Application and Research Status of Inhibitors in Cemented Carbides AITranslate
Abstract AITranslate
The types,adding methods,dosages and action mechanism of common grain growth inhibitors are described,and the effects of different inhibitors on the physical and mechanical properties of the cemented carbides are introduced.On the basis of a large number of research results,some existing problems in this field are pointed out,such as the differences of experimental results caused by the inconsistency of research methods,experimental conditions,types and dosages of inhibitors.
KeyWords AITranslate
1王文广,张贺佳,王全兆,马宗义,陈礼清.碳化物抑制剂对WC-2.5TiC-10Co超细晶硬质合金微观组织及力学性能的影响[J].材料研究学报,2015,29(12):881-888. 被引量:9
2付军,宋晓艳,魏崇斌,刘雪梅,王海滨,高杨,王瑶.复合添加晶粒长大抑制剂对WC-Co复合粉烧结硬质合金的影响[J].稀有金属材料与工程,2014,43(8):1928-1934. 被引量:11
3夏艳萍,余怀民,魏修宇,张卫兵.添加Cr3C2对WC-Co硬质合金微观组织和性能的影响[J].硬质合金,2017,34(5):300-305. 被引量:8
4罗重麟.稀土元素对硬质合金性能影响的研究[J].硬质合金,1991,8(2):12-19. 被引量:24
5邱智海.WC-Co硬质合金中的添加剂[J].硬质合金,2004,21(2):121-124. 被引量:10
6张祎,马俊,狄平,朱世根.La_2O_3对WC-MgO复合材料组织和力学性能的影响[J].中国有色金属学报,2010,20(10):1982-1988. 被引量:4
7贾佐诚.超细晶硬质合金的发展[J].硬质合金,2000,17(1):58-63. 被引量:42
8张雪辉,黄柱,徐畅,李晓闲,蔡志勇,陈颢.Cr_3C_2对SPS烧结WC-6Co硬质合金组织与性能的影响[J].中国有色金属学报,2017,27(8):1580-1588. 被引量:10
9吴厚平,张立,王振波,陈述,熊湘君.镧、铈在WC-Co合金中赋存状态的研究[J].中国稀土学报,2009,27(5):693-697. 被引量:9
10李体军,熊计,郭智兴,杨天恩,周黎明.WC-x%TiC-6%Co硬质合金特征及冲刷磨损性能的研究[J].硬质合金,2017,34(2):129-135. 被引量:6
1汪振华,刘奎,黄雷,袁军堂.放电等离子烧结WC-6wt.%Co-VC超细晶硬质合金力学性能和微观组织研究[J].南京理工大学学报,2020,44(5):524-530. 被引量:2
2杨诚辉,徐国钻,刘如铁,张龙辉,羊求民.不同氧化钨还原制备钨粉及其特性研究[J].稀有金属与硬质合金,2022,50(2):19-25. 被引量:1
3袁军文,曾瑞霖,徐涛,尹超,董涛.含钒添加剂对纳米硬质合金性能的影响[J].硬质合金,2023,40(1):1-7.
4黄公治,尹超,蒋甘澍.碳化物抑制剂在硬质合金中的应用与研发现状[J].硬质合金,2023,40(2):147-157.
1罗鑫,洪源昆,吴佳逸,李绍轩,羊求民.超细硬质合金WC晶粒大小对其摩擦磨损性能的影响[J].稀有金属与硬质合金,2022,50(3):93-97.
2王红云,王韶毅,刘莉,唐彦渊,羊求民.配碳量对原位碳热反应制备Co_(x)W_(y)C复合粉末微观结构的影响[J].稀有金属与硬质合金,2022,50(5):47-51.
3袁军文,曾瑞霖,徐涛,尹超,董涛.含钒添加剂对纳米硬质合金性能的影响[J].硬质合金,2023,40(1):1-7.
1米深深,肖然,王姣,李荣华,张增强.添加方式对不同固化剂稳定土壤重金属的影响[J].农业环境科学学报,2019,38(8):1946-1953. 被引量:5
2钟欣平,喻阳华,杨丹丽,侯堂春.干热河谷石漠化区火龙果地不同耕作方式的土壤矿质元素特征[J].广西植物,2019,39(8):1050-1058. 被引量:2
3何伟锋,陈勇志.工艺参数对WC-Co硬质合金组织及力学性能的影响[J].热加工工艺,2019,48(14):75-79. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The types,adding methods,dosages and action mechanism of common grain growth inhibitors are described,and the effects of different inhibitors on the physical and mechanical properties of the cemented carbides are introduced.On the basis of a large number of research results,some existing problems in this field are pointed out,such as the differences of experimental results caused by the inconsistency of research methods,experimental conditions,types and dosages of inhibitors.
quote
| GB/T 7714-2015 | [1] DONG Kai-lin, SHI kai-hua, GU Jin-bao, et al. Application and Research Status of Inhibitors in Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2019(4): 76-82. |
| MLA | [1] DONG Kai-lin, et al., "Application and Research Status of Inhibitors in Cemented Carbides." Rare Metals and Cemented Carbides, no. 4, 2019, pp. 76-82. |
| APA | [1] DONG Kai-lin, SHI kai-hua, GU Jin-bao, ZENG Wei, & WU Xiang. (2019). Application and Research Status of Inhibitors in Cemented Carbides. Rare Metals and Cemented Carbides(4), 76-82. |
| IEEE | [1] DONG Kai-lin, SHI kai-hua, GU Jin-bao, ZENG Wei, and WU Xiang, "Application and Research Status of Inhibitors in Cemented Carbides," Rare Metals and Cemented Carbides, no. 4, pp. 76-82, 2019. keywords: {cemented carbide;inhibitor;action mechanism;property} |