daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

pH-Responsive Capsules Fabricated by Interfacial Photo-Cross-Linking Utilizing the Photoreactivity and pH-Responsiveness of Thymine AITranslate

Osaka Prefecture University; Osaka Prefecture University; Osaka Prefecture University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

pH-responsive capsules are useful materials for various applications, such as drug delivery systems and nano-/microreactors. Herein, we developed pH-responsive capsules through interfacial photo-cross-linking with thymine-functionalized parent polymer particles, where thymine functioned as a photoreactive and pH-responsive group. A sufficient hydrophilicity of the capsule polymers was necessary to achieve the controlled release of encapsulated molecules by utilizing the pH-responsiveness of thymine groups. Based on a series of solubility tests for various polymers derived from 4-vinylbenzyl thymine (VBT), styrene (St), 2-vinylpyridine (2VP), and 4-vinylpyridine (4VP), P(St-2VP-VBT) and P(St-VBT) were suitable for preparing capsule particles by interfacial photo-cross-linking. Release tests revealed that P(St-2VP-VBT), but not P(St-VBT), could release its cargo under basic conditions, where thymine transforms from the nonionic to anionic state. This behavior indicates that the increased hydrophilicity of the polymer shell layer obtained by copolymerization with 2VP is critical for cargo release induced by thymine deprotonation. Furthermore, P(St-2VP-VBT) also responded to acidic pH owing to protonation of the pyridine groups. Finally, we successfully created acidic and alkaline dual pH-responsive capsules via interfacial photo-cross-linking using P(St-2VP-VBT) particles.

KeyWords AITranslate

Capsule particles Interfacial photocrosslinking Nucleobase Polymer particles Stimuli responsive pH Colloid
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01283

Chinese Library Classification Number:

Citation Information:

pH-responsive capsules are useful materials for various applications, such as drug delivery systems and nano-/microreactors. Herein, we developed pH-responsive capsules through interfacial photo-cross-linking with thymine-functionalized parent polymer particles, where thymine functioned as a photoreactive and pH-responsive group. A sufficient hydrophilicity of the capsule polymers was necessary to achieve the controlled release of encapsulated molecules by utilizing the pH-responsiveness of thymine groups. Based on a series of solubility tests for various polymers derived from 4-vinylbenzyl thymine (VBT), styrene (St), 2-vinylpyridine (2VP), and 4-vinylpyridine (4VP), P(St-2VP-VBT) and P(St-VBT) were suitable for preparing capsule particles by interfacial photo-cross-linking. Release tests revealed that P(St-2VP-VBT), but not P(St-VBT), could release its cargo under basic conditions, where thymine transforms from the nonionic to anionic state. This behavior indicates that the increased hydrophilicity of the polymer shell layer obtained by copolymerization with 2VP is critical for cargo release induced by thymine deprotonation. Furthermore, P(St-2VP-VBT) also responded to acidic pH owing to protonation of the pyridine groups. Finally, we successfully created acidic and alkaline dual pH-responsive capsules via interfacial photo-cross-linking using P(St-2VP-VBT) particles.

quote

GB/T 7714-2015 [1] Yukiya Kitayama, Akali Dosaka, Atsushi Harada. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01283.
MLA [1] Yukiya Kitayama, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01283.
APA [1] Yukiya Kitayama, Akali Dosaka, & Atsushi Harada. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01283
IEEE [1] Yukiya Kitayama, Akali Dosaka, and Atsushi Harada, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01283. keywords: {Capsule particles;Interfacial photocrosslinking;Nucleobase;Polymer particles;Stimuli responsive;pH;Colloid}