立群,黄苏勇.液相沉淀法制备超细碳酸钴的工艺研究[J].生物化工,2022,8(1):48-50.

8周常行,申峻,刘刚,曹敏,耿雅雯,张慧超.HY型分子筛催化蒽与1-十一烯烃的反应[J].石化技术与应用,2022,40(2):82-85.

9李振宇,淮丽媛,郝盼盼,赵玺,王永钊,张炳森,谌春林,张建.碳纳米管负载钯基催化剂催化氧化2,5-呋喃二甲醇合成2,5-呋喃二甲酸[J].催化学报(英文),2022,43(3):793-801. 被引量:1

10高琦,吴浩,郑江峰,黄仁忠,张颖,文定强.复杂铜钴合金酸浸-氧化酸浸工艺及动力学研究[J].中国有色冶金,2022,51(1):90-95.

Basic Information:

DOI:

Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]

Citation Information:

The method of sulfation roasting-selective decomposition-water leaching was used to recover rare earth from CeFeB waste,and meanwhile the reaction mechanism of CeO2 and Ce valence change in the re-covery process were investigated.The results show that the optimal recovery process conditions are sulfuric acid concentration of 14.5mol/L,sulfuric acid dosage of 2times the theoretical amount,sulfation roasting temperature and time of 300℃and 60min,and selective decomposition temperature and time of 700℃and 120min.Under the above optimized conditions,the rare earth leaching rate reaches 95.46%,the impurity Fe enters into the filter residue in the form of Fe2O3,and the rare earth oxide Nd0.20Ce0.80O1.90is ob-tained after the leaching solution is precipitated with oxalic acid and the precipitate is roasted.The products of sulfation roasting process are Ce(SO4)2,RE2(SO4)3and Fe2(SO4)3.Ce2(SO4)3,Fe2O3and indecompo-sable other RE2(SO4)3are obtained in the selective decomposition process,and the decomposition product SO3further reacts with unreacted CeO2to form Ce2(SO4)3.During the water leaching process,the water-soluble Ce2(SO4)3and RE2(SO4)3dissolve into the leachate,and the water-insoluble Fe2O3enters into the filter residue,thereby realizing the effective separation and recovery of rare earth from CeFeB waste.

quote

GB/T 7714-2015 [1] LI Yu-hang, DENG Yong-chun, JIANG Yin-ju, et al. Recovery of Rare Earth from CeFeB Waste by Sulfation Roasting-Selective Decomposition-Water Leaching[J]. Rare Metals and Cemented Carbides, 2022(1): 1-5.
MLA [1] LI Yu-hang, et al., "Recovery of Rare Earth from CeFeB Waste by Sulfation Roasting-Selective Decomposition-Water Leaching." Rare Metals and Cemented Carbides, no. 1, 2022, pp. 1-5.
APA [1] LI Yu-hang, DENG Yong-chun, JIANG Yin-ju, XIN Wen-bin, TANG Jia-yue, & LIANG Yu-yu. (2022). Recovery of Rare Earth from CeFeB Waste by Sulfation Roasting-Selective Decomposition-Water Leaching. Rare Metals and Cemented Carbides(1), 1-5.
IEEE [1] LI Yu-hang, DENG Yong-chun, JIANG Yin-ju, XIN Wen-bin, TANG Jia-yue, and LIANG Yu-yu, "Recovery of Rare Earth from CeFeB Waste by Sulfation Roasting-Selective Decomposition-Water Leaching," Rare Metals and Cemented Carbides, no. 1, pp. 1-5, 2022. keywords: {rare earth recovery;CeFeB waste;sulfation roasting;selective decomposition;water leaching;process optimization;reaction mechanism}