daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Hydrogen Evolution Reaction in Alkaline Media: Alpha- or Beta-Nickel Hydroxide on the Surface of Platinum? AITranslate

Tsinghua University; Nanjing University; Institute of High Energy Physics; Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University; Nanjing University; Tsinghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Reducing the energy consumption of a hydrogen evolution reaction (HER) at a platinum (Pt) electrode is important for the hydrogen economy. Herein, we report the loading of alpha- or beta-nickel hydroxide (α- or β-Ni(OH)2) nanostructures on the surface of a Pt electrode to improve its catalytic activity and stability for HER in alkaline electrolytes. Both experimental and theoretical studies reveal that β-Ni(OH)2 is a better co-catalyst of Pt than α-Ni(OH)2 for promoting the HER, attributed to the higher water dissociation ability of β-Ni(OH)2, as well as the stronger interactions between β-Ni(OH)2 and the Pt electrode. Particularly, the overpotential of the HER in 0.1 M KOH at 10 mA cm–2 is decreased from 278 mV at the Pt electrode to 92 mV at the β-Ni(OH)2/Pt electrode, and the Tafel slope decreased from 62 to 42 mV dec–1, correspondingly. The performance of the β-Ni(OH)2/Pt catalytic electrode surpasses that of most of the previously reported electrodes for the same purpose.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01103

Chinese Library Classification Number:

Citation Information:

Reducing the energy consumption of a hydrogen evolution reaction (HER) at a platinum (Pt) electrode is important for the hydrogen economy. Herein, we report the loading of alpha- or beta-nickel hydroxide (α- or β-Ni(OH)2) nanostructures on the surface of a Pt electrode to improve its catalytic activity and stability for HER in alkaline electrolytes. Both experimental and theoretical studies reveal that β-Ni(OH)2 is a better co-catalyst of Pt than α-Ni(OH)2 for promoting the HER, attributed to the higher water dissociation ability of β-Ni(OH)2, as well as the stronger interactions between β-Ni(OH)2 and the Pt electrode. Particularly, the overpotential of the HER in 0.1 M KOH at 10 mA cm–2 is decreased from 278 mV at the Pt electrode to 92 mV at the β-Ni(OH)2/Pt electrode, and the Tafel slope decreased from 62 to 42 mV dec–1, correspondingly. The performance of the β-Ni(OH)2/Pt catalytic electrode surpasses that of most of the previously reported electrodes for the same purpose.

quote

GB/T 7714-2015 [1] Xiaowen Yu, Jun Zhao, LiRong Zheng, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01103.
MLA [1] Xiaowen Yu, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01103.
APA [1] Xiaowen Yu, Jun Zhao, LiRong Zheng, Yue Tong, Miao Zhang, Guochuang Xu, Chun Li, Jing Ma, & Gaoquan Shi. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01103