Dissociative Host-Dopant Bonding Facilitates Molecular Doping in Halide Perovskites AITranslate
Abstract AITranslate
Molecular doping is a promising strategy to fine-tune the electronic properties of halide perovskites and accelerate their implementation in next-generation optoelectronics. However, a deeper understanding of the role of host-dopant interactions in these systems is needed to fully exploit the potential of this avenue. Herein, we demonstrate a surface post-treatment strategy employing n-type molecular dopant n-DMBI-H to modulate free hole density in p-type CH3NH3Sn0.75Pb0.25I3 films. We show that the adsorption of n-DMBI-H on surface Sn atoms, followed by the dissociation of an electron-donating hydride from the dopant, facilitates charge transfer to the perovskite and hole trapping at the dissociated hydride. We identify this mechanism as a key factor dictating doping compensation in perovskites, allowing carrier density control within nearly 1 order of magnitude via the dissociated molecular dopant located at film surfaces and grain boundaries. We then exploit n-DMBI-H in perovskite/transport layer junctions, achieving reduced carrier losses and improved contact selectivity and performance in p-i-n, Sn-rich perovskite solar cells. We expect this work to provide carrier density tuning guidelines for a broad range of tin-based perovskite applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00818
Chinese Library Classification Number:
Citation Information:
Molecular doping is a promising strategy to fine-tune the electronic properties of halide perovskites and accelerate their implementation in next-generation optoelectronics. However, a deeper understanding of the role of host-dopant interactions in these systems is needed to fully exploit the potential of this avenue. Herein, we demonstrate a surface post-treatment strategy employing n-type molecular dopant n-DMBI-H to modulate free hole density in p-type CH3NH3Sn0.75Pb0.25I3 films. We show that the adsorption of n-DMBI-H on surface Sn atoms, followed by the dissociation of an electron-donating hydride from the dopant, facilitates charge transfer to the perovskite and hole trapping at the dissociated hydride. We identify this mechanism as a key factor dictating doping compensation in perovskites, allowing carrier density control within nearly 1 order of magnitude via the dissociated molecular dopant located at film surfaces and grain boundaries. We then exploit n-DMBI-H in perovskite/transport layer junctions, achieving reduced carrier losses and improved contact selectivity and performance in p-i-n, Sn-rich perovskite solar cells. We expect this work to provide carrier density tuning guidelines for a broad range of tin-based perovskite applications.
quote
| GB/T 7714-2015 | [1] Luis Lanzetta, Luca Gregori, Luis Huerta Hernandez, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00818. |
| MLA | [1] Luis Lanzetta, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00818. |
| APA | [1] Luis Lanzetta, Luca Gregori, Luis Huerta Hernandez, Anirudh Sharma, Stefanie Kern, Anna M. Kotowska, AbdulHamid Emwas, Luis GutiérrezArzaluz, David J. Scurr, Matthew Piggott, Daniele Meggiolaro, Md Azimul Haque, Filippo De Angelis, & Derya Baran. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00818 |
| IEEE | [1] Luis Lanzetta, Luca Gregori, Luis Huerta Hernandez, Anirudh Sharma, Stefanie Kern, Anna M. Kotowska, AbdulHamid Emwas, Luis GutiérrezArzaluz, David J. Scurr, Matthew Piggott, Daniele Meggiolaro, Md Azimul Haque, Filippo De Angelis, and Derya Baran, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00818. |