Urea and Thiourea-Functionalized, Pyridinium-Based Ionic Polymers Convert CO2 to Cyclic Carbonate under Mild Conditions AITranslate
Abstract AITranslate
The employment of hydrogen-bond donors has become an important metal-free method for activating organic molecules considering their competency in epoxide activation and stabilization of reaction intermediates. In this work, pyridinium-based ionic polymers (PIP) were synthesized, which readily reacted with 3,5-bis(trifluoromethyl)phenyl isothiocyanate and 3,5-bis(trifluoromethyl) phenyl isocyanate under ambient conditions to introduce thiourea and urea structures into the porous polymer. Consequently, bifunctional polymers PIP-thiourea and PIP-urea containing quaternary ammonium centers and dual hydrogen-bond donors were fabricated. The polymers were tested as catalysts for the cycloaddition reaction of CO2 and epoxides. The results reveal a higher catalytic activity of both catalysts PIP-thiourea and PIP-urea than that of catalyst PIP, which confirms the efficacy of the hydrogen bonds introduced by the post-modification in epoxide activation and catalytic activity improvement. A substantial yield of the corresponding cyclic carbonate products can be obtained with only 0.3 mol % catalysts. In addition, the as-synthesized heterogeneous catalysts exhibited good stability and excellent recyclability. Hopefully, the designed polymers will prove to play a powerful role in catalytic reactions for CO2 utilization.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00734
Chinese Library Classification Number:
Citation Information:
The employment of hydrogen-bond donors has become an important metal-free method for activating organic molecules considering their competency in epoxide activation and stabilization of reaction intermediates. In this work, pyridinium-based ionic polymers (PIP) were synthesized, which readily reacted with 3,5-bis(trifluoromethyl)phenyl isothiocyanate and 3,5-bis(trifluoromethyl) phenyl isocyanate under ambient conditions to introduce thiourea and urea structures into the porous polymer. Consequently, bifunctional polymers PIP-thiourea and PIP-urea containing quaternary ammonium centers and dual hydrogen-bond donors were fabricated. The polymers were tested as catalysts for the cycloaddition reaction of CO2 and epoxides. The results reveal a higher catalytic activity of both catalysts PIP-thiourea and PIP-urea than that of catalyst PIP, which confirms the efficacy of the hydrogen bonds introduced by the post-modification in epoxide activation and catalytic activity improvement. A substantial yield of the corresponding cyclic carbonate products can be obtained with only 0.3 mol % catalysts. In addition, the as-synthesized heterogeneous catalysts exhibited good stability and excellent recyclability. Hopefully, the designed polymers will prove to play a powerful role in catalytic reactions for CO2 utilization.
quote
| GB/T 7714-2015 | [1] Yinpeng Wang, Jiaxian Duan. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00734. |
| MLA | [1] Yinpeng Wang, and Jiaxian Duan. ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00734. |
| APA | [1] Yinpeng Wang, & Jiaxian Duan. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00734 |
| IEEE | [1] Yinpeng Wang and Jiaxian Duan, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00734. keywords: {carbon dioxide fixation;cycloaddition;heterogeneous catalysis;hydrogen bonds;mesoporous materials} |