Cr-Si Co-impregnation by Double Glow Plasma Surface Alloying Technique and Wear Resistance Improvement of γ-TiAl-based Alloy AITranslate

Nanjing University of Aeronautics and Astronautics University of Materials Science and Technology;Nanjing University of Aeronautics and Astronautics University of Materials Science and Technology;Nanjing University of Aeronautics and Astronautics University of Materials Science and Technology;Nanjing University of Aeronautics and Astronautics University of Materials Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cr-Si co-impregnation on surface of γ-TiAl-based alloy was carried out by double glow plasma surface alloying technique. Morphology, composition and phase structure were investigated by OM, SEM and XRD. The hardness of the impregnation layer was determined by micro Vickers hardness tester. The influences of Cr-Si co-impregnation on wear resistance of γ-TiAl-based alloy surface were studied through ball-disc friction and wear experiments without lubrication. The results show that there are three sublayers on the alloy impregnation surface. The element content changes continuously in the impregnation layer. The impregnation layer is combined with the substrate by metallurgical bonding. Hardness of the alloy surface increases to HV0.11 200~ l 250. The transition layer connected to the substrate is of better strength and toughness ,which can effectively improve the wear resistance of the alloy.

KeyWords AITranslate

γ-TiAl-based alloy plasma metal impregnation Cr-Si co-impregnation wear resistance

1李成明,贺志勇,徐重.离子钨钼共渗的扩散机制[J].中国有色金属学报,2000,10(2):185-188. 被引量:6

2吴红艳,张平则,马士剑,徐重.Ti2AlNb基合金等离子表面渗铬层组织结构对耐磨性能的影响[J].润滑与密封,2007,32(6):68-70. 被引量:3

3魏世忠,朱金华,徐流杰,龙锐.残余奥氏体量对高钒高速钢性能的影响[J].材料热处理学报,2005,26(1):44-47. 被引量:29

4MAXiao-xia LIANGWei ZHAOXing-guo SHIJu-yan BIANLi-ping.Study on the Formation Mechanism of the Solid Siliconized Layer on Ti-48Al Alloy[J].材料热处理学报,2004,25(05B):681-683. 被引量:1

5陈国良.金属间化合物结构材料研究现状与发展[J].材料导报,2000,14(9):1-5. 被引量:74

6张平则,李忠厚,贺志勇,徐重,张高会.Ti-6Al-4V表面双层辉光离子渗Cr研究[J].兵器材料科学与工程,2005,28(1):17-20. 被引量:22

7马士剑,张平则,缪强,徐重.γ-TiAl辉光等离子无氢渗碳后的组织及性能研究[J].热处理,2007,22(5):26-29. 被引量:2

8梁文萍,徐重,缪强,刘小萍,贺志勇.Ti_2AlNbO相合金双层辉光等离子渗Mo摩擦性能[J].稀有金属材料与工程,2006,35(11):1826-1829. 被引量:10

9田宗军,王东生,沈理达,刘志东,黄因慧.等离子喷涂纳米Al_2O_3-13TiO_2陶瓷涂层研究[J].稀有金属材料与工程,2009,38(10):1740-1744. 被引量:11

10田宗军,王东生,沈理达,黄因慧,刘志东.TiAl合金表面激光重熔陶瓷涂层组织及耐磨性能[J].南京航空航天大学学报,2009,41(3):348-353. 被引量:5

1李梅,田晓东,王甜甜,李保忠.纯钼Cr-Si共渗层的组织及形成机理[J].金属热处理,2016,41(7):83-86. 被引量:2

2陆小会,高原,韦文竹,张光耀,蔡航伟,王成磊.稀土表面高速钢磨粒磨损耐磨性研究[J].稀有金属,2013,37(5):750-756. 被引量:5

3刘沙沙,陈志勇,李忠厚.超硬高速钢的表面冶金工艺研究[J].热加工工艺,2007,36(20):56-58.

4张维,高原,袁琳,王成磊.W-Mo-Dy三元共渗合金层的研究[J].材料热处理学报,2011,32(S1):140-143. 被引量:1

5李忠厚,张艳梅,张平则,徐重.基材碳含量对离子渗W、Mo、Co的影响[J].材料热处理学报,2004,25(6):91-95. 被引量:11

6李冰,高原,陈选楠,黄学锋,赖涛,陈文琦.等离子共渗W-Mo-Y工艺及渗层组织的研究[J].表面技术,2011,40(1):86-89. 被引量:1

7张维平,马海波.铜合金表面激光熔覆研究现状[J].机械工程材料,2009,33(9):6-9. 被引量:8

8高原,袁琳,陈选楠,张维,李冰,黄学峰.Q195钢表面等离子铬-镍共渗的扩散机理分析[J].稀有金属材料与工程,2012,41(S2):272-274. 被引量:1

9李冰,高原,王成磊,陈选楠,黄学锋.等离子W、Mo、Y共渗层的组织研究[J].稀有金属材料与工程,2012,41(S2):10-13. 被引量:2

10高原,张维,王成磊,李冰,陈选楠,黄学锋,袁琳.W-Mo-Y等离子共渗合金层的研究[J].材料热处理学报,2011,32(7):130-133. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG178[金属学及工艺—金属表面处理]

Citation Information:

Cr-Si co-impregnation on surface of γ-TiAl-based alloy was carried out by double glow plasma surface alloying technique. Morphology, composition and phase structure were investigated by OM, SEM and XRD. The hardness of the impregnation layer was determined by micro Vickers hardness tester. The influences of Cr-Si co-impregnation on wear resistance of γ-TiAl-based alloy surface were studied through ball-disc friction and wear experiments without lubrication. The results show that there are three sublayers on the alloy impregnation surface. The element content changes continuously in the impregnation layer. The impregnation layer is combined with the substrate by metallurgical bonding. Hardness of the alloy surface increases to HV0.11 200~ l 250. The transition layer connected to the substrate is of better strength and toughness ,which can effectively improve the wear resistance of the alloy.

quote

GB/T 7714-2015 [1] LI Ya-fei, ZHANG Ping-ze, LI Chuang, et al. Cr-Si Co-impregnation by Double Glow Plasma Surface Alloying Technique and Wear Resistance Improvement of γ-TiAl-based Alloy[J]. Rare Metals and Cemented Carbides, 2011(3): 38-43.
MLA [1] LI Ya-fei, et al., "Cr-Si Co-impregnation by Double Glow Plasma Surface Alloying Technique and Wear Resistance Improvement of γ-TiAl-based Alloy." Rare Metals and Cemented Carbides, no. 3, 2011, pp. 38-43.
APA [1] LI Ya-fei, ZHANG Ping-ze, LI Chuang, & YU Jin-wen. (2011). Cr-Si Co-impregnation by Double Glow Plasma Surface Alloying Technique and Wear Resistance Improvement of γ-TiAl-based Alloy. Rare Metals and Cemented Carbides(3), 38-43.
IEEE [1] LI Ya-fei, ZHANG Ping-ze, LI Chuang, and YU Jin-wen, "Cr-Si Co-impregnation by Double Glow Plasma Surface Alloying Technique and Wear Resistance Improvement of γ-TiAl-based Alloy," Rare Metals and Cemented Carbides, no. 3, pp. 38-43, 2011. keywords: {γ-TiAl-based alloy;plasma metal impregnation;Cr-Si co-impregnation wear resistance}