Original Core–Shell Structure of Cubic CsPbBr3@Amorphous CsPbBrx Perovskite Quantum Dots with a High Blue Photoluminescence Quantum Yield of over 80% AITranslate

University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

All-inorganic perovskite cesium lead halide quantum dots (QDs) have been widely investigated as promising materials for optoelectronic application because of their outstanding photoluminescence (PL) properties and benefits from quantum effects. Although QDs with full-spectra visible emission have been synthesized for years, the PL quantum yield (PLQY) of pure blue-emitting QDs still stays at a low level, in contrast to their green- or red-emitting counterparts. Herein, we obtained core–shell structured cubic CsPbBr3@amorphous CsPbBrx (A-CsPbBrx) perovskite QDs via a facile hot injection method and centrifugation process. The core–shell structure QDs showed a record blue emission PLQY of 84%, which is much higher than that of blue-emitting cubic CsPbBr3 QDs and CsPbBrxCl3–x QDs. Furthermore, a blue-emitting QDs-assisted LED with bright pure blue emission was prepared and illustrated the core–shell QDs’ promising prospect in optoelectrical application.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01243

Chinese Library Classification Number:

Citation Information:

All-inorganic perovskite cesium lead halide quantum dots (QDs) have been widely investigated as promising materials for optoelectronic application because of their outstanding photoluminescence (PL) properties and benefits from quantum effects. Although QDs with full-spectra visible emission have been synthesized for years, the PL quantum yield (PLQY) of pure blue-emitting QDs still stays at a low level, in contrast to their green- or red-emitting counterparts. Herein, we obtained core–shell structured cubic CsPbBr3@amorphous CsPbBrx (A-CsPbBrx) perovskite QDs via a facile hot injection method and centrifugation process. The core–shell structure QDs showed a record blue emission PLQY of 84%, which is much higher than that of blue-emitting cubic CsPbBr3 QDs and CsPbBrxCl3–x QDs. Furthermore, a blue-emitting QDs-assisted LED with bright pure blue emission was prepared and illustrated the core–shell QDs’ promising prospect in optoelectrical application.

quote

GB/T 7714-2015 [1] Shixun Wang, Chenghao Bi, Jifeng Yuan, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01243.
MLA [1] Shixun Wang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01243.
APA [1] Shixun Wang, Chenghao Bi, Jifeng Yuan, Linxing Zhang, & Jianjun Tian. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01243
IEEE [1] Shixun Wang, Chenghao Bi, Jifeng Yuan, Linxing Zhang, and Jianjun Tian, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01243.