Electrochemical Energy and Interfaces Laboratory Department of Mechanical and Automation EngineeringThe Chinese University of Hong Kong;Electrochemical Energy and Interfaces Laboratory Department of Mechanical and Automation EngineeringThe Chinese University of Hong Kong; Beijing University of Chemical TechnologyBeijing100029;Electrochemical Energy and Interfaces Laboratory Department of Mechanical and Automation EngineeringThe Chinese University of Hong Kong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Redox flow batteries are promising energy storage technologies. Low-cost electrolytes are the prerequisites for large-scale energy storage applications. Herein, we describe an ultra-low-cost sulfur–manganese (S–Mn) redox flow battery coupling a Mn2+/MnO2(s) posolyte and polysulfide negolyte. In addition to the intrinsically low cost active materials, the polysulfide negolyte removes the long-unresolved metal dendrite issue of metal–Mn batteries (e.g., Zn–Mn2+/MnO2(s) batteries), enabling substantially improved cycling stability at a high areal capacity (50–100 mAh cm–2). Due to the low cost of both sulfur and manganese species, this system promises an ultralow electrolyte cost of $11.00 kWh–1 (based on achieved capacity). This work broadens the horizons of aqueous manganese-based batteries beyond metal–manganese chemistry and offers a practical route for low-cost and long-duration energy storage applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02524

Chinese Library Classification Number:

Citation Information:

Redox flow batteries are promising energy storage technologies. Low-cost electrolytes are the prerequisites for large-scale energy storage applications. Herein, we describe an ultra-low-cost sulfur–manganese (S–Mn) redox flow battery coupling a Mn2+/MnO2(s) posolyte and polysulfide negolyte. In addition to the intrinsically low cost active materials, the polysulfide negolyte removes the long-unresolved metal dendrite issue of metal–Mn batteries (e.g., Zn–Mn2+/MnO2(s) batteries), enabling substantially improved cycling stability at a high areal capacity (50–100 mAh cm–2). Due to the low cost of both sulfur and manganese species, this system promises an ultralow electrolyte cost of $11.00 kWh–1 (based on achieved capacity). This work broadens the horizons of aqueous manganese-based batteries beyond metal–manganese chemistry and offers a practical route for low-cost and long-duration energy storage applications.

quote

GB/T 7714-2015 [1] Jiafeng Lei, Yanxin Yao, Yaqin Huang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02524.
MLA [1] Jiafeng Lei, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02524.