The stress–strain behavior of WC-Co hardmetals AITranslate

V. Bakul Institute for Superhard Materials of the National Academy of Sciences of Ukraine;V. Bakul Institute for Superhard Materials of the National Academy of Sciences of Ukraine
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The calculating algorithm for construction of the stress–strain curves of WC-Co hardmetals in simple tension and compression has been described. The algorithm is based on the mathematical means of mechanics of composite materials and in situ deformation properties of constituents. The mean field approach has been applied. The stress–strain behavior depends on such microstructural parameters as cobalt volume fraction, mean carbide grain size, and contiguity of carbide phase. The technological thermal residual microstresses have been taken into account. The wide comparison of theoretical and available experimental results has been done. It has been shown, that the given calculating algorithm has the good predictive capability. The analytical expressions of tensile and compressive strength of WC-Co hardmetals have been given.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.05.055

Chinese Library Classification Number:

Citation Information:

The calculating algorithm for construction of the stress–strain curves of WC-Co hardmetals in simple tension and compression has been described. The algorithm is based on the mathematical means of mechanics of composite materials and in situ deformation properties of constituents. The mean field approach has been applied. The stress–strain behavior depends on such microstructural parameters as cobalt volume fraction, mean carbide grain size, and contiguity of carbide phase. The technological thermal residual microstresses have been taken into account. The wide comparison of theoretical and available experimental results has been done. It has been shown, that the given calculating algorithm has the good predictive capability. The analytical expressions of tensile and compressive strength of WC-Co hardmetals have been given.

quote

GB/T 7714-2015 [1] V.T. Golovchan, N.V. Litoshenko. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.05.055.
MLA [1] V.T. Golovchan, and N.V. Litoshenko. Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.05.055.
APA [1] V.T. Golovchan, & N.V. Litoshenko. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.05.055
IEEE [1] V.T. Golovchan and N.V. Litoshenko, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.05.055.