Study on the Kinetics of Extracting Vanadium and Iron from Sulfuric Acid Solution with P507 AITranslate

School of Chemistry and Chemical Engineering,Henan Polytechnic University;School of Chemistry and Chemical Engineering,Henan Polytechnic University;School of Chemistry and Chemical Engineering,Henan Polytechnic University;School of Chemistry and Chemical Engineering,Henan Polytechnic University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Vanadium is usually associated with other metals as a rare metal.A large number of impurity ions,such as iron,could exist in the sulfuric acid leaching solution of vanadium-bearing ore,which significantly impacts the subsequent separation and enrichment of vanadium.The study of extraction kinetics is an important method for determining the control steps in the extraction process,and the difficulty in extracting metal ions.A self-designed cylindrical constant interface cell was used to study the kinetics of extracting V(Ⅳ)and Fe(Ⅱ)from sulfuric acid solution with P507 as the extractant.The results show that the aqueous phase serves as the diffusion resistance zone of the extraction process,which is a chemical reaction-controlled type.The extraction rates of V(Ⅳ)and Fe(Ⅱ)both demonstrate an upward trend with the increase of stirring speed and extraction temperature.The apparent activation energy of V(Ⅳ)extraction is 48.68 kJ/mol,and that of Fe(Ⅱ)extraction is 135.11 kJ/mol.P507 is more likely to extract V(Ⅳ)from sulfuric acid solution,presenting the potential to achieve the efficient separation of V(Ⅳ)from Fe(Ⅱ).

KeyWords AITranslate

P507 extraction kinetics sulfuric acid vanadium iron

1吴伟民.鲜食中熟葡萄新品种——紫金秋浓[J].中国果业信息,2023,40(1):66-66.

2乔洪虎,杨向东.不同溶剂对光气介质体系影响比较[J].化工设计,2023,33(3):7-10.

3李通,崔凯辉,隋娜,黄焜.基于共存阳离子竞争吸附的稀土萃取过程界面盐效应[J].中国有色金属学报,2023,33(12):4201-4213.

4韦将.两款葡萄新品种[J].农村新技术,2022(4):43-44.

5Na Sui,Shukai Miao,Kaihui Cui,Fancheng Meng,Kun Huang.Non-equilibrium kinetic separation of thulium,yttrium and erbium on the surface of freely rising oil droplets[J].Journal of Rare Earths,2024,42(1):200-209.

6李洪博,韩东,张津榕,姜雪,葛富彪,胡振光.高浓度稀土浸出液的协同分步萃取试验研究[J].中国有色冶金,2023,52(6):53-59.

7杨和见,任宝光,陈小鹏,王琳琳,梁杰珍,张众尧.氢化松脂体系汽液平衡测定与关联[J].高校化学工程学报,2023,37(5):858-862.

8张严心,王梦祎,陈黎,周宇昊,陶文铨.Ca(OH)_(2)脱水过程数值研究及强化[J].工程热物理学报,2024,45(1):143-151.

9夏云生,赵屹萱,梁彦坤,林笑寒,田宝.Co-Ni催化剂的还原动力学[J].渤海大学学报(自然科学版),2023,44(4):317-320.

10谭金鹏,李伟锋,陈雪莉.预分选汽车破碎残余物热解特性及其动力学分析[J].环境工程学报,2023,17(11):3647-3659.

Basic Information:

DOI:

Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]

Citation Information:

Vanadium is usually associated with other metals as a rare metal.A large number of impurity ions,such as iron,could exist in the sulfuric acid leaching solution of vanadium-bearing ore,which significantly impacts the subsequent separation and enrichment of vanadium.The study of extraction kinetics is an important method for determining the control steps in the extraction process,and the difficulty in extracting metal ions.A self-designed cylindrical constant interface cell was used to study the kinetics of extracting V(Ⅳ)and Fe(Ⅱ)from sulfuric acid solution with P507 as the extractant.The results show that the aqueous phase serves as the diffusion resistance zone of the extraction process,which is a chemical reaction-controlled type.The extraction rates of V(Ⅳ)and Fe(Ⅱ)both demonstrate an upward trend with the increase of stirring speed and extraction temperature.The apparent activation energy of V(Ⅳ)extraction is 48.68 kJ/mol,and that of Fe(Ⅱ)extraction is 135.11 kJ/mol.P507 is more likely to extract V(Ⅳ)from sulfuric acid solution,presenting the potential to achieve the efficient separation of V(Ⅳ)from Fe(Ⅱ).

quote

GB/T 7714-2015 [1] LI Wang, WANG Lin, ZHU Xiao-bo, et al. Study on the Kinetics of Extracting Vanadium and Iron from Sulfuric Acid Solution with P507[J]. Rare Metals and Cemented Carbides, 2024(1): 1-5.
MLA [1] LI Wang, et al., "Study on the Kinetics of Extracting Vanadium and Iron from Sulfuric Acid Solution with P507." Rare Metals and Cemented Carbides, no. 1, 2024, pp. 1-5.
APA [1] LI Wang, WANG Lin, ZHU Xiao-bo, & LIU Yue. (2024). Study on the Kinetics of Extracting Vanadium and Iron from Sulfuric Acid Solution with P507. Rare Metals and Cemented Carbides(1), 1-5.
IEEE [1] LI Wang, WANG Lin, ZHU Xiao-bo, and LIU Yue, "Study on the Kinetics of Extracting Vanadium and Iron from Sulfuric Acid Solution with P507," Rare Metals and Cemented Carbides, no. 1, pp. 1-5, 2024. keywords: {P507;extraction;kinetics;sulfuric;acid;vanadium;iron}