A Novel “Water-in-Ionic Liquid” Electrolyte for Zn Metal Batteries AITranslate
Abstract AITranslate
Success in the development of aqueous batteries hinges on strict design principles for the aqueous electrolyte: utilize the high ionic conductivity but limit the redox activity of water. Here we develop a new type of electrolyte, a “water-in-ionic liquid” electrolyte, where the water molecule is sealed in a water trap composed of ions by short-range intermolecular interactions. In this way, the water molecule is protected by the surrounding anion-abundant framework and simultaneously plays its lubricant role for ionic conduction, realizing a high stability together with a high ionic conductivity (1.18 × 10–2 S cm–1) of the electrolyte. This water-confined motif promotes the formation of an explicit interphase (SEI) on a Zn metal anode, which is clearly observed for the first time and contributes to a substantially reversible Zn electrochemistry. Notably, due to the intermolecular constraint, the volatilization of this electrolyte is alleviated, which is helpful for batteries with an open system. As a proof of concept, we demonstrate zinc–air batteries (ZABs) with superior longevity compared to those using typical aqueous electrolyte under lean-electrolyte conditions (300 h vs 72 h, respectively).
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02520
Chinese Library Classification Number:
Citation Information:
Success in the development of aqueous batteries hinges on strict design principles for the aqueous electrolyte: utilize the high ionic conductivity but limit the redox activity of water. Here we develop a new type of electrolyte, a “water-in-ionic liquid” electrolyte, where the water molecule is sealed in a water trap composed of ions by short-range intermolecular interactions. In this way, the water molecule is protected by the surrounding anion-abundant framework and simultaneously plays its lubricant role for ionic conduction, realizing a high stability together with a high ionic conductivity (1.18 × 10–2 S cm–1) of the electrolyte. This water-confined motif promotes the formation of an explicit interphase (SEI) on a Zn metal anode, which is clearly observed for the first time and contributes to a substantially reversible Zn electrochemistry. Notably, due to the intermolecular constraint, the volatilization of this electrolyte is alleviated, which is helpful for batteries with an open system. As a proof of concept, we demonstrate zinc–air batteries (ZABs) with superior longevity compared to those using typical aqueous electrolyte under lean-electrolyte conditions (300 h vs 72 h, respectively).
quote
| GB/T 7714-2015 | [1] Zhiming Zhao, Joanne Lai, Duc Tam Ho, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02520. |
| MLA | [1] Zhiming Zhao, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02520. |
| APA | [1] Zhiming Zhao, Joanne Lai, Duc Tam Ho, Yongjiu Lei, Jian Yin, Long Chen, Udo Schwingenschlögl, & Husam N. Alshareef. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02520 |
| IEEE | [1] Zhiming Zhao, Joanne Lai, Duc Tam Ho, Yongjiu Lei, Jian Yin, Long Chen, Udo Schwingenschlögl, and Husam N. Alshareef, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02520. |