daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Status on Preparation and Application of WC-Co Gradient Cemented Carbides for Mining AITranslate

Zigong Cemented Carbide Co.,Ltd.;Zigong Cemented Carbide Co.,Ltd.;Zigong Cemented Carbide Co.,Ltd.;Zigong Cemented Carbide Co.,Ltd.;Zigong Cemented Carbide Co.,Ltd.;Zigong Cemented Carbide Co.,Ltd.;Zigong Cemented Carbide Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The preparation methods of WC-Co gradient cemented carbides for mining at home and abroad are summarized,including carburizing,melt infiltration,layered pressing(construction)and locally coating grain inhibitor and sintering.The research status of these four methods and the application of gradient alloys are introduced.The constraints of promotion application of gradient cemented carbide as mining alloys are analyzed,and the application prospects of WC-Co gradient cemented carbides in mining and the technical problems in industrial production are prospected.

KeyWords AITranslate

gradient cemented carbide WC-Co application in mining research status application prospect

1郭圣达,吕健,陈颢,羊建高,钟明龙,朱二涛.非均匀结构硬质合金的研究现状及发展趋势[J].稀有金属与硬质合金,2013,41(6):67-69. 被引量:14

2余立新,胡惠勇.世界硬质合金材料技术新进展[J].硬质合金,2006,23(1):52-57. 被引量:25

3杨维才,吴恩熙.真空渗碳制备双相梯度硬质合金的研究[J].硬质合金,1999,16(3):154-158. 被引量:9

4孙绪新.梯度硬质合金的研制[J].粉末冶金技术,1998,16(4):260-264. 被引量:20

5张武装,刘咏,黄伯云,羊建高.WC-Co梯度结构硬质合金的研究进展[J].粉末冶金材料科学与工程,2004,9(2):121-125. 被引量:5

6余立新,陆庆忠,刘华平.渗碳法制备矿用梯度硬质合金[J].凿岩机械气动工具,2013,39(2):5-11. 被引量:1

7吴恩熙.国外梯度硬质合金的发展[J].稀有金属与硬质合金,1995,23(3):57-60. 被引量:18

8高荣根,李沐山.梯度结构硬质合金的开发与应用[J].硬质合金,2000,17(2):77-84. 被引量:15

9张立,黄伯云,吴恩熙.双相结构梯度硬质合金的研究现状[J].材料导报,2000,14(12):17-19. 被引量:17

10张立.相图在硬质合金成分与工艺设计中的应用[J].硬质合金,2000,17(2):69-71. 被引量:5

1葛世荣.采煤机技术发展历程(七)——截割机构[J].中国煤炭,2020,46(12):15-29. 被引量:2

2吕蓉,肖平安,顾景洪,古思敏,赵吉康.TiCp/Cr15高铬铸铁复合材料的制备与性能[J].复合材料学报,2021,38(9):2956-2964. 被引量:3

3武姜汝,冯校飞,韩日宏,齐海波.激光熔覆硬质相增强的镍基合金涂层性能的研究进展[J].热加工工艺,2022,51(14):18-22. 被引量:1

1葛世荣.采煤机技术发展历程(八)——可靠性技术[J].中国煤炭,2021,47(1):11-26. 被引量:6

2陈刚,邓人钦,贾寓真,刘国跃,吕蓉.WC_(p)/M42高速钢复合材料的制备与性能[J].有色金属工程,2022,12(8):30-38. 被引量:1

3江海湖,陈刚,贾寓真,刘国跃,胡莎,田茂森.NbC_(p)/ASP2030高速钢复合材料的制备与性能[J].有色金属工程,2023,13(5):23-30.

4赵吉康,肖平安,顾景洪,钟斯远.TiCN_(p)增强高铬铸铁复合材料的制备与性能[J].材料导报,2023,37(13):191-195.

5周梁栋,张亮,吴文恒,汪良,李翔,邹定锦.添加WC颗粒对钴基合金激光熔覆层组织形貌和显微硬度的影响研究[J].表面工程与再制造,2023,23(3):17-23.

6乔峰.长臂型采煤机摇臂故障分析及预防措施[J].煤矿机械,2023,44(8):180-183.

1王培安,吴淑芳,郭欢欢.前筒挤压成形方案分析与参数优化[J].西华大学学报:自然科学版,2019,38(3):32-42. 被引量:6

2郭广达,刘恩洋,刘甫,易镇江,朱少华,纪志康.颗粒增强镁基复合材料的制备技术与展望[J].铸造技术,2018,39(11):2632-2636.

3苑世剑,刘伟,王国峰,何祝斌,凡晓波.轻合金复杂薄壁构件流体压力成形技术新进展[J].上海航天,2019,36(2):31-37. 被引量:7

4谭千榆,王鹏,时凯华,曾伟.Co-Ni-Cr复合粘结相矿用合金的研制及生产[J].四川冶金,2019,41(3):29-33. 被引量:1

5刘绪超,杨发展,张娜,罗佳,魏海明.基于Workbench的微织构刀具对铝合金切屑影响[J].机床与液压,2019,47(16):12-16. 被引量:2

6虎琳,李崇俊,张永辉.RMI法制备C/C-SiC炭陶复合材料的热学性能研究[J].炭素技术,2017,36(6):24-27. 被引量:2

7王厚明,倪德印.榨油机榨螺的气体渗碳法[J].中国油脂,1981,0(4):1-11.

8吴云霞,吕凤军,邢立新,刘新星.独山城地区多元信息干热岩预测模型[J].吉林大学学报:地球科学版,2019,49(3):880-892. 被引量:3

9闫笑,同帜,王佳悦,刘婷,周广瑞.烧结温度对黄土陶瓷膜支撑体性能的影响[J].硅酸盐通报,2019,38(8):2657-2661. 被引量:2

10马文丽,阎峰云,魏富中,杨飞.SiC_p表面处理对SiC_p/6061Al复合材料性能的影响[J].热加工工艺,2019,48(14):71-74. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

The preparation methods of WC-Co gradient cemented carbides for mining at home and abroad are summarized,including carburizing,melt infiltration,layered pressing(construction)and locally coating grain inhibitor and sintering.The research status of these four methods and the application of gradient alloys are introduced.The constraints of promotion application of gradient cemented carbide as mining alloys are analyzed,and the application prospects of WC-Co gradient cemented carbides in mining and the technical problems in industrial production are prospected.

quote

GB/T 7714-2015 [1] GU Jin-bao, GAO Jian, SHI Kai-hua, et al. Research Status on Preparation and Application of WC-Co Gradient Cemented Carbides for Mining[J]. Rare Metals and Cemented Carbides, 2019(4): 83-88.
MLA [1] GU Jin-bao, et al., "Research Status on Preparation and Application of WC-Co Gradient Cemented Carbides for Mining." Rare Metals and Cemented Carbides, no. 4, 2019, pp. 83-88.
APA [1] GU Jin-bao, GAO Jian, SHI Kai-hua, SHU Jun, ZENG Wei, DONG Kai-lin, & DONG Ding-qian. (2019). Research Status on Preparation and Application of WC-Co Gradient Cemented Carbides for Mining. Rare Metals and Cemented Carbides(4), 83-88.
IEEE [1] GU Jin-bao, GAO Jian, SHI Kai-hua, SHU Jun, ZENG Wei, DONG Kai-lin, and DONG Ding-qian, "Research Status on Preparation and Application of WC-Co Gradient Cemented Carbides for Mining," Rare Metals and Cemented Carbides, no. 4, pp. 83-88, 2019. keywords: {gradient cemented carbide;WC-Co;application in mining;research status;application prospect}