Anti-dazzle Principle and Application of Nanometer-sized Compound Metal Oxide Films AITranslate
Abstract AITranslate
In this paper is described the anti-dazzle principle of nanometer-sized compound metal oxide films.A multi-layered films has a structure in which a material having a low refractive index and a material having a high refractive index are alternately stacked to form films.Its anti-reflection effect is a synergistic effect produced by the optical interference function of each layer.
KeyWords AITranslate
1郭玉忠,王剑华,黄瑞安,王贵青.掺杂SnO_2透明导电薄膜电学及光学性能研究[J].无机材料学报,2002,17(1):131-138. 被引量:42
2李青山,张金朝,宋鹂.三防纳米级ATO透明导电薄膜材料的研究和应用[J].材料导报,2002,16(2):34-36. 被引量:11
1李世平,李玲.添加纳米颗粒对复合镀层性能的影响[J].材料导报,2006,20(F05):75-78. 被引量:2
1李晖,谢华,邹刚.Ni-P-纳米SiC化学复合镀层组织与性能研究[J].表面技术,2009,38(1):37-39. 被引量:8
2杜登学,张志鹏,李文鹏,隋永红,王姗姗.镍基纳米复合镀层的研究进展[J].材料保护,2010,43(9):45-49. 被引量:4
1张天舒,沈瑜生.一种新型金属复合氧化物半导体气敏材料体系[J].传感器技术,1996,15(6):18-20. 被引量:4
2高鹏.高对比度防反射彩色显示管[J].彩色显像管,1995(3):37-41.
3赵博选.互补型自动防眩EC电致变色后视镜的研制[J].甘肃科技,2013,29(20):14-17. 被引量:1
4双层夜视增光眼镜[J].家庭科技,2008(1):16-16.
5宗平.新款单片车门区驱动芯片L99DZ70XP[J].军民两用技术与产品,2009(1):11-11.
6Elena Yu. KONYSHEVA.Reduction of CeO2 in composites with transition metal complex oxides under hydrogen containing atmosphere and its correlation with catalytic activity[J].化学科学与工程前沿:英文版,2013(3):249-261. 被引量:1
7苏锋.演绎成熟之美——摩托罗拉LM-P70显示器[J].微电脑世界,2004(17):46-46.
8任光林.PDP用防反射滤光膜[J].显示器件技术,2004(4):27-29. 被引量:1
9数码buy家[J].电脑爱好者,2008,0(22):102-102.
10冯春瑶,矫庆泽,李蕾,张春英,段雪.双(羟基)金属复合氧化物的表面改性[J].应用化学,2001,18(2):140-142. 被引量:21
Basic Information:
DOI:
Chinese Library Classification Number:TN104.3[电子电信—物理电子学];TB383[一般工业技术—材料科学与工程]
Citation Information:
In this paper is described the anti-dazzle principle of nanometer-sized compound metal oxide films.A multi-layered films has a structure in which a material having a low refractive index and a material having a high refractive index are alternately stacked to form films.Its anti-reflection effect is a synergistic effect produced by the optical interference function of each layer.
quote
| GB/T 7714-2015 | [1] LI Li-li, WANG Xiao-lan, DUAN Xue-chen. Anti-dazzle Principle and Application of Nanometer-sized Compound Metal Oxide Films[J]. Rare Metals and Cemented Carbides, 2003(4): 10-11. |
| MLA | [1] LI Li-li, et al., "Anti-dazzle Principle and Application of Nanometer-sized Compound Metal Oxide Films." Rare Metals and Cemented Carbides, no. 4, 2003, pp. 10-11. |
| APA | [1] LI Li-li, WANG Xiao-lan, & DUAN Xue-chen. (2003). Anti-dazzle Principle and Application of Nanometer-sized Compound Metal Oxide Films. Rare Metals and Cemented Carbides(4), 10-11. |
| IEEE | [1] LI Li-li, WANG Xiao-lan, and DUAN Xue-chen, "Anti-dazzle Principle and Application of Nanometer-sized Compound Metal Oxide Films," Rare Metals and Cemented Carbides, no. 4, pp. 10-11, 2003. keywords: {anti-reflection;anti-dazzle;conductive films;nanometer materials} |