Analysis and the Latest Research of Basic Mechanics on Efficacy Loss of Hydrogen Storage Alloy Electrode AITranslate
Abstract AITranslate
Analysis is made of the basic mechanics about efficacy loss of the electrode, such as pulverization of alloy particle, oxidation of element, amorphous after hydrogen absorption and crystalline after hydrogen desorption,and electrochemical corrosion. The latest research is reviewed. The way how to restrain or lower capacity degradation of electrode and improve cyclic property of hydrogen storage alloy electrode is introduced.
KeyWords AITranslate
1杨丽颖,董小平,耿晓光,王青,林玉芳,张羊换.稀土镁镍系合金的循环贮氢性能与粉化特性研究[J].粉末冶金工业,2011,21(2):19-24. 被引量:5
2Liao B,Lei Y Q,Chen L X,et al. Effect of the La/Mg ratio on the structure and electrochemical properties of Lax Mg3-x Ni9 (co = 1.6 - 2.2) hydrogen storage electrode alloys for nickelmetal hydride batteries [J]. J Power Sources, 2004,129 (2) : 358-367.
3.朱光潜美学文集(二)[M].上海:上海文艺出版社,1983.344-345.
4周增林,宋月清,黄长庚,崔舜,张永健,李学军,黄倬.热处理对La_(0.7)Mg_(0.3)(Ni_(0.85)Co_(0.15))_(3.4)贮氢电极合金性能的影响[J].西安交通大学学报,2007,41(11):1373-1379. 被引量:6
5Tanaka H, Senoh H, Kuriyama N, et al. Cycle durability of Ca-Mg-Ni alloys and factors which cause degradation of hydrogen storage capacity[J]. Materials Science and Engineering B,2004,108:81-90.
6Liu Y F,Pan H G,Gao M X,et al. Function of Al on the cycling behavior of the La-Mg-Ni-Co-type alloy electrodes[J]. International Journal of Hydrogen Energy, 2008,33:124-133.
7Dong X P, Zhang Y H, Lu F X, et al. Investigation on microstructures and electrochemical performances of La0.75 Mg0.25 Ni3.5 Cox (x = 0 - 0.6 ) hydrogen storage alloys [J]. International Journal of Hydrogen Energy, 2007,32(18) :4 949-4 956.
8Liu Y F,Pan H G,Yue Y J,etal. Cycling durability and degradation behavior of La-Mg-Ni-Co-type metal hydride electrodes[J]. Journal of Alloys and Compounds, 2005, 395(1-2) :291-299.
9Shang G Y,Han S M,Hao J S,etal. Study on self-discharge property of Nd0. 88 Mg0. 12 Ni3. 10 +x Al0. 20 (x = 0.00, 0.10,0. 20,0. 30) hydrogen storage alloys[J]. Journal of Alloys and Compounds,2010, 493: 573-576.
10Wang Y Z, Zhao M S. Structure and electrochemical characteristics of Ti0.10 Zr0. 15 V0. 35 Cr0.10 Ni0. 30 -LaNi4 Al0. 4 Mn0. 3Co0.3 composite hydrogen storage alloy[J]. International Journal of Hydrogen Energy, 2010,35 (12) : 8 268-8 274.
1邢磊,李一鸣,张羊换,任慧平,金自力.快淬-退火La_4MgNi_(19)合金的电化学储氢性能及其失效行为[J].稀有金属,2017,41(12):1318-1326. 被引量:5
2郑坤,杨倩,杨洋,罗永春.La0.7Y0.3Ni3.4-xMnxAl0.1(Х=0~0.5)储氢合金微观结构和电化学性能[J].金属功能材料,2020,27(1):16-23. 被引量:6
1Yang-Huan Zhang,Gang Huang,Ze-Ming Yuan,Shi-Hai Guo,Yan Qi,Dong-Liang Zhao.Electrochemical hydrogen storage behaviors of as-cast and spun RE-Mg-Ni-Co-Al-based AB2-type alloys applied to Ni-MH battery[J].稀有金属:英文版,2020,0(2):181-192. 被引量:1
2徐庆飞,翟亭亭,韩忠刚,张羊换.Pr替代Ti对TiFe系储氢合金微观结构和电化学性能的影响[J].金属功能材料,2021,28(3):42-48. 被引量:2
3杨洋,姜婉婷,邓安强,罗永春.R-Y-Ni系A5B19型(R=Y,La,Pr,Nd,Sm)储氢合金的微观结构和电化学性能[J].金属功能材料,2021,28(4):13-19. 被引量:2
4佘翔,刘冬梅,李雪.电动汽车用La-Fe-B储氢合金的制备与电化学性能研究[J].无机盐工业,2021,53(10):64-69. 被引量:2
5程丽群,左付山.新能源汽车电池用无镁储氢合金的制备与性能研究[J].无机盐工业,2021,53(11):71-76. 被引量:3
6侯晓东,邓安强,赵刘强,杨洋,罗永春.Co元素对La-Y-Ni系A_(2)B_(7)型储氢合金的微观结构及电化学性能的影响[J].金属功能材料,2021,28(6):1-8. 被引量:4
7聂光辉,魏垂泉.热处理对新能源汽车用(La_(0.7)Mg_(0.3))Ni_(x)合金储氢特性的影响研究[J].热加工工艺,2021,50(24):39-42. 被引量:1
8郗玉平,罗志欢,田可欣.快淬速度对汽车用储氢合金电化学性能的影响[J].实验室研究与探索,2022,41(2):8-12. 被引量:1
9李通,罗新宇,陈子然.退火温度对汽车镍氢电池用储氢合金电化学性能的影响[J].稀土,2022,43(5):93-101.
10苑慧萍,李志念,沈浩,蒋利军.稀土储氢材料的研究进展[J].中国材料进展,2023,42(2):98-104. 被引量:1
1徐梅,郦剑,董仕节.点焊电极失效的研究进展[J].热加工工艺,2003,32(4):46-48. 被引量:10
2帅歌旺,方平,郭正华,郭吉萍.镀锌钢板电阻点焊电极的失效分析[J].热加工工艺,2009,38(13):122-124. 被引量:14
3董仕节,ZHOU Norman.点焊镀锌钢板时电极表面熔敷TiC涂层对电极失效的影响[J].中国有色金属学报,2005,15(2):184-191. 被引量:22
4常保华,都东,陈强,Zhou Y.电极点蚀形貌对铝合金电阻点焊的影响[J].焊接学报,2007,28(5):29-32.
5张清,李全安,文九巴,张兴渊.镀镍对AB_5型贮氢合金电化学性能的影响[J].表面技术,2006,35(3):23-24. 被引量:3
6申海燕.锂离子电池正极材料Li_xMn_2O_4的研究进展[J].湖南冶金,2005,33(6):3-7.
7董仕节,Y.Zhou.表面处理对微型点焊镀镍钢板和镍板时电极失效的影响[J].湖北汽车工业学院学报,2002,16(2):11-16. 被引量:2
8董仕节,Zhou Norman.点焊镀锌钢板时球形电极表面熔敷TiC涂层对电极失效的分析[J].湖北汽车工业学院学报,2004,18(4):26-30. 被引量:2
9李青松,罗震,李中伟,张东文.铝合金电阻点焊电极延寿技术的研究[J].电焊机,2009,39(7):59-61. 被引量:3
10郑雪萍,曲选辉.锂离子电池正极材料LiMn_2O_4研究现状[J].稀有金属快报,2005,24(7):1-5. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TG139.7[一般工业技术—材料科学与工程]
Citation Information:
Analysis is made of the basic mechanics about efficacy loss of the electrode, such as pulverization of alloy particle, oxidation of element, amorphous after hydrogen absorption and crystalline after hydrogen desorption,and electrochemical corrosion. The latest research is reviewed. The way how to restrain or lower capacity degradation of electrode and improve cyclic property of hydrogen storage alloy electrode is introduced.
quote
| GB/T 7714-2015 | [1] DONG Xiao-ping, YANG Li-ying, ZHU Kai-ning, et al. Analysis and the Latest Research of Basic Mechanics on Efficacy Loss of Hydrogen Storage Alloy Electrode[J]. Rare Metals and Cemented Carbides, 2011(4): 25-30. |
| MLA | [1] DONG Xiao-ping, et al., "Analysis and the Latest Research of Basic Mechanics on Efficacy Loss of Hydrogen Storage Alloy Electrode." Rare Metals and Cemented Carbides, no. 4, 2011, pp. 25-30. |
| APA | [1] DONG Xiao-ping, YANG Li-ying, ZHU Kai-ning, WANG Tao, & ZHONG Yang. (2011). Analysis and the Latest Research of Basic Mechanics on Efficacy Loss of Hydrogen Storage Alloy Electrode. Rare Metals and Cemented Carbides(4), 25-30. |
| IEEE | [1] DONG Xiao-ping, YANG Li-ying, ZHU Kai-ning, WANG Tao, and ZHONG Yang, "Analysis and the Latest Research of Basic Mechanics on Efficacy Loss of Hydrogen Storage Alloy Electrode," Rare Metals and Cemented Carbides, no. 4, pp. 25-30, 2011. keywords: {hydrogen storage alloy;efficacy loss of electrode;capacity degradation;cyclic property} |