Experimental Study on Preparation of Ferrous Oxalate with Titanium Dioxide Waste Water AITranslate
Abstract AITranslate
Titanium dioxide waste water is a kind of acidic waste water containing a lot of iron ions, which has important recovery value.Using titanium dioxide waste water as raw material, ferrous oxalate was prepared by adding sodium oxalate.The effects of sodium oxalate dosage, reaction temperature, stirring strength and reaction time on the precipitation rate of iron were analyzed.The phase and microstructure of the precipitated products were analyzed by XRD and SEM-EDS.The results show that the precipitation rate of iron is more than 82% under the optimized conditions of titanium dioxide waste water volume of 50 mL,temperature of 20 ℃,sodium oxalate dosage of 12 g, stirring strength of 300 r/min and reaction time of 30 min, and the precipitate is the granular crystal of ferrous oxalate dihydrate with a purity of more than 98%.This study provides a method for efficient recovery of iron resources in acidic solution system.
KeyWords AITranslate
1王建伟,任秀莲,魏琦峰,杨东,吴成龙.钛白废酸的综合利用研究现状及展望[J].无机盐工业,2009,41(9):4-7. 被引量:26
2崔艳,曹波.关于硫酸法钛白粉生产工艺中废水处理的研究[J].当代化工研究,2017(6):106-107. 被引量:2
3李潜,张启修.萃取法回收钛白水解废酸中硫酸的实验研究[J].稀有金属与硬质合金,2003,31(1):4-7. 被引量:10
4杨涛,王志坚,肖劲,刘吉波,余荣旻,邓志军.赤泥和钛白废液中提钪的浸出工艺研究[J].矿冶,2015,24(5):37-40. 被引量:11
5邓刚.硫酸法钛白生产工艺红石膏产生量分析[J].广东化工,2017,44(11):147-149. 被引量:1
6卢阶主,张亮玖.硫酸法钛白废液萃取富集钪[J].山西冶金,2019,42(2):10-12. 被引量:4
7朱晓波,牛泽鹏,李望,白云涛,王涛,任博.溶剂萃取法回收钛白废液中钒的实验研究[J].稀有金属与硬质合金,2020(1):9-12. 被引量:4
8李望,赵恒,朱晓波.钛白废液制备黄钾铁矾的实验研究[J].稀有金属与硬质合金,2018,46(3):35-37. 被引量:1
1李望,王雯博,段理哲,朱晓波.伯胺7101萃取分离钒及有机相乳化分析[J].矿冶工程,2021,41(4):76-78.
2钟艳君,吴振国,田海,郭孝东,钟本和,王辛龙.碳包覆LiFe_(0.5)Co_(0.5)PO_4固溶体正极材料的制备及其电化学性能(英文)[J].无机化学学报,2018,34(8):1581-1589. 被引量:1
3邓强,杨林,王辛龙,庄海波,郭磊.草酸反萃萃取剂中铁离子的工艺研究[J].应用化工,2021,50(2):433-437. 被引量:1
4李梦醒,潘瑞,徐冰洁,邱奔,韩召.砷的还原热力学及纳米零价铁除砷初步探究[J].工业水处理,2021,41(4):37-42. 被引量:3
5罗文波,张琼,江爱敏,焦梅,龙潇.从废镍氢电池浸出液中选择性沉淀稀土[J].湿法冶金,2022,41(2):150-153.
6梁晨,马雅丽,闫立山.IN718合金增材制造温度场仿真及微观组织分析[J].组合机床与自动化加工技术,2022(2):91-94.
7张伟光,张廷安,孙颖,吕国志,曹雪娇.磷-硫-钒-水体系酸性溶液中钒的提取热力学分析[J].稀有金属材料与工程,2021,50(12):4265-4271.
8郝博魁,邓小洲,蔡启舟,肖凤赞,郑卫星,田韵森,陈哲.稀土与镁含量对蠕墨铸铁凝固过程及石墨形态的影响[J].铸造技术,2022,43(1):14-18.
9孙海波,徐淑波,张森,李阳,任国成,景财年.SLM成形不同孔隙结构骨支架的仿真与实验研究[J].精密成形工程,2022,14(2):123-128. 被引量:3
10刘娜娜,徐新阳,陈熙,刘源.SCR废催化剂中钒和钨常温常压浸出新工艺[J].东北大学学报:自然科学版,2022,43(3):414-422.
Basic Information:
DOI:
Chinese Library Classification Number:TF09[冶金工程—冶金物理化学]
Citation Information:
Titanium dioxide waste water is a kind of acidic waste water containing a lot of iron ions, which has important recovery value.Using titanium dioxide waste water as raw material, ferrous oxalate was prepared by adding sodium oxalate.The effects of sodium oxalate dosage, reaction temperature, stirring strength and reaction time on the precipitation rate of iron were analyzed.The phase and microstructure of the precipitated products were analyzed by XRD and SEM-EDS.The results show that the precipitation rate of iron is more than 82% under the optimized conditions of titanium dioxide waste water volume of 50 mL,temperature of 20 ℃,sodium oxalate dosage of 12 g, stirring strength of 300 r/min and reaction time of 30 min, and the precipitate is the granular crystal of ferrous oxalate dihydrate with a purity of more than 98%.This study provides a method for efficient recovery of iron resources in acidic solution system.
quote
| GB/T 7714-2015 | [1] TAO Rong-rong, NIU Ze-peng, ZHU Xiao-bo, et al. Experimental Study on Preparation of Ferrous Oxalate with Titanium Dioxide Waste Water[J]. Rare Metals and Cemented Carbides, 2022(1): 6-9. |
| MLA | [1] TAO Rong-rong, et al., "Experimental Study on Preparation of Ferrous Oxalate with Titanium Dioxide Waste Water." Rare Metals and Cemented Carbides, no. 1, 2022, pp. 6-9. |
| APA | [1] TAO Rong-rong, NIU Ze-peng, ZHU Xiao-bo, LI Wang, & ZHANG Zhi-guo. (2022). Experimental Study on Preparation of Ferrous Oxalate with Titanium Dioxide Waste Water. Rare Metals and Cemented Carbides(1), 6-9. |
| IEEE | [1] TAO Rong-rong, NIU Ze-peng, ZHU Xiao-bo, LI Wang, and ZHANG Zhi-guo, "Experimental Study on Preparation of Ferrous Oxalate with Titanium Dioxide Waste Water," Rare Metals and Cemented Carbides, no. 1, pp. 6-9, 2022. keywords: {ferrous oxalate;crystal;precipitation;iron ion;titanium dioxide waste water} |