The Latest Development of the Cemented Carbide Buttons AITranslate
Abstract AITranslate
The comparison of grades and properties is conducted between cemented carbide buttons at home and abroad. Meanwhile, the latest development is summarized in respect of alloy materials, preparation process and button profile of cemented carbide buttons, and the improvement methods of alloy materials are detailed in respect of superfine-crystallization and nano-crystallization, functional gradient optimization and trace element addition. Besides, the suggestions are made to the future development of cemented carbide buttons.
KeyWords AITranslate
1Ulrik Beste. On the nature of cemented carbide wear in rock drilling[D]. Uppsala: Uppsala University, 2004.
2中国产业信息网.我国硬质合金产量两年内或达3万吨[EB/OL].http://www.hardalloy.corn.cn/news-info.asp?id=13072,2013-05-14.
3宁曙光,李常春.耐钝硬质合金齿[J].凿岩机械气动工具,1994,20(4):28-31. 被引量:2
4周建华,卢伟民.国内外硬质合金生产现状及近期发展动向分析[J].稀有金属与硬质合金,2006,34(1):36-41. 被引量:25
5Porat R,Berger S, Rosen A. Synthesis and processing of nanocrystalline WC-Co powders[J]. Proceedings of the 14th International Plansee Seminar, 1997,2 : 183-187.
6冯国磊,陈家旺.纳米材料用于复合柱齿的实验研究[J].矿业研究与开发,2004,24(5):58-59. 被引量:1
7张愈祖,周建华,卢伟民.国内外矿用硬质合金研究的新进展[J].凿岩机械气动工具,2004,30(2):30-34. 被引量:4
8Upadhyaya A, Sarathy D, Wagner G Advances in alloy design aspects of cemented carbides [J]. Materials andDesign,2001,22(6) :511 -517.
9Sandvik R T. PM special feature rock tools leads the way in drilling[J]. Metal Powder Rep, 1992,47( 12): 48 -50.
10程秀兰,刘宇.硬质合金梯度球齿的研究[J].硬质合金,2002,19(Z):37-41.
1谭千榆,王鹏,时凯华,曾伟.Co-Ni-Cr复合粘结相矿用合金的研制及生产[J].四川冶金,2019,41(3):29-33. 被引量:1
2王艳芝,李启泉,刘书锋,王长通.高性能工程工具截齿材料的研究进展概述[J].中原工学院学报,2019,30(3):18-21.
3文晓.矿用WC-Co硬质合金球齿的失效分析与改善[J].福建冶金,2019,48(6):23-27.
4邹芹,张萌蕾,李艳国.添加剂改性WC硬质合金的性能与应用研究[J].制造技术与机床,2021(7):9-15. 被引量:2
1陈振磊,喻琛,邵鸣宇.不同粘结相硬质合金的研究进展[J].机械研究与应用,2021,34(5):204-209. 被引量:2
2曹瑞军,李开深,李腾飞,何盛亚.金刚石含量对金刚石强化硬质合金耐磨性影响[J].硬质合金,2022,39(3):165-171. 被引量:1
3王春光,张立,黄祥,聂仁鑫,钟志强,龙佳威.合金添加剂对WC基硬质合金氧化行为及其关联特性的影响[J].粉末冶金材料科学与工程,2023,28(3):296-304. 被引量:1
1杨强.钒钛磁铁矿冶炼条件下高炉炉前耐火材料的改进[J].钢铁钒钛,2012,33(2):67-70. 被引量:1
2Evans,D,陈晓勇.氧气炼钢耐火材料的改进[J].国外耐火材料,1991,16(3):33-36.
3宫川信夫,胡山.转炉出钢口耐火材料的改进[J].江西冶金,1989,9(4):39-41.
4杨立志.AOD炉用耐火材料的改进(摘译)[J].太钢译文,1995(3):1-4.
5张志仁.鹿岛制铁所RH精炼炉用耐火材料的改进[J].太钢译文,1994(2):1-6.
6郭杰,张海奇.钢包寿命的提高及耐火材料的改进[J].耐火材料,1998,32(6):359-360.
7程秀梅.精炼钢包用耐火材料的改进[J].国外耐火材料,1994,19(9):34-37. 被引量:1
8王鲁毅,王福有,孙贵春.900t回转窑耐火材料的改进[J].鞍钢技术,2009(4):59-62. 被引量:2
9覃伟坚.功能梯度硬质合金球齿的研制[J].中国钨业,1999,14(5):198-201. 被引量:11
10邢守正.环冷机耐火材料的改进[J].矿业工程,2013,11(3):38-39.
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
The comparison of grades and properties is conducted between cemented carbide buttons at home and abroad. Meanwhile, the latest development is summarized in respect of alloy materials, preparation process and button profile of cemented carbide buttons, and the improvement methods of alloy materials are detailed in respect of superfine-crystallization and nano-crystallization, functional gradient optimization and trace element addition. Besides, the suggestions are made to the future development of cemented carbide buttons.
quote
| GB/T 7714-2015 | [1] MIN Zhao-yu, LIAO Jun, ZAN Xiu-qi, et al. The Latest Development of the Cemented Carbide Buttons[J]. Rare Metals and Cemented Carbides, 2013(5): 56-61. |
| MLA | [1] MIN Zhao-yu, et al., "The Latest Development of the Cemented Carbide Buttons." Rare Metals and Cemented Carbides, no. 5, 2013, pp. 56-61. |
| APA | [1] MIN Zhao-yu, LIAO Jun, ZAN Xiu-qi, & SHI Kai-hua. (2013). The Latest Development of the Cemented Carbide Buttons. Rare Metals and Cemented Carbides(5), 56-61. |
| IEEE | [1] MIN Zhao-yu, LIAO Jun, ZAN Xiu-qi, and SHI Kai-hua, "The Latest Development of the Cemented Carbide Buttons," Rare Metals and Cemented Carbides, no. 5, pp. 56-61, 2013. keywords: {cemented carbide button;alloy material;preparation process;button profile;the latest development;suggestion} |