pH-Responsive Swelling Micelles for the Treatment of Methicillin-Resistant Staphylococcus aureus Biofilms AITranslate

Brown University; Brown University; Brown University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Biofilm formation exacerbates the challenge of eradicating drug-resistant bacterial infections. Methicillin-resistant Staphylococcus aureus (MRSA) is one of the major pathogens that leads to biofilm infections of the skin and soft tissue and device-associated infections. Here, we report a pH-responsive micelle that swells while releasing the loaded antibiotic, ciprofloxacin, in the low pH environment of MRSA biofilms. The antibiotic-loaded micelles were found to be more effective at eliminating MRSA biofilm bacteria and biofilm supernatant bacteria compared to treatment with free ciprofloxacin or pH-responsive micelles without encapsulated antibiotics. Blank pH-responsive micelles exhibited either comparable or greater reduction in MRSA biofilm bacteria burden compared to biofilms treated with only ciprofloxacin. Overall, our studies demonstrate the promise of using pH-swelling nanoparticles for the treatment of biofilm bacteria.

KeyWords AITranslate

methicillinresistant Staphylococcus aureus (MRSA) biofilms micelles nanoparticles antimicrobial infection
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01307

Chinese Library Classification Number:

Citation Information:

Biofilm formation exacerbates the challenge of eradicating drug-resistant bacterial infections. Methicillin-resistant Staphylococcus aureus (MRSA) is one of the major pathogens that leads to biofilm infections of the skin and soft tissue and device-associated infections. Here, we report a pH-responsive micelle that swells while releasing the loaded antibiotic, ciprofloxacin, in the low pH environment of MRSA biofilms. The antibiotic-loaded micelles were found to be more effective at eliminating MRSA biofilm bacteria and biofilm supernatant bacteria compared to treatment with free ciprofloxacin or pH-responsive micelles without encapsulated antibiotics. Blank pH-responsive micelles exhibited either comparable or greater reduction in MRSA biofilm bacteria burden compared to biofilms treated with only ciprofloxacin. Overall, our studies demonstrate the promise of using pH-swelling nanoparticles for the treatment of biofilm bacteria.

quote

GB/T 7714-2015 [1] Carly Deusenbery, Carolina Gomez Casas, Anita Shukla. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01307.
MLA [1] Carly Deusenbery, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01307.
APA [1] Carly Deusenbery, Carolina Gomez Casas, & Anita Shukla. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01307
IEEE [1] Carly Deusenbery, Carolina Gomez Casas, and Anita Shukla, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01307. keywords: {methicillinresistant Staphylococcus aureus (MRSA);biofilms;micelles;nanoparticles;antimicrobial;infection}