daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Composition-temperature phase diagram of BexZn1−xO from first principles AITranslate

Institute of High Performance Computing; Nanyang Technological University; Nanyang Technological University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Density-functional calculations have been performed to obtain the composition-temperature phase diagram for the BexZn1−xO alloys. Consistent density-functional theory within local density approximation has been employed for relaxing the atomic structures, calculating the enthalpy of formation, and determining the lattice vibrational contributions to the free energy. The results show that lattice vibrations significantly reduce the critical temperature. The predicted phase diagram is consistent with the experimental observation that alloying Mg with BexZn1−xO suppresses phase separation.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.01.040

Chinese Library Classification Number:

Citation Information:

Density-functional calculations have been performed to obtain the composition-temperature phase diagram for the BexZn1−xO alloys. Consistent density-functional theory within local density approximation has been employed for relaxing the atomic structures, calculating the enthalpy of formation, and determining the lattice vibrational contributions to the free energy. The results show that lattice vibrations significantly reduce the critical temperature. The predicted phase diagram is consistent with the experimental observation that alloying Mg with BexZn1−xO suppresses phase separation.

quote

GB/T 7714-2015 [1] Chee Kwan Gan, Xiao Feng Fan, JerLai Kuo. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.01.040.
MLA [1] Chee Kwan Gan, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.01.040.