daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Biocompatible, Flexible, and Oxygen-Permeable Silicone-Hydrogel Material for Stereolithographic Printing of Microfluidic Lab-On-A-Chip and Cell-Culture Devices AITranslate

Technical University of Munich; 1950 University Avenue Suite 600; Technical University of Munich; Technical University of Munich; 1950 University Avenue Suite 600; Technical University of Munich; Technical University of Munich; Technical University of Munich; 1950 University Avenue Suite 600
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We present a photocurable, biocompatible, and flexible silicone-hydrogel hybrid material for stereolithographic (SLA) printing of biomedical devices. The silicone-hydrogel polymer is similar to mixtures used for contact lenses. It is flexible and stretchable with a Young’s modulus of 78 MPa and a maximum elongation at break of 51%, shows a low degree of swelling (<4% v/v) in water, and can be bonded easily to flat glass substrates via a surface-modification method. The in vitro cytotoxicity of the material is assessed with a WST-8 cell viability assay using five different cell lines: HT1080, L929, and Hs27 fibroblasts, cardiomyocyte-like HL-1 cells, and neuronal-phenotype PC-12 cells. On this account, the silicone-hydrogel polymer is compared to several other common SLA printing materials used for cell-culture applications and polydimethylsiloxane (PDMS). A simple extraction step in water is sufficient for reaching biocompatibility of the material with respect to the tested cell types. The oxygen permeability of the silicone-hydrogel material is investigated and compared to that of PDMS, Medicalprint clear─a commercial resin for medical products, and a short-chain hydrogel-based resin. As a proof of concept, we demonstrate a 3D-printed microfluidic device with integrated valves and mixers. Furthermore, we show a printed culture chamber for analyzing signal propagation in HL-1 cardiomyocyte cell networks. Ca2+ imaging is used to observe the signal propagation through the cardiac cell layers grown in the microchannels. The cells are shown to maintain normal electrophysiological activity within the printed chambers. Overall, the biocompatible silicone-hydrogel material will be an advancement for SLA printing in cell-culture and microfluidic lab-on-a-chip applications.

KeyWords AITranslate

stereolithographic printing silicones hydrogels biocompatible materials flexible materials
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01071

Chinese Library Classification Number:

Citation Information:

We present a photocurable, biocompatible, and flexible silicone-hydrogel hybrid material for stereolithographic (SLA) printing of biomedical devices. The silicone-hydrogel polymer is similar to mixtures used for contact lenses. It is flexible and stretchable with a Young’s modulus of 78 MPa and a maximum elongation at break of 51%, shows a low degree of swelling (<4% v/v) in water, and can be bonded easily to flat glass substrates via a surface-modification method. The in vitro cytotoxicity of the material is assessed with a WST-8 cell viability assay using five different cell lines: HT1080, L929, and Hs27 fibroblasts, cardiomyocyte-like HL-1 cells, and neuronal-phenotype PC-12 cells. On this account, the silicone-hydrogel polymer is compared to several other common SLA printing materials used for cell-culture applications and polydimethylsiloxane (PDMS). A simple extraction step in water is sufficient for reaching biocompatibility of the material with respect to the tested cell types. The oxygen permeability of the silicone-hydrogel material is investigated and compared to that of PDMS, Medicalprint clear─a commercial resin for medical products, and a short-chain hydrogel-based resin. As a proof of concept, we demonstrate a 3D-printed microfluidic device with integrated valves and mixers. Furthermore, we show a printed culture chamber for analyzing signal propagation in HL-1 cardiomyocyte cell networks. Ca2+ imaging is used to observe the signal propagation through the cardiac cell layers grown in the microchannels. The cells are shown to maintain normal electrophysiological activity within the printed chambers. Overall, the biocompatible silicone-hydrogel material will be an advancement for SLA printing in cell-culture and microfluidic lab-on-a-chip applications.

quote

GB/T 7714-2015 [1] Sabine Zips, Lukas Hiendlmeier, Lennart Jakob Konstantin Weiß, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01071.
MLA [1] Sabine Zips, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01071.
APA [1] Sabine Zips, Lukas Hiendlmeier, Lennart Jakob Konstantin Weiß, Heike Url, Tetsuhiko F. Teshima, Richard Schmid, Markus Eblenkamp, Petra Mela, & Bernhard Wolfrum. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01071
IEEE [1] Sabine Zips, Lukas Hiendlmeier, Lennart Jakob Konstantin Weiß, Heike Url, Tetsuhiko F. Teshima, Richard Schmid, Markus Eblenkamp, Petra Mela, and Bernhard Wolfrum, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01071. keywords: {stereolithographic printing;silicones;hydrogels;biocompatible materials;flexible materials}