Nonfullerene Ternary Organic Photovoltaics with Long-Wavelength Light-Absorption Guest Donor Materials to Improve Photovoltaic Performance AITranslate

Yunnan Normal University; Yunnan Normal University; Yunnan Minzu University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In order to achieve efficient organic photovoltaics (OPVs), a ternary strategy was adopted with the efficient long-wavelength light-absorption donor material of PSBTBT as the third component material (guest donor) and the D18-Cl:BTP-eC9 binary film as the host photoactive layer, which facilitates the acquisition of absorption spectra complementary to those of D18-Cl and BTP-eC9. The PL spectrum of D18-Cl was covered by the absorption spectrum of PSBTBT, which further supports the energy transfer from D18-Cl to PSBTBT. In addition, the addition of a small amount of PSBTBT to the D18-Cl:BTP-eC9 binary film slightly changed the bulk and surface morphology of the photoactive layer, while appropriate phase separation size and a smooth surface could be achieved for both the D18-Cl:BTP-eC9 binary film and the optimized ternary film. Thus, with 10% PSBTBT as the third component material (D18-Cl/PSBTBT/BTP-eC9 ratio of 0.9:0.1:1.2), the ternary OPV shows a higher power conversion efficiency (PCE) of 17.35%. The improvement of photovoltaic performance is due to the short-circuit current density (JSC) enhancement from 24.65 to 26.23 mA cm–2, even though the open-circuit voltage (VOC) weakly decreased from 0.905 to 0.900 V. This work provides an effective method to find a guest polymer that matches the host binary photoactive layer, broadens the absorption spectrum, and provides efficient energy transfer within both donor materials.

KeyWords AITranslate

ternary exciton dissociation energy transfer guest donor organic photovoltaics
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01639

Chinese Library Classification Number:

Citation Information:

In order to achieve efficient organic photovoltaics (OPVs), a ternary strategy was adopted with the efficient long-wavelength light-absorption donor material of PSBTBT as the third component material (guest donor) and the D18-Cl:BTP-eC9 binary film as the host photoactive layer, which facilitates the acquisition of absorption spectra complementary to those of D18-Cl and BTP-eC9. The PL spectrum of D18-Cl was covered by the absorption spectrum of PSBTBT, which further supports the energy transfer from D18-Cl to PSBTBT. In addition, the addition of a small amount of PSBTBT to the D18-Cl:BTP-eC9 binary film slightly changed the bulk and surface morphology of the photoactive layer, while appropriate phase separation size and a smooth surface could be achieved for both the D18-Cl:BTP-eC9 binary film and the optimized ternary film. Thus, with 10% PSBTBT as the third component material (D18-Cl/PSBTBT/BTP-eC9 ratio of 0.9:0.1:1.2), the ternary OPV shows a higher power conversion efficiency (PCE) of 17.35%. The improvement of photovoltaic performance is due to the short-circuit current density (JSC) enhancement from 24.65 to 26.23 mA cm–2, even though the open-circuit voltage (VOC) weakly decreased from 0.905 to 0.900 V. This work provides an effective method to find a guest polymer that matches the host binary photoactive layer, broadens the absorption spectrum, and provides efficient energy transfer within both donor materials.

quote

GB/T 7714-2015 [1] Ziyu Yang, Zhiyong Liu, Lan Chen. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01639.
MLA [1] Ziyu Yang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01639.
APA [1] Ziyu Yang, Zhiyong Liu, & Lan Chen. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01639
IEEE [1] Ziyu Yang, Zhiyong Liu, and Lan Chen, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01639. keywords: {ternary;exciton dissociation;energy transfer;guest donor;organic photovoltaics}