Synthesis of Aliphatic Acids from CO2 and Water at Efficiencies Close to the Photosynthesis Limit Using Mixed Copper and Iron Oxide Films AITranslate

Kyungpook National University; Texas A&M University at Qatar; Qatar University; Kyungpook National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The photocatalytic conversion of CO2 and water into value-added chemicals remains a great challenge. This study shows that uniformly mixed copper and iron oxide (CuO/CuFeO2; CFO) bulky heterojunction films are capable of converting CO2 and water into C1–C6 aliphatic acid anions and O2 at a solar-to-chemical energy conversion (STC) efficiency close to 3% under simulated sunlight in the absence of any sacrificial chemicals or electrical biases. When the CFO film is simply wired to a Pt foil, C1 (formate, with selectivity of 100%) and O2 are produced at a near-stoichiometric ratio at an STC efficiency of ∼5% via the Z-scheme charge transfer mechanism. The CFO films are durable over 1 week and recyclable over 5 weeks under continuous irradiation. The addition of chloride enhances formate production, with an STC efficiency of 10%, while inhibiting the deformation of CFOs. Density functional theory computations support the observed selectivity and durability.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01281

Chinese Library Classification Number:

Citation Information:

The photocatalytic conversion of CO2 and water into value-added chemicals remains a great challenge. This study shows that uniformly mixed copper and iron oxide (CuO/CuFeO2; CFO) bulky heterojunction films are capable of converting CO2 and water into C1–C6 aliphatic acid anions and O2 at a solar-to-chemical energy conversion (STC) efficiency close to 3% under simulated sunlight in the absence of any sacrificial chemicals or electrical biases. When the CFO film is simply wired to a Pt foil, C1 (formate, with selectivity of 100%) and O2 are produced at a near-stoichiometric ratio at an STC efficiency of ∼5% via the Z-scheme charge transfer mechanism. The CFO films are durable over 1 week and recyclable over 5 weeks under continuous irradiation. The addition of chloride enhances formate production, with an STC efficiency of 10%, while inhibiting the deformation of CFOs. Density functional theory computations support the observed selectivity and durability.

quote

GB/T 7714-2015 [1] Unseock Kang, Sun Hee Yoon, Dong Suk Han, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01281.
MLA [1] Unseock Kang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01281.
APA [1] Unseock Kang, Sun Hee Yoon, Dong Suk Han, & Hyunwoong Park. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01281
IEEE [1] Unseock Kang, Sun Hee Yoon, Dong Suk Han, and Hyunwoong Park, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01281.