Abstract AITranslate

We present a facile procedure for preparing thick (up to 300 nm) poly(3-sulfopropyl methacrylate) brushes using SI-ARGET-ATRP by conducting the reaction in a fluid film between the substrate and a coverslip. This method is advantageous in a number of ways: it does not require deoxygenation of the reaction solution, and the monomer conversion is much higher than usual since only a minimal amount of solution (microliters) is used, resulting in a tremendous reduction (∼50×) of wasted reagents. Moreover, this method is particularly suitable for grafting brushes to large substrates.

KeyWords AITranslate

polymer brushes ATRP RDRP SIATRP ARGET
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01628

Chinese Library Classification Number:

Citation Information:

We present a facile procedure for preparing thick (up to 300 nm) poly(3-sulfopropyl methacrylate) brushes using SI-ARGET-ATRP by conducting the reaction in a fluid film between the substrate and a coverslip. This method is advantageous in a number of ways: it does not require deoxygenation of the reaction solution, and the monomer conversion is much higher than usual since only a minimal amount of solution (microliters) is used, resulting in a tremendous reduction (∼50×) of wasted reagents. Moreover, this method is particularly suitable for grafting brushes to large substrates.

quote

GB/T 7714-2015 [1] Lars B. Veldscholte, Sissi de Beer. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01628.
MLA [1] Lars B. Veldscholte, and Sissi de Beer. ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01628.
APA [1] Lars B. Veldscholte, & Sissi de Beer. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01628
IEEE [1] Lars B. Veldscholte and Sissi de Beer, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01628. keywords: {polymer brushes;ATRP;RDRP;SIATRP;ARGET}