A Nonflammable Electrolyte for High-Voltage Lithium Metal Batteries AITranslate
Abstract AITranslate
The electrochemical instability of the polar solvents in electrolytes often causes reduction/oxidation at the surface of both Li anodes and nickel-rich cathodes in high-voltage lithium metal batteries (LMBs). Here, we design a bipolar molecule-regulated electrolyte with a capsule-like solvation structure and nonflammability to stabilize high-voltage LMBs. The key enabler is to design and synthesize a nonflammable bipolar molecule with a ion-dissociative polar head and a perfluorinated nonpolar tail. The bipolar solvent promotes the formation of capsule-like solvation sheaths via weak coordination and encapsulates the polar molecules inside the primary solvation shell, drastically reducing the detrimental decomposition of solvents. Finally, the assembled high-voltage cell provides high capacity retention (Li||LiNi0.8Co0.1Mn0.1O2: >90%) during 200 charge/discharge cycles under strict conditions. The capsule-like electrolyte also enables a 420 mAh pouch cell with a cell-level energy density of 440 Wh kg–1 along with long cycling stability over 150 cycles (retention: 92%).
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00706
Chinese Library Classification Number:
Citation Information:
The electrochemical instability of the polar solvents in electrolytes often causes reduction/oxidation at the surface of both Li anodes and nickel-rich cathodes in high-voltage lithium metal batteries (LMBs). Here, we design a bipolar molecule-regulated electrolyte with a capsule-like solvation structure and nonflammability to stabilize high-voltage LMBs. The key enabler is to design and synthesize a nonflammable bipolar molecule with a ion-dissociative polar head and a perfluorinated nonpolar tail. The bipolar solvent promotes the formation of capsule-like solvation sheaths via weak coordination and encapsulates the polar molecules inside the primary solvation shell, drastically reducing the detrimental decomposition of solvents. Finally, the assembled high-voltage cell provides high capacity retention (Li||LiNi0.8Co0.1Mn0.1O2: >90%) during 200 charge/discharge cycles under strict conditions. The capsule-like electrolyte also enables a 420 mAh pouch cell with a cell-level energy density of 440 Wh kg–1 along with long cycling stability over 150 cycles (retention: 92%).
quote
| GB/T 7714-2015 | [1] Guangzhao Zhang, Jiawei Li, Qingrong Wang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00706. |
| MLA | [1] Guangzhao Zhang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00706. |
| APA | [1] Guangzhao Zhang, Jiawei Li, Qingrong Wang, Hui Wang, Jun Wang, Kai Yu, Jian Chang, Chaoyang Wang, Xiang Hong, Qiang Ma, & Yonghong Deng. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00706 |
| IEEE | [1] Guangzhao Zhang, Jiawei Li, Qingrong Wang, Hui Wang, Jun Wang, Kai Yu, Jian Chang, Chaoyang Wang, Xiang Hong, Qiang Ma, and Yonghong Deng, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00706. |